Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.54 g/cc | 0.0556 lb/in³ | ISO 1183 |
DuPont Performance Polymers Crastin® SK615SF NC010 PBT
(Unverified Data**) Crastin® SK615SF is a 30% glass fiber reinforced, low viscosity polybutylene terephthalate for injection molding. It has high flow characteristics and is specifically suitable for super fast produc.. |
|||
Density | 1.54 g/cc | 0.0556 lb/in³ | ISO 1183/A |
Solvay Specialty Polymers Amodel® A-1133 NL WH 505 Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1133 NL resin is a 33% glass reinforced polyphthalamide (PPA) which is distinguished by its high-reflectivity white color. This grade features a high deflection temperature for compatibilit.. |
|||
Density | 1.54 g/cc | 0.0556 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36XXP PC LNP* Lubricomp* DFL36XXP is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Density | 1.54 - 1.58 g/cc | 0.0556 - 0.0571 lb/in³ | ISO R 1184 |
Fainplast Compounds RE 925 Rigid PVC, Extrusion Various profiles |
|||
Density | 1.54 g/cc | 0.0556 lb/in³ | Mixed; ASTM D1475-85 |
Lord Adhesives Aeroglaze® K3425 Sandable Primer/Surfacer For application on epoxy graphite or other plastic substrates or over a suitable primer on metal.Limitations - Aeroglaze® K3425 primer/surfacer contains no inhibiting pigments and is not suitable.. |
|||
Density | 1.54 g/cc | 0.0556 lb/in³ | ISO 1183/A |
Solvay TECHNYL® A 30 H1 V25 PA66, 25% glass fiber, Conditioned Description: Flame-retardant polyamide 66, 25% glass-fiber reinforced, heat stabilized for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Applications:.. |
|||
Density | 1.54 g/cc | 0.0556 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP OCP36 PPS LNP* LUBRICOMP* OCP36 is a compound based on Polyphenylene Sulfide resin containing 30% Carbon Fiber, 15% PTFE/Silicone. Added features of this grade include: Wear Resistant, Bearing Grade, Electr.. |
|||
Density | 1.54 g/cc | 0.0556 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® 4031 PBT (Europe-Africa-Middle East) VALOX 4031 is a 30% high strength glass fibre reinforced PBT injection moulding resin with excellent strength, stiffness and heat resistance. Applications: appliance handles, spotlights, electric mo.. |
|||
Density | 1.54 g/cc | 0.0556 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® IQ420 PBT Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc. |
|||
Density | 1.54 g/cc | 0.0556 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP STAT-KON OEL36A PPS - BRANCHED LNP* STAT-KON* OEL36A is a compound based on PPS - Branched resin containing 15% PTFE, 30% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive. |
|||
Density | 1.54 g/cc | 0.0556 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP LF006 PEEK (Asia Pacific) LNP* Thermocomp* LF006 is a compound based on Polyetheretherketone resin containing Glass Fiber. |
|||
Density | 1.54 g/cc | 0.0556 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP ZF406XXX PPO Blend (Asia Pacific) LNP THERMOCOMP* ZF406XXX is a compound based on PPO Blend resin containing Flame Retardant, Glass Fiber. Added features of this material include: Flame Retardant. |
|||
Density | 1.54 g/cc | 0.0556 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP PF009 PA 6 (Asia Pacific) LNP THERMOCOMP* PF009 is a compound based on Nylon 6 resin containing Glass Fiber. |
|||
Density | 1.54 g/cc | 0.0556 lb/in³ | ASTM D792 |
Plenco 7507 Phenolic, Granular, Compression Molded PLENCO 07507 is an organic reinforced phenolic molding compound offering improved dimensional stability under humid conditions. 07507 offers excellent resistance to degradation from detergent solut.. |
|||
Density | 1.54 g/cc | 0.0556 lb/in³ | ISO 1183 |
Polyplastics Duranex® 3216 Polybutylene Terephthalate (PBT), Standard, FR, UL approved regrind 50%, 15% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Density | 1.54 g/cc | 0.0556 lb/in³ | ASTM D792 |
Plenco 4309 Phenolic, Nodular, Injection Molded PLENCO 04309 is a heat resistant, glass reinforced phenolic molding compound offering improved mechanical strength and electrical strength properties. UL recognized under component file E40654. 0430.. |
|||
Density | 1.54 g/cc | 0.0556 lb/in³ | dry; ISO 1183 |
DSM Novamid® 1010GN2-20 NAT/BK37 PA6-GF20 FR(17) 20% Glass Reinforced, Flame Retardant |
|||
Density | 1.54 g/cc | 0.0556 lb/in³ | ISO 1183 |
DSM Stanyl® TW271F6 (DAM) Nylon 46 30% Glass Reinforced, Heat Stabilized, PTFE Lubricated (North America) Information provided by DSM Engineering Plastics. |
|||
Density | 1.54 g/cc | 0.0556 lb/in³ | ISO 1183 |
DSM Stanyl® TW271F6 Nylon 46-30% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Density | 1.54 g/cc | 0.0556 lb/in³ | ISO 1183 |
DuPont Performance Polymers Delrin® 520MP NC010 Acetal (POM)
(Unverified Data**) 20% Teflon® Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 520MP is a medium viscosity acetal homopolymer containing 20% Teflon PTFE Micropowder. It is designe.. |
|||
Density | 1.54 g/cc | 0.0556 lb/in³ | ASTM D792 |
Ensinger Tecatron® XP-81 Compression Molded PPS Compound, Filled with 15% Graphite and 15% Carbon Fiber Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Density | 1.54 g/cc | 0.0556 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® HTN 92G45DH2 BK083 Polyphthalamide (PPA) 35% Glass Reinforced PPA High Performance Polyamide with DuPont Zytel HTN92G45DH2 BK083 is a 45% glass reinforced high performance polyamide resin using DuPont SHIELD Technology with high flow and e.. |
|||
Density | 1.54 - 1.58 g/cc | 0.0556 - 0.0571 lb/in³ | ISO R 1183 |
Fainplast Compounds AP 80 Flexible PVC, Flame Retardant Insulation General purposes |
|||
Density | 1.54 - 1.58 g/cc | 0.0556 - 0.0571 lb/in³ | ISO R 1183 |
Fainplast Compounds GA 89 Flexible PVC, Flame Retardant Sheathing General purposes |
|||
Density | >= 1.54 g/cc | >= 0.0556 lb/in³ | |
Aremco HiE-Coat™ 840-M High Emissivity Coating, Inorganic-Ceramic Filled Ceramic-based, black-pigmented coating for carbon and stainless steel to 2000 °F (1093°C). |
|||
Density | 1.54 g/cc @Temperature 23.0 °C |
0.0556 lb/in³ @Temperature 73.4 °F |
ASTM D792 |
Beijing Ranger Chem PBT-201-G20 291 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Density | 1.54 g/cc | 0.0556 lb/in³ | ASTM D792 |
Plaslok 504 Black (COM) Heat Resistant Mineral/Cellulose Filled Phenolic Molding Compound
(discontinued **)&l Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 504 is a two-stage, mineral and cellu.. |