Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.300 g/cc | 0.04697 lb/in³ | |
Solvay Specialty Polymers Diofan® A 736 Polyvinylidene Chloride (PVDC)
(Unverified Data**) DIOFAN® A 736 is a PVDC latex used as a flexible underlayer for coating on paper, cardboard and rigid PVC foils, to be covered with an appropriate topcoat.Additional Information: PROCESSING - DRYIN.. |
|||
Density | 1.300 g/cc | 0.04697 lb/in³ | |
Solvay Specialty Polymers Diofan® A 050 Polyvinylidene Chloride (PVDC)
(Unverified Data**) DIOFAN® A 050 is a standard grade PVDC latex for coating on various substrates. It is generally used as a topcoat on paper, cardboard and as a coating on plastic films.Additional Information: PROCE.. |