Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.57 g/cc | 0.0567 lb/in³ | ISO 1183 |
Lanxess Durethan® BKV 50 H2.0 EF 900116 Nylon 6, 50% Glass Fiber PA 6, injection molding grade, 50% glass fibers, good heat-ageing resistance, low viscosity (easy flow)Application Examples: mirror baseplates |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | |
LATI Latishield 66-10A H2 CETG/400 PA66, Steel/Glass Fiber Reinforced, Mineral Filled, Heat Stabilized EMI shielding product based on Polyamide 66 (PA66). Steel fibers. Heat stabilized. Glass fibers / Mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Ameri.. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP WFP36 PBT LNP LUBRICOMP* WFP36 is a compound based on PBT resin containing 30% Glass Fiber, 15% PTFE/Silicone. Added features of this material include: Wear Resistant. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP WFP36 PBT (Asia Pacific) LNP LUBRICOMP* WFP36 is a compound based on Polybutylene Terephalate resin containing Silicone, Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Torlon® 4645 Polyamide-imide (PAI) Torlon® 4645, an injection-moldable, wear-resistant grade of polyamide-imide (PAI), has been formulated to give outstanding wear resistance in lubricated wear applications.Features: Flame Retarda.. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6 GF50 HS UV BK 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant, UV Stabilizer and Heat StabilizerFeatures: Lubricated, Good UV Resi.. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6 GF50 IM 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Impact ModifierFeatures: Impact ModifiedProcessing Method: Injection MoldingIn.. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6 GF50 L 50% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6/6 GF50 HS L BK 50% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc.. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6/6 GF50 L BK 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: LubricantFeatures: Lubricated Appearance: BlackInformation provided by TP Comp.. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6/6 GF50 L UV 50% Glass Filled (Dry) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant and UV StabilizerFeatures: Lubricated and Good UV ResistanceInformat.. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP OF006 PPS - Linear LNP* THERMOCOMP* OF006 is a compound based on Linear PPS containing 30% Glass Fiber. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Amodel® A-8940 HS Polyphthalamide (PPA), 40% Glass Fiber Amodel® A-8940 HS is a 40% glass-fiber-reinforced, heat-stabilized polyphthalamide (PPA) with a high heat deflection temperature and very high tensile strength. Excellent creep resistance and low.. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP VERTON RV00ASXP PA 66 (Europe-Africa-Middle East) LNP* VERTON* RV00ASXP is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Heat Stabilized. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ISO 1183 |
Unitika B2040G50 PA66, 50% Glass Fiber Reinforced, Conditioned Information provided by Unitika Ltd. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ASTM D792 |
Plenco 6527 Phenolic, Granular, Transfer Molded PLENCO 06527 is a woodflour and mineral filled resole phenolic molding compound.Information supplied by Plenco. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ASTM D792 |
Plenco 4304 Phenolic, Nodular, Injection Molded PLENCO 04304 is a heat resistant, mineral filled phenolic molding compound offering improved mechanical strength properties along with excellent dimensional stability. UL recognized under component .. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ASTM D542-90 |
DuPont™ Kapton® 250FN029 Polyimide/FEP Composite Film 250 Gauge film structure consisting of a 50 µm (2 mil) base polyimide film with a 13 µm (0.5 mil) coating of Teflon® FEP on one side.Kapton® Type HN film coated with Teflon® FEP fluoropolymer r.. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ISO 1183 |
DuPont Performance Polymers Crastin® LW9030FR NC010 PBT+ASA
(Unverified Data**) 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030FR NC010 is a 30% glass fiber reinforced flame retardant polybutylene terephthal.. |
|||
Density | 1.57 g/cc @Temperature 23.0 °C |
0.0567 lb/in³ @Temperature 73.4 °F |
DIN 53 479 |
Ensinger TECASINT 1031 Polyimide, 40% Graphite Filled (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ISO 1183 |
DuPont Performance Polymers Rynite® 935SUV BK593 Polyethylene Terephthalate (PET)
(Unverified Data**) 35% Glass Reinforced UV Stabilized Polyethylene Terephthalate Rynite 935SUV BK593 is a 35% glass fiber /mineral reinforced UV stabilized modified polyethylene terephthalate resin with low warpage de.. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | cured; ASTM D794 |
3M Scotchcast™ 5388 Electrical Epoxy Powder Resin 3M Scotchcast Electrical Resin 5388 is a one-part, blue pigmented, rapid heat curing powder resin, designed to provide a continuous, tough moisture and chemical resistant dielectric coating to a var.. |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | |
3M Scotchkote™ 162HB Epoxy Coating 3M Scotchkote Epoxy Coating 163HB has been specifically developed as a 100% solids lining for the internals of pipes, tanks, vessels and other equipment in contact with fresh water, sea water, raw w.. |
|||
Density | 1.57 - 1.61 g/cc | 0.0567 - 0.0582 lb/in³ | ISO R 1184 |
Fainplast Compounds RE 130 Rigid PVC, Extrusion Pipes and profiles |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® HTN 51G45HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTN51G45HSL BK083 is a 45% glass reinforced, heat stabilized, lubricated high performance polyamide resin. It is also a PPA resin.Information provided by DuPont Performance Polymers |
|||
Density | 1.57 g/cc | 0.0567 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP PFB91S PA 6 LNP* THERMOCOMP* PFB91S is a compound based on Nylon 6 resin containing Proprietary Filler(s). |