Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.73 g/cc | 0.0625 lb/in³ | 50% resin content |
Park Electrochemical Nelco® N8000Q Cyanate Ester Epoxy Laminate and Prepreg The Nelco N8000 is a high-Tg cyanate ester laminate and prepreg system that provides superior performance and product integrity and is ideal for board designs with higher layer counts, finer lines a.. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | STN 64 0111 |
Plastcom SLOVASTER® B GF 30 FRL 4 Polybutylene Terephthalate, 30% Chemically Coupled Glass Fiber, Bromine Hydrocarbon Flame Retardant FeaturesPBT with the content of 30% chemically coupled glass fiber and flame retardant based on bromine hydrocarbons. Anisotropy of shrinkage enables injection moulding of round, cylindrical or oth.. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ISO 1183 |
DuPont Performance Polymers Rynite® RE19051 BK507 PET
(Unverified Data**) Rynite® RE19051 BK507 is a 40% glass and mineral reinforced, flame retardant, polyethylene terephthalate black resin.Information provided by DuPont Performance Polymers |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ASTM D792 |
Plenco 50045 PET, Pellet, Injection Molded, Black
(discontinued **) PLENCO 50045 is an engineering grade glass reinforced polyethylene terephthalate resin designed for higher physical strength. It is UL listed and available in white, natural, and black.Information s.. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ASTM D792 |
Rostone Rosite® 4950BS SMC Thermoset Polyester, 10% Glass Reinforced
(discontinued **) Key Features: Low Shrink; Tight DimensionsRemarkable physical and electrical strength combined with excellent dimensional stability. Information provided by Oneida-Rostone Group. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | |
LATI Larpeek 10 G/50 PEEK, 50% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Density | 1.73 - 1.78 g/cc @Temperature 22.0 - 24.0 °C |
0.0625 - 0.0643 lb/in³ @Temperature 71.6 - 75.2 °F |
|
Shandong Dongyue Shenzhou New Material Co Fluorocarbon Solvent Conformable with: Q/DYS 012-2007Fluorocarbon solvent is a mixture of perfluorocarbon circular ether. It is a colorless transparent liquid, odorless, nontoxic and uninflammable. It is unsoluble in .. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ASTM D792 |
Sumitomo Bakelite North America E 7459A Long Glass Fiber Reinforced Epoxy EM 7459A is a medium strength fiberglass reinforced epoxy molding compound, which features enhanced impact strength and toughness.Information provided by Sumitomo Bak North America, Inc. |
|||
Density | 1.73 - 1.88 g/cc | 0.0626 - 0.0678 lb/in³ | |
Saint-Gobain Chemfab® 1584N PTFE Coated Fiberglass Conveyor Belting Description: General Notes on Saint Gobain Belting Products:Saint Gobain Performance Plastics developed its belting materials for applications that require superior release characteristics, permeabi.. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | |
UCAR Carbon UCAR® PGX Pressure Molded Graphite Available in low ash monolithic sizes as large as 73" diameter, Grade PGX has excellent erosion resistance and thermal properties.Typical Applications:Fluidized bed reactors Centrifugal casting mold.. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ASTM D792 |
Plenco 6343 Phenolic, Granular, Transfer Molded PLENCO 06343 is a mica reinforced phenolic molding compound, offering for a low power factor, low electrical losses, and good electrical properties after long exposures to high humidity. UL recogniz.. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ASTM D792 |
Tipco Tipcolite® THD 121 Phenolic Compound, Wood Flour, having Medium Flow & High Strength Medium Flow Phenolic Compound, Reinforced with Wood FlourApplications: Electrical & ElectronicsProcessing: Compression MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India... |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ASTM D792 |
Plenco 6343 Phenolic, Granular, Compression Molded PLENCO 06343 is a mica reinforced phenolic molding compound, offering for a low power factor, low electrical losses, and good electrical properties after long exposures to high humidity. UL recogniz.. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | |
Trelleborg Emerson & Cuming Eccobond® 2780-45 One-Component High Temperature Performance Epoxy Adhesive Emerson & Cuming 2780-45 Eccobond® One-Component High Temperature Performance Epoxy AdhesiveFilled, pourable, high temperature resistant, epoxy adhesive. Long term resistance to boiling glycol. Exc.. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ISO 1183 |
DuPont Performance Polymers Rynite® RE19051 BK507 Polyethylene Terephthalate (PET) 40% Glass/Mineral Reinforced Flame Retardant Polyethylene Terephthalate Rynite RE19051 BK507 is a 40% glass and mineral reinforced flame retardant polyethylene terephthalate black resin.Information .. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ISO 1183 |
Eurostar Starflam RF0023E PA66/6, 10% Glass Filled, Injection Molded Starflam RF0023E is a Mineral Flame Retardant, Halogen Free and Phosphorous Free, Glass Fiber Reinforced, Polyamide 66/6 Injection Molding (also known as RF1002Z230EM)Information provided by Polymer.. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | |
Dow Saran® 525 PVDC SARAN® 525 barrier polymer, a copolymer of vinylidene chloride and vinyl chloride, designed for sheet coextrusion and forming into rigid plastic barrier containers for food applications. It is supp.. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ISO 1183 |
DSM Arnite® AV2 360 S PET-33% Glass Reinforced (European Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | |
A. Schulman ComAlloy Hiloy® 435 Glass/Mineral Reinforced, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.50% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | |
A. Schulman ComAlloy Voloy® 681 Nylon 6/6, Glass Fiber/Bead Reinforced, Nylon 6/6 Alloy, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.45% Glass Fiber/Bead Reinforced. Halogen- and phosphorous-freeThe ComAlloy product line has been integrated into the A Schulman prod.. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ISO 1183 |
BASF Ultradur® B 4040 G10 50% Glass Filled BK 15029 PBT + PET Description: Injection molding grade with 50% glass fibers for industrial parts with excellent surface quality, for example external door handles in vehicles, visible sunroof frames, oven door handl.. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ISO 1183 |
Sumitomo Bakelite North America RX® 790 Fiberglass Reinforced Phenolic Novolac RX 790 is a fiberglass reinforced phenolic novolac compound, featuring a good balance of strength and toughness. Information supplied by Sumitomo Bak North America. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Verton OV00A PPS LNP* Verton* OV00A is a compound based on Polyphenylene Sulfide resin containing Long Glass Fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Density | 1.73 g/cc | 0.0625 lb/in³ | ISO 1183 |
BASF Ultradur® B 4300 G10 50% Glass Filled PBT Description: Injection-molding grades containing 50% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, small-motor hou.. |