Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.69 g/cc | 0.0611 lb/in³ | ASTM D792 |
Owens Corning Glass Fiber Reinforced Polyester (Pultruded), 55 wt.% glass Polyester thermosets are available in many formulations. They can be formulated for good to excellent resistance to acids, weak alkalis, and organic solvents. However, they are not recommended for u.. |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | ISO 1183 |
DuPont Performance Polymers Crastin® SK645FR BK851 PBT
(Unverified Data**) Crastin® SK645FR BK851 is a flame retardant , 30% glass reinforced black polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.75mm.Information provided by DuPont Performance P.. |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP DFL38 PC LNP* Lubricomp* DFL-4038 is a Polycarbonate containing 40% Glass Fiber, 15% PTFE. Added features include: Internally Lubricated. |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | ISO 1183 |
Lanxess Durethan® DP BM 65 X FM30 901510 Nylon 6, 65% Mineral + Glass Fiber PA, injection molding and hybrid grade based on PA 6, 65% mineral/glass fibers, UL 94V-0 at 1.2 mm, reduced cycle times (easy flow), Thin wall application, free from halogen and phosphorous, low smo.. |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP OFL36 PPS - Branched (Asia Pacific) LNP LUBRICOMP* OFL36 is a compound based on PPS - Branched resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP OFL36A PPS - Branched LNP* LUBRICOMP* OFL36A is a compound based on PPS - Branched resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP OFL36A PPS - Branched (Europe-Africa-Middle East) LNP LUBRICOMP* OFL36 is a compound based on PPS - Branched resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP OFL36XXC PPS - Linear LNP* LUBRICOMP* OFL36XXC is a compound based on PPS - Linear resin containing 30% Glass Fiber, 15% PTFE. Added features of this grade are: Wear Resistant. |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP HX03408 PA11 LNP* Thermocomp* HX03408 is a compound based on Nylon 11 containing Proprietary Fillers. Added feature includes: Clean Compound System |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP WBL36L PBT LNP* LUBRICOMP* WBL36L is a compound based on PBT resin containing 30% Glass Bead, 15% PTFE. Added features of this material include: Wear Resistant, Low Extractible. |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® SHF4960 PBT (Europe-Africa-Middle East) Valox Super high flow grade, 30% glass filled Flame retardant, High CTI, heat stabilized with mold release. |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | |
SMAC BARRIER® Damping Material SMAC BARRIER® is a new material developed by SMAC to complete the range of solutions for noise reduction into an aircraft. SMAC BARRIER® is an acoustic layer designed to reduce the transmissio.. |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP VERTON RV0079 PA 66 (Asia Pacific) LNP VERTON* RV0079 is a compound based on Nylon 66 resin containing Flame Retardant, Long Glass Fiber, Long Glass. Added features of this material include: Easy Molding. |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | ISO 1183 |
DSM Arnite® B427 SE/R PBT-GF35 FR(17) 35% Glass Reinforced, Flame Retardant |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® GV-6 FWA black 9225 PA*-GF60 Product description: Grivory GV-6 FWA black 9225 is a 60% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copol.. |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® GV-6 FWA nat PA*-GF60 Product description: Grivory GV-6 FWA natural is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | dry; ISO 1183 |
DSM Stanyl® TW278F10 (PA46+PTFE)-GF50 50% Glass Reinforced, Heat Stabilized, Wear and Friction Modified |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | ASTM D792 |
Ensinger Tecatron® XP-68 Compression Molded PPS Compound, 25% Fiberglass with Graphite Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® GV-6H black PA*-GF60 Product description: Grivory GV-6H black 9915 is a 60% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® GVL-6H black 9839 PA*-GF60 Product description: Grivory GVL-6H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 60% long glass fibers. Grivory GVL-6H blac.. |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® GVX-6 H nat PA*-GF60 Product description: Grivory GVX-6H natural is a 60% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline polyamide with partially aromatic copolyamid.. |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | ISO 1183 |
Eurotec® Tecopet® PT74 GR45 BK002 PR PET, 45% glass fiber reinforced, high heat stabilized, black Information provided by Eurotec® |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | |
A. Schulman ComAlloy E-16769N Internally Lubricated, Glass Fiber Reinforced PPS Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | |
A. Schulman ComAlloy Voloy® 417 Polyester - PBT, Glass/Mineral Reinforced, Flame Retardant, UL Data provided by the manufacturer, ComAlloy International Company.43% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Density | 1.69 - 1.89 g/cc | 0.0611 - 0.0683 lb/in³ | Molded |
Bulk Molding Compounds BMC T40(25)-XHS Die Casting Replacement Grade Molding Compound BMC T40(25)-XHS is a high strength molding compound with excellent dimensional stability. It is UL recognized and is available in a wide range of colors. Because of its superior physical propertie.. |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | ISO 1183 |
DSM Arnite® TV4 260 S PBT-30% Glass Reinforced (European and Asian Grade) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | ISO 1183 |
EMS-Grivory Grivory® GV-6H EF nat PA*-GF60 Product description: Grivory GV-6H EF black 9915 is a 60% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copol.. |
|||
Density | 1.69 g/cc | 0.0611 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP VERTON RV0079 PA 66 LNP VERTON* RV0079 is a compound based on Nylon 66 resin containing 35% Long Glasss Fiber. Added features of this material include: Flame Retardant, Structural. |