Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.70 g/cc | 0.0614 lb/in³ | |
Premix Thermoplastics PREWHITE PE 13-60 PREWHITE PE 13-60 is a PE-LD based white masterbatch, developed especially for medical packages made by injection or blow molding of PE-LD, PE-LLD or PE-HD.Due to the good dispersion PREWHITE PE 13-.. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ISO 1183 |
LATI LARPEEK 10 G/50 50% Glass Reinforced Polyetheretherketone (PEEK)
(Unverified Data**) Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°.. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ISO 1183 |
Menzolit Menzolit® SMC 0200 Unsaturated Polyester UP SMC 0200 is a general purpose SMC for a wide range of applications. Typically, it is used as housings, covers and functional components in mechanical engineering. The flammability meets the demands .. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ISO 1183 |
Menzolit Menzolit® SMC 1600 Unsaturated Polyester UP SMC 1600 is a special SMC for sanitary applications. The glass level has been selected to combine good mouldability with good strength and stiffness properties. The material shows an increased resis.. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ISO 1183 |
Menzolit Menzolit® SMC 1650 Unsaturated Polyester UP SMC 1650 is a specially designed anti-microbial polyester moulding compound which incorporates a "germ killer" . It has been tested and found to be compliant for resistance to fungal defacement in .. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ISO 1183 |
Lanxess Pocan® DP 7244 000000 PBT, 30% Glass Fiber PBT, 30% glass fibers, injection molding, flame retardant |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ISO 1183 |
Lanxess Pocan® T 3150 XF 000000 PBT + PET, 55% Glass Fiber PBT+PET, 55% glass fibers, injection molding, improved flowability, low tendency to warp, increased temperature peak load, increased strength and increased modulus |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ASTM D572 |
Haysite 54500 Polyester SMC, 35% Glass Reinforced A high strength fiberglass reinforced thermoset polyester compound formulated for injection, compression, or transfer molding. This material exhibits excellent electrical and mechanical properties, .. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6 GF60 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6/6 GF60 L BK 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Lubricant Features: Lubricated Appearance: BlackInformation provided by TP Com.. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6/6 GF60 X 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File N.. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ASTM D792 |
ScanTube ECTFE Tubing Information provided by ScanTube, Inc. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ISO 1183 |
Unitika A1022GFL60 PA6, 60% Glass Fiber Reinforced, Dry Information provided by Unitika Ltd. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ASTM F1315 |
Thermoseal ML-5270 PTG Gasketing Thermoseal ML-5270 is a high performance synthetic fiber and polychloroprene binder gasket material that is resistant to refrigerants and oil mixtures. Its unique Multi-Layer Technology structure pr.. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | Relative Density; ISO 1183 |
Vyncolit 2723 W Novolac Phenolic Mineral and organic filled phenolic molding compound with excellent mechanical, thermal and dielectric properties. I2/FO classified under NF F 16-101 (Fire & Smoke classification).USES: Circuit bre.. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | Relative Density; ISO 1183 |
Vyncolit 2950 W Novolac Phenolic Mineral and glass fiber filled phenolic molding compound with a very high strain to failure in flexure. UL listed.USES: Armature insulation.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ISO 1183 |
DuPont Performance Polymers Rynite® 545 BK504 Polyethylene Terephthalate (PET)
(Unverified Data**) 45% Glass Reinforced Polyethylene Terephthalate Rynite 545 BK504 is a 45% glass reinforced modified polyethylene terephthalate with good strength and stiffness excellent dimensional stability and cr.. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ISO 1183 |
Eurotec® Tecodur® PB70 GR30 NL XA 21 PBT/PET 30% glass fiber reinforced, UL94 V0 Excellent stiffness and hardnessGood mechanical strengthGood creep and fatigue behaviorVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance.. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ISO 1183 |
Eurotec® Tecopet® PT70 GR30 NL100 XD70 PET, 30% glass fiber reinforced, flame retardant - halogen (RoHS compliant), long-term heat stabilized, natural Information provided by Eurotec® |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ASTM D792 Method A |
Arlon 25N Low-Cost Ceramic Hydrocarbon High Frequency, Low Loss Thermoset Laminate and Prepreg for Double-sided, Multilayer and Mixed Dielectric Printed Circuit BoardsLow loss ceramic-filled thermoset resinTight dielectric tolerance cont.. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | |
BASF Heligoen® Blue L 6990 F Color Additive Description: Highly transparent Phthalocyanine blue pigment with neutral flopChemical Structure: Cu-phthalocyanine, alpha-stabPhysical form: PowderSuitable for: Baking systems, Waterborn systems, Ac.. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
Arlon Thermabond® R36300W008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: Low Outgassing, Thermally Conductive, Electrically Insulating, Thermabond® Bonds without primerRecommended Primers: Dow Corning S2260Design/Construction: Liner: FEP Product: Uncured S.. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ISO 1183 |
BASF Petra® 140 45% Glass Filled PET Petra 140 is a 45% glass reinforced injection molding polyethylene terephthalate (PET) offering an increased level of strength, stiffness, high temperature performance and dimensional stability. Ex.. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ISO 1183 |
BASF Petra® 140 BK-112 45% Glass Filled PET Petra 140 BK-112 is a 45% glass reinforced, pigmented black, polyethylene terephthalate (PET) injection molding compound offering an increased level of strength, stiffness, high temperature performa.. |
|||
Density | 1.70 - 1.76 g/cc | 0.0614 - 0.0636 lb/in³ | Molding; IS 867-1963 |
Amity Thermosets ATO 156 Phenolic Molding Glass Filler, Compression Molded Characteristics:High electrical insulationHigh mechanical strengthDimensional stabilityLow water absorptionColor-black Medium flow Applications: High electric insulation componentsHigh voltage swit.. |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ASTM D792 |
Ashley Polymers Ashlene® E128 PET Polyester, 45% Glass Reinforced PET Polyester, economy grade with 45% glass reinforcement.Data provided by the manufacturer |
|||
Density | 1.70 g/cc | 0.0614 lb/in³ | ASTM D792 |
Ashley Polymers Ashlene® PE128 PET Polyester, 45% Glass Reinforced PET Polyester, with 45% glass reinforcement.Data provided by the manufacturer |