Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.650 g/cc | 0.05961 lb/in³ | Coating; 40 g/m² PVDC coating on PVC 250 |
Solvay Specialty Polymers Diofan® A 736 Polyvinylidene Chloride (PVDC)
(Unverified Data**) DIOFAN® A 736 is a PVDC latex used as a flexible underlayer for coating on paper, cardboard and rigid PVC foils, to be covered with an appropriate topcoat.Additional Information: PROCESSING - DRYIN.. |
|||
Density | 1.650 g/cc | 0.05961 lb/in³ | Coating |
Solvay Specialty Polymers Ixan® SGA-1 Polyvinylidene Chloride (PVDC)
(Unverified Data**) IXAN® SGA-1 is a self-adhesive coat for use on aluminium, steel and plastic films, metallised or not. This universal grade may also be used as an adhesion primer for laminating or coating on plasti.. |
|||
Density | 1.650 g/cc | 0.05961 lb/in³ | Coating on BOPP |
Solvay Specialty Polymers Diofan® A 050 Polyvinylidene Chloride (PVDC)
(Unverified Data**) DIOFAN® A 050 is a standard grade PVDC latex for coating on various substrates. It is generally used as a topcoat on paper, cardboard and as a coating on plastic films.Additional Information: PROCE.. |