Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | >= 1.394 g/cc | >= 0.05036 lb/in³ | Limit; M2E-71-043 |
Indorama Ventures Mexico Polyclear™ Plus 1111 PET Resin Description: La resina Polyclear® Plus PET 1111 de Arteva Specialties, es un copolimero para empaque con una viscosidad intrinseca de 0.84 dl/g. Los envases fabricados con este material tienen un.. |
|||
Density | >= 1.394 g/cc | >= 0.05036 lb/in³ | Limit; M2E-71-043 |
Indorama Ventures Mexico Polyclear™ Preserve 2201 PET Resin Description: La resina Polyclear® Preserve PET 2201 de Arteva Specialties, es un copolimero para empaque con una viscosidad intrinseca de 0.84 dl/g y esta disenada para ofrecer un redimiento supe.. |
|||
Density | >= 1.394 g/cc | >= 0.05036 lb/in³ | Limit; M2E-71-043 |
Indorama Ventures Mexico Polyclear™ Refresh 1101 PET Resin Description: La resina Polyclear® Refresh PET 1101 de Arteva Specialties, es un copolimero para empaque con una viscosidad intrinseca de 0.84 dl/g. Los envases fabricados con este material tienen.. |
|||
Density | >= 1.394 g/cc | >= 0.05036 lb/in³ | Limit; M2E-71-043 |
Indorama Ventures Mexico Polyclear™ Splash 3301 PET Resin Description: La resina Polyclear® Splash PET 3301 de Arteva Specialties, es un copolimero para empaque con una viscosidad intrinseca de 0.74 dl/g. La resina Polyclear® Splash PET 3301 ha sido .. |
|||
Density | >= 1.394 g/cc | >= 0.05036 lb/in³ | Limit; M2E-71-043 |
Indorama Ventures Mexico Polyclear™ T-94 PET Resin Description: La resina Polyclear® PET T-94 de Arteva Specialities es un copolimero de baja velocidad de cristalizacion, ideal para la fabricacion de pared gruesa, con una viscosidad intrinseca de.. |
|||
Density | 1.394 g/cc | 0.05036 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Stat-kon REL36 PA 66 LNP* Stat-Kon* REL36 is a compound based on Nylon 6/6 containing carbon fiber and PTFE. Characteristics of this grade are Statically Conductive.This data was supplied by SABIC-IP for the Americas r.. |
|||
Density | 1.394 g/cc | 0.05036 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP EC006E PEI LNP THERMOCOMP* EC006E is a compound based on Polyetherimide resin containing 30% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive |
|||
Density | 1.394 g/cc | 0.05036 lb/in³ | JIS-Z-8807 |
Denka VINYKON M7100 PVC, M grade for soft injection molding A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |
|||
Density | 1.394 g/cc | 0.05036 lb/in³ | JIS-Z-8807 |
Denka VINYKON W2035 PVC, W grade for insulation, for sheaths A PVC resin compound offering excellent physical properties and workability. A broad product lineup is available, including hard and soft grades, as well as those for extrusion and injection molding.. |