Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.60 g/cc | 0.0578 lb/in³ | ISO 1183 |
Nilit FRIANYL A63 H-SG50 Nylon 6.6 for injection molding, 50% mineral filled Nylon 6.6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Density | 1.60 g/cc | 0.0579 lb/in³ | |
Garlock BLUE-GARD® 3400 Compressed Aramid Fiber Gasketing, SBR Binder Aramid fiber, high-temperature fillers, and SBR binder. Often used in low-pressure saturated steam applications.Excellent SealabilityUnique blend of aramid fibers, fillers, and a SBR rubber binder p.. |
|||
Density | 1.60 g/cc | 0.0578 lb/in³ | ASTM D572 |
Haysite HCR-125 Corrosion Resistant Vinyl Ester/Glass Sheet A fiber glass reinforced thermoset sheet using DEREKANE® 470 vinylester in the resin matrix with flame retardant and ultraviolet inhibitors. Standard color is beige. Derakane® 470 is a registe.. |
|||
Density | 1.60 g/cc @Temperature 121 °C |
0.0579 lb/in³ @Temperature 250 °F |
Dry Density |
Mid-Mountain Materials THERMOSEAL® FIBERPAK® M33 Moldable Description: A family of high temperature moldables designed for a wide variety of uses. THERMOSEAL® FIBERPAK® MOLDABLES may be formed into shapes or linings, pushed into cracks and holes, or .. |
|||
Density | 1.60 g/cc | 0.0578 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP OX91041 PPS - LINEAR (Europe-Africa-Middle East) LNP* LUBRICOMP* OX91041 is a compound based on PPS Linear resin containing Carbon Fiber, Glass Fiber, PTFE. Added features include: Internally Lubricated, Electrically Conductive. |
|||
Density | 1.60 g/cc | 0.0578 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP WFP36 PBT (Europe-Africa-Middle East) LNP* Lubricomp* WFP36 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, PTFE, Silicone. |
|||
Density | 1.60 g/cc | 0.0578 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Omnix® 9050 Polyamide, High Performance (HPPA), 50% Glass Fiber Omnix® 9050 is a 50% glass-fiber reinforced high-performance polyamide. It is hot-water moldable and intended for use in components requiring superior mechanical properties even after moisture ab.. |
|||
Density | 1.60 g/cc | 0.0578 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6/6 GF/M15 HS L BK 40/15% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by Weight and Mineral Filler, 15% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures.. |
|||
Density | 1.60 g/cc | 0.0578 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP Thermocomp EF008E PEI (Asia Pacific) LNP* Thermocomp* EF008E is a compound based on Polyetherimide resin containing Glass Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Asia Pac.. |
|||
Density | 1.60 g/cc | 0.0578 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP JF006LXZ PES LNP* THERMOCOMP* JF006LXZ is a compound based on Polyethersulfone resin containing 30% Glass Fiber. Added features of this material include: Low Extractible. |
|||
Density | 1.60 g/cc | 0.0578 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP PDXE98480 PEI LNP* Thermocomp* PDXE98480 is a compound based on Polyetherimide with Proprietary Fillers. Added feature of this grade: Reinforced. |
|||
Density | 1.60 g/cc | 0.0578 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP 9X94104 PEI (Europe-Africa-Middle East) LNP* THERMOCOMP* 9X94104 is a compound based on Polyetherimide resin containing Glass Fiber. |
|||
Density | 1.60 g/cc | 0.0578 lb/in³ | DIN 53479 |
Polyram PlusTek PA324G6 Nylon 6.6, UL-94 V-0 30% Glass Fiber Self extinguishing (UL-94 V-0) 30% glass fiber reinforced polyamide 6.6 for component with high stiffness and dimensional stabilityInformation provided by Polyram Ram On Ind. |
