Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.71 g/cc | 0.0618 lb/in³ | |
Plastcom SLOVAMID 6 GF 65 PA6, 65% glass fibre FeaturesPA 6 for injection moulding, chemically strengthened with 65% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | STN EN ISO 1183-1 |
Plastcom SLOVAMID® 6 GF 65/2M PA6 reinforced with glass fiber PA 6 for injection molding, reinforced with 65% of glass fiber, for moldings used in the automotive, electrical, engineering and consumer-goods industry. Application: grips of electrotools, hobby to.. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | |
Plastcom SLOVASTER® B GF 50 PBT, 50% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 50% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ISO 1183 |
DuPont Performance Polymers Crastin® SK609 BK851 PBT
(Unverified Data**) Crastin® SK609 BK851 is a 50% glass fiber reinforced, lubricated, black polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP UFL269SA PPA (Asia Pacific) LNP* Lubricomp* UFL269SA is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Heat Stabilized,.. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP PF00C PA 6 (Asia Pacific) LNP* Thermocomp* PF00C is a compound based on Nylon 6 resin containing Glass Fiber. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RF0069S PA 66 LNP THERMOCOMP* RF0069S is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added features of this material include: Flame Retardant, Heat Stabilized. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP VERTON RV00CESS PA6.6 (Europe-Africa-Middle East) LNP Verton* RV00CESS is a compound based on PA 66 resin containing Long Glass Fiber. Added features include: Easy Molding, Heat Stabilized. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ASTM D792 |
Lubrizol Isoplast® 101LGF60NAT Engineering Thermoplastic Polyurethane Resin Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ASTM-D792 |
Polyram Polytron A60B02 Nylon 66, Chemically Coupled 60% Long Fiber A CHEMICALLY COUPLED 60% LONG FIBER GLASS REINFORCED BLACK NYLON 6.6 HEAT STABILIZED, UV STABILIZED FOR INJECTIONInformation provided by Polyram Ram On Ind. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ASTM D792 |
Covestro Baydur® STR/C-400 BB Polyurethane Composite SRIM Foam, 60% Glass Filled, MDI-based 2-Component Liquid System Contains directed chopped fiber preform glass.0.16 in. thickness.Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bay.. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ISO 1183 |
DuPont Performance Polymers Crastin® SK609 BK851 Polybutylene Terephthalate (PBT)
(Unverified Data**) 50% Glass Reinforced Polybutylene Terephthalate Crastin SK609 BK851 is a 50% glass fiber reinforced lubricated black polybutylene terephthalate resin for injection molding.Information provided by Du.. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ASTM D792 |
Ensinger Tecapeek® XP-110 Compression Molded PEEK Compound, 45% Mineral Filled Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in.. |
|||
Density | 1.71 g/cc @Temperature 23.0 °C |
0.0618 lb/in³ @Temperature 73.4 °F |
ISO 1183 |
Akro-Plastic Akromid® A3 GF 60 (2424) PA 6.6 Dry, 60% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Density | 1.71 - 1.78 g/cc | 0.0618 - 0.0643 lb/in³ | Molded |
Bulk Molding Compounds BMC T40(25)-XHS-15869 Die Casting Replacement Grade Molding Compound BMC T40(25)-XHS-15869 is a high strength molding compound with excellent dimensional stability. It is UL recognized and is available in a wide range of colors. Because of its superior physical pro.. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ASTM D792 |
Ashley Polymers Ashlene® PBT 130, 50% Glass Reinforced A 50% glass reinforced PBT designed for maximum rigidity of engineered parts.Data provided by the manufacturer |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ISO R 1183 |
Multibase Multibatch® MP 52255 Injection Molding HPP. 70% CaCO3 Filled.Information provided by Multibase |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ISO 1183 |
Polyplastic Armlen® PE MF 70-2FR Magnesium Hydroxide Filled Polyethylene 70% Magnesium HydroxideFor extrusion of fire resistant aluminum composite panels.Information provided by PolyPlastic Group. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | Dry As Molded |
Solvay Specialty Polymers Amodel® AF-1133 V0 Polyphthalamide (PPA) Resin, 33% Glass Reinforced, at 50% RH
(di AMODEL AF-1133 V0 resin in a 33% glass reinforced, flame retarded polyphthalamide (PPA) which exhibits a high deflection temperature, tensile strength, and flexural modulus. The material has good d.. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP VERTON RV00CES PA 66 LNP VERTON* RV00CES is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP VERTON RV00CES PA 66 LNP VERTON* RV00CES is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP VERTON RV00CESS PA 66 LNP VERTON* RV00CESS is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP VERTON RV00CESS PA 66 LNP VERTON* RV00CESS is a compound based on Nylon 66 resin containing 60% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP VERTON RV00CESS PA 66 (Asia Pacific) LNP VERTON* RV00CESS is a compound based on Nylon 66 resin containing Long Glass. Added features of this material include: Easy Molding. |
|||
Density | 1.71 g/cc | 0.0618 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP VERTON RV00CEXP PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00CE is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Easy Molding. |