Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.49 g/cc | 0.0538 lb/in³ | STN 64 0111 |
Plastcom SLOVAMID 66 GF 30 FRA 5 Polyamide 66, 30% Glass Fiber, Halogen Flame Retardant FeaturesPA 66 for injection moulding, reinforced with 30% glass fiber and halogen flame retardant. Application in electrical industry: breakers, coil forms, covers, terminals. Slightly decreased f.. |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | ASTM D792 |
Ravago Manufacturing Americas Hylon® N1043HL Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | ISO 1183/A |
Solvay Specialty Polymers Amodel® A-1133 DW Polyphthalamide (PPA)
(discontinued **) Amodel A-1133 DW is a 33% glass-fiber reinforced polyphthalamide (PPA) grade approved for use with potable water in the United States, the United Kingdom and France. - Natural: A-1133 NT DW - Black:.. |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | ISO 1183 |
Nilit FRIANYL A63 HS-GV50 Nylon 6.6 for injection molding, 50% glass fiber reinforced Nylon 6.6 for injection molding, high impact resistance.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | ISO 1183 |
LATI LATILUB 73/13-20T Polyoxymethylene Base (POM), 10% Mixed PTFE Self Lubricating Plastic
(Unverified D Description: Latilub self-lubricating plastic materials are more and more often designed to replace metals in applications such as gears, bushings, cams, slides, etc), for which, besides their intri.. |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | ISO 1183/A |
Solvay TECHNYL® A 218 V43 Black 21 N PA66, 43% glass fiber, Conditioned Description: Polyamide PA66, reinforced with 43% of glass fiber, heat stabilized, for injection molding.Available in: North AmericaProduct Applications: TECHNYL® A 218 V43 is used in all sectors .. |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP OCP36A PPS - Branched (Asia Pacific) LNP* Lubricomp* OCL-4536 is a compound based on PPS - Branched resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Internally Lubricated, Electrically Conductive.. |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP LUBRICOMP RBL36XXJ PA 66 LNP* LUBRICOMP* RBL36XXJ is a compound based on Nylon 66 containing 30% Glass Bead, 15% PTFE. Added features of this grade include: Low Extractable, Healthcare, Wear Resistant. |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP RX05496 PA 66 LNP* LUBRICOMP* RX05496 is a compound based on Nylon 66 resin containing 30% Mixed Glass, 15% PTFE, Silicone. Added features of this material include: Wear Resistant. |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® EH7020HF PBT+PET (Asia Pacific) Valox EH7020HF is a mineral filled PBT/PET that offers good surface appearance, high flow and good heat performance. EH7020HF was developped for automotiove bezel application that require basecoat +.. |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | ASTM D792 |
Techmer ES Luriblend® PA6/6 GF30 TL5 LE 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%)Features: Lubricated, Good Wear Resistance, Low Friction and Low Extracta.. |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Thermocomp KF002A Acetal Homopolymer (Asia Pacific) LNP THERMOCOMP* KF002A is a compound based on Acetal Homopolymer resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP KF002L Acetal Homopoly (Asia Pacific) LNP* Thermocomp* KF002L is a compound based on Acetal Homopolymer resin containing Glass Fiber. Added features of this material include: Low Extractible. |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | ASTM D792 |
Techmer ES Electrablend® PA6 04001 BL Glass/Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Stainless Steel FiberAdditive: LubricatedFeatures: Electromagnetic Shielding (EMI), Lubricated and Radio Frequency Shielding (RFI.. |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | ASTM D792 |
Sumitomo Bakelite North America XB-22 Fiberglass Reinforced Phenolic Novolac XB-22 is a fiberglass reinforced phenolic novolac molding compound, with excellent dimensional stability and good strength at elevated temperatures. This material is formulated for low thermal condu.. |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | ISO 1183-87 |
Wellman Wellamid® GFX1872-N1 (PTFE) Nylon 66, 33% Glass Reinforced, Lubricated All information provided by Wellman Engineered Resins. |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | ISO 1183-87 |
Wellman Wellamid® MR410 22H-NBK1 40% Mineral Reinforced Nylon 66 Description: Mineral Reinforced Nylon 66Information provided by Wellman. |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | Nominal Laminate |
Hexcel® HexPly® M52 120°C/250°F Curing Epoxy, M52/40%/193P/CHS-3K Fiber: HS Carbon, Plain Weave, 193 g/m2Information provided by HexCel |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | ISO 1183 |
Polyplastics Duranex® 3116 Polybutylene Terephthalate (PBT), Standard, FR, UL approved regrind 50%, 7.5% GF filled DURANEX® is a crystalline thermoplastic based on polybutylene terephthalate (PBT) that can be readily strengthened, modified, or otherwise performance enhanced through the addition of glass fibers .. |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | DAM; ISO 1183 |
DuPont Performance Polymers Zytel® 70G43L NC010 Nylon 66
(Unverified Data**) 43% Glass Reinforced Polyamide 66Zytel 70G43L NC010 is a 43% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | dry; ISO 1183 |
BASF Ultramid® 8234G HS 44% Glass Filled PA6 (Conditioned) Ultramid 8234G HS is a heat stabilized, 44% glass fiber reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensio.. |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | dry; ISO 1183 |
BASF Ultramid® 8260 HS PA6 (Conditioned) |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | ISO 1183 |
BASF Ultrason S 2010 G6 30% Glass Filled PSU Ultrason S 2010 G6 is a 30% glass reinforced, medium viscosity injection molding PSU grade with high rigidity and strength. |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | |
A. Schulman ComAlloy Hiloy® 616 Nylon 6, Mineral Reinforced Data provided by the manufacturer, ComAlloy International Company.40% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | (Dry) |
BASF Capron® 8234G 44% Glass-Filled Nylon 6 (Conditioned)
(discontinued **) Capron 8234G is a 44% glass fiber reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensional stability. It is .. |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | ISO data |
BASF Capron® 8260 HS BK-102 40% Mineral-Filled Nylon 6 (Dry)
(discontinued **) Capron 8260 HS BK-102 is a heat stabilized, pigmented black, 40% mineral reinforced nylon 6 injection molding resin. It possesses high stiffness, dimensional stability and heat resistance combined .. |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | DAM; ASTM D792 |
Ravago Manufacturing Americas Hylon® N1043L Nylon 6/6 (Cond)
(discontinued **) Information provided by Ravago. |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | ISO 1183/A |
Solvay Specialty Polymers Amodel® A-1933 HSL Polyphthalamide (PPA)
(Unverified Data**) Amodel A-1933 HSL is a 33% glass reinforced grade of polyphthalamide (PPA) resin. This grade was developed specifically for improved performance in a 50/50 ethylene glycol and water environment. Thi.. |
|||
Density | 1.49 g/cc | 0.0538 lb/in³ | ISO 1183/A |
Solvay Specialty Polymers Amodel® HFZ A-1133 L Polyphthalamide (PPA)
(Unverified Data**) Amodel® HFZ A-1133 L is a high-flow, 33% glass fiber reinforced polyphthalamide (PPA) grade. Natural: HFZ A-1133 L NT Black: HFZ A-1133 L BK 937Information provided by Solvay Specialty Polymers. |