|||
Density | 1.60 g/cc | 0.0578 lb/in³ | Relative Density; ISO 1183 |
Vyncolit X7010 Novolac Phenolic Glass fiber reinforced molding compound with excellent mechanical and thermal properties.USES: Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Density | 1.60 g/cc | 0.0578 lb/in³ | D792 |
Zhejiang Juner 301-G20 20% Glass Fibre Reinforced and Flammable Resistant Applications: Electrons and Electricity: TV Components, Plugs of Computers, Exhaust Fans of Computers, Plugs, Sockets, Shells of Electronics, Framework of Level Output Transformers, Pipe Pedestals, .. |
|||
Density | 1.60 g/cc | 0.0578 lb/in³ | |
Zircar Refractory Composites RS-DA Refractory Sheet ZIRCAR Refractory Sheet Type RS-D is a structural high-alumina product supplied in thin sheet form. It is composed of high purity alumina, reinforced with high-alumina ceramic fibers. Refractory She.. |
|||
Density | 1.60 g/cc | 0.0578 lb/in³ | Cured |
Chesterton MRS S2 Metal Rebuilding System An advanced ceramic composite for the resurfacing and protection of all metal surfaces. It is normally applied at a thickness of 250 microns (10 mils) per coat. Non-shrinking, 100% solids. MRS S2 is.. |
|||
Density | 1.60 g/cc | 0.0578 lb/in³ | ISO 1183 |
Eurostar Starflam AFR560B5 PA66, Mineral/Glass Fiber Reinforced, Flame Retardant, Injection Molding Starflam AFR560B5 is a Flame Retardant, Mineral Filled and Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Density | 1.60 g/cc | 0.0578 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
Arlon 32980X050 0.050" Uncured Silicone Rubber on Polyester Film Design/Construction:Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: Polyester FilmThis data represents typical values for the production material and should not be used as material.. |
|||
Density | 1.60 g/cc | 0.0578 lb/in³ | |
BASF Heligoen® Blue K 6911 D Color Additive Chemical Structure: Cu-phthalocyanine alpha stabApplication: Colourant for plastics; PVC-p, PVC-u, PUR, LD-PE, HD-PE, PP, PS, SB, SAN, PMMA, PA, PETP, CA/CAB, and UPRecommendations for food applicat.. |
|||
Density | 1.60 g/cc @Temperature 23.0 °C |
0.0578 lb/in³ @Temperature 73.4 °F |
ASTM D792 |
Beijing Ranger Chem PBT-201-G30 291 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Density | 1.60 g/cc @Temperature 23.0 °C |
0.0578 lb/in³ @Temperature 73.4 °F |
ASTM D792 |
Beijing Ranger Chem PBT-MFC-101G30 FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Density | 1.60 g/cc | 0.0578 lb/in³ | |
BASF Heligoen® Blue K 6850 Color Additive Chemical Structure: Cu-Phthalocyanine alpha instab.Application: Colourant for plastics; PVC-p, PVC-u and UPRecommendations for food applications: BgVV, FDA, FrancePhysical form: PowderInformation pr.. |
|||
Density | 1.60 - 1.64 g/cc | 0.0578 - 0.0592 lb/in³ | ISO R 1184 |
Fainplast Compounds RE 140/1 Rigid PVC, Extrusion Drain-pipes |
|||
Density | 1.60 g/cc | 0.0578 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® FR50 BK505 Nylon 66
(Unverified Data**) 25% Glass Reinforced Flame Retardant Polyamide 66 Zytel FR50 BK505 is a 25% glass fiber reinforced flame retardant black polyamide 66 resin for injection molding.Information provided by DuPont Perfo.. |
|||
Density | 1.60 g/cc | 0.0578 lb/in³ | ISO 1183 |
LATI LATILUB 80-40GRT Polyphenylene sulfide Base (PPS), 40% Graphite and PTFE Self Lubricating Plastic
(U Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
Density | 1.60 g/cc | 0.0578 lb/in³ | ISO 1183 |
Lanxess Durethan® AKV 25 F30 000000 Nylon 66, 25% Glass Fiber PA 66, 25% glass fiber, injection molding, flame retardantInformation provided by LANXESS. |