Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.31 g/cc | 0.0473 lb/in³ | ISO 1183 |
SABIC Innovative Plastics EXTEM XH1015 TPI Resin (Europe-Africa-Middle East) Thermoplastic Polyimide Extem* XH1015 Resin. |
|||
Density | 1.31 g/cc | 0.0473 lb/in³ | ISO 1183-1 |
Quadrant EPP Ketron® 1000 PEEK unfilled, extruded (ISO Data) Ketron PEEK-1000 stock shapes are produced from virgin polyetheretherketone resin and offer the highest toughness and impact strength of all Ketron PEEK grades. Both Ketron PEEK-1000 natural & black.. |
|||
Density | 1.31 g/cc | 0.0473 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® LUX2289 PC (Europe-Africa-Middle East) Lexan* LUX2289 resin is an injection molding grade with high light reflectance and UV stabilized |
|||
Density | 1.31 - 1.55 g/cc | 0.0473 - 0.0560 lb/in³ | Average value: 1.42 g/cc Grade Count:8 |
Overview of materials for Phenolic, Carbon Fiber Composite This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Carbon Fiber Composite". Each property range of values reported is minimum and maximum values .. |
|||
Density | 1.31 g/cc | 0.0473 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® FXV310SK PBT (Europe-Africa-Middle East) LIMITED USE, No New Customers / Applications as of Jan. 2010: VALOX FXV310SK is an unreinforced PBT injection moulding resin with high flow characteristics and containing a metal sparkle Visual FX. .. |
|||
Density | 1.31 g/cc | 0.0473 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® HX312C PBT (Europe-Africa-Middle East) Unreinforced PBT with release. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant. EtO and stea.. |
|||
Density | 1.31 g/cc | 0.0473 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Valox® IQ3001 PBT (Asia Pacific) Valox IQ3001 is an unfilled environmentally responsible iQ-PBT resin modified with elastomer. Targeted for flexible hinge applications. |
|||
Density | 1.31 g/cc | 0.0473 lb/in³ | ASTM D792 |
Techmer ES HiFill® PA6 GF25 L BK 25% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 25% Filler by WeightAdditive: Lubricant Features: LubricatedAppearance: BlackInformation provided by TP Comp.. |
|||
Density | 1.31 g/cc | 0.0473 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Xenoy® 364 PBT This data was supplied by SABIC-IP for the Americas region. |
|||
Density | 1.31 g/cc | 0.0473 lb/in³ | ASTM D792 |
Techmer ES HiFill® PBT 1226 Availability: North AmericaForms: PelletsFeatures: Medium FlowAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Density | 1.31 g/cc | 0.0473 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP THERMOCOMP PF005 PA 6 (Europe-Africa-Middle East) 25% glass fibre reinforced Polyamide 6 injection moulding resin. |
|||
Density | 1.31 g/cc | 0.0473 lb/in³ | ISO 1183 |
Suzhou Hipro Polymers Hiprolon® 70 MC HLS G30 Nylon 610, 30% glass fiber filled Hiprolon® 70 MC HLS G30 polyamide 6.10 compound reinforced with 30% chopped glass fiber for injection molding. Features: high heat resistance, dimension stability, impact resistance, good flow ab.. |
|||
Density | 1.31 g/cc | 0.0473 lb/in³ | ASTM-D792 |
Polyram Polytron P50N01 Homopolymer Polypropylene, Chemically Coupled 50% Long Glass Fiber A CHEMICALLY COUPLED 50% LONG GLASS FIBER REINFORCED NATURAL POLYPROPYLENE HEAT STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind. |
|||
Density | 1.31 g/cc | 0.0473 lb/in³ | DIN 53479 |
Polyram RamLloy PA917G6 PP/NYLON 66 alloy, 30% Glass Fiber 30% glass fiber reinforced PA66/PP alloy with reduced water absorption, dimensional stability and UV stabilized for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Density | 1.31 g/cc | 0.0473 lb/in³ | Film Density; ASTM D1505 |
Eastman Eastobond 19412 Copolyester, Film Eastobond 19412 is a terephthalate-based copolyester. It is identical to our 19411 resin in every aspect, except that the 19412 has been crystallized for drying purposes and ease of handling. Eastob.. |
|||
Density | 1.31 g/cc | 0.0473 lb/in³ | ASTM D792 |
Eastman Tenite Butyrate 264E0096908 Natural, Trsp Cellulose Acetate Butyrate Plasticizer 22%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
Density | 1.31 g/cc | 0.0473 lb/in³ | ASTM D 792 |
Cossa Polimeri ESTAPROP H 05100 GFC Polypropylene, 50% Glass Filled PP homopolymer 50% chemically coupled glass fiberExcellent stiffness, excellent impact strengthInformation provided by Cossa Polimeri S.r.l. |
|||
Density | 1.31 g/cc | 0.0473 lb/in³ | |
DuPont Performance Polymers Crastin® SK692FR BK507 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 15% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin® SK692FR is a 15% glass reinforced flame retardant polybutylene terephthalate for injection moulding.Information provided by .. |
|||
Density | 1.31 g/cc | 0.0473 lb/in³ | ISO 1183 |
BASF Ultramid® S3WG6 Balance 30% Glass Filled PA 610 (Dry) Description: BASF supplies polyamide 610 for processing by injection molding under the trade name Ultramid® Balance which is produced by polycondensation of hexamethylene diamine and sebacic acid. .. |
|||
Density | 1.31 g/cc | 0.0473 lb/in³ | |
Arkema Group Orgalloy® RS 6030 AT Nylon 6 Alloy, 30% Glass Fiber (Conditioned) RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties... |
|||
Density | 1.31 g/cc | 0.0473 lb/in³ | ASTM D792 |
Ashley Polymers Ashlene® 105 PBT Polyester A general purpose polyester with low shrinkage and good flow.Data provided by the manufacturer |
|||
Density | 1.31 g/cc | 0.0473 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP STAT-KON QEP35M PA6.10 LNP STAT-KON QEP35M is a compound based on Nylon 6/10 resin containing 25% Milled Carbon Fiber, 15% PTFE/Silicone. Added features of this grade include: Electrically Conductive, Wear Resistant. |