Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.217 g/cc | 0.04397 lb/in³ | ASTM D792 |
SABIC Innovative Plastics Lexan® 920 PC Opaque colors, low viscosity, superior flame retardance. |
|||
Density | 1.217 g/cc | 0.04397 lb/in³ | ASTM D792 |
SABIC Innovative Plastics Lexan® 920 PC (Asia Pacific) Opaque colors, low viscosity, superior flame retardance. |
|||
Density | 1.217 g/cc | 0.04397 lb/in³ | ASTM D792 |
SABIC Innovative Plastics Lexan® 920A PC Low viscosity injection moldable, flame retardant PC. Exceptional surface appearance. Clear, tints and opaque colors. |
|||
Density | 1.217 g/cc | 0.04397 lb/in³ | ASTM D792 |
SABIC Innovative Plastics Lexan® 923 PC Opaque colors, low viscosity, superior flame retardance. Decreased smoke and lowered toxic gas emission. UV-stabilized. |
|||
Density | 1.217 g/cc | 0.04397 lb/in³ | ASTM D792 |
SABIC Innovative Plastics Lexan® 923 PC (Asia Pacific) Opaque colors, low viscosity, superior flame retardance. Decreased smoke and lowered toxic gas emission. UV-stabilized. |
|||
Density | 1.217 g/cc | 0.04397 lb/in³ | ASTM D792 |
SABIC Innovative Plastics Lexan® 923A PC Low viscosity, flame retardant with exceptional surface. Clear, tints and opaque colors. UV-stabilized. |
|||
Density | 1.217 g/cc | 0.04397 lb/in³ | ASTM D792 |
SABIC Innovative Plastics Lexan® 923A PC (Asia Pacific) Low viscosity, flame retardant with exceptional surface. Clear, tints and opaque colors. UV-stabilized. |
|||
Density | 1.217 g/cc | 0.04397 lb/in³ | ASTM D792 |
SABIC Innovative Plastics Lexan® 943 PC Opaque colors, medium viscosity, superior flame retardance. UV-stabilized. |
|||
Density | 1.217 g/cc | 0.04397 lb/in³ | ASTM D792 |
SABIC Innovative Plastics Lexan® 943A PC Medium viscosity, superior flame retardance. UV-Stabilized. Clear, tints and opaque colors. |
|||
Density | 1.217 g/cc | 0.04397 lb/in³ | ASTM D792 |
SABIC Innovative Plastics Lexan® 950 PC Opaque colors, high viscosity, superior flame retardance. |
|||
Density | 1.217 g/cc | 0.04397 lb/in³ | ASTM D792 |
SABIC Innovative Plastics Lexan® 920A PC (Asia Pacific) Low viscosity injection moldable, flame retardant PC. Exceptional surface appearance. Clear, tints and opaque colors. |
|||
Density | 1.217 g/cc | 0.04397 lb/in³ | ASTM D792 |
SABIC Innovative Plastics Lexan® 940A PC Medium viscosity, flame retardant PC. Exceptional surface. Clear, tints and opaque colors. |
|||
Density | 1.217 g/cc | 0.04397 lb/in³ | ASTM D792 |
SABIC Innovative Plastics Lexan® 943 PC (Asia Pacific) Opaque colors, medium viscosity, superior flame retardance. UV-stabilized. |
|||
Density | 1.217 g/cc | 0.04397 lb/in³ | ASTM D792 |
SABIC Innovative Plastics Lexan® 943A PC (Asia Pacific) Medium viscosity, superior flame retardance. UV-Stabilized. Clear, tints and opaque colors. |
|||
Density | 1.217 g/cc | 0.04397 lb/in³ | ASTM D792 |
SABIC Innovative Plastics Lexan® 950A PC (Asia Pacific) Transparent, clear and colors, high viscosity, flame retardant with exceptional surface. |
|||
Density | 1.217 g/cc | 0.04397 lb/in³ | ASTM D792 |
SABIC Innovative Plastics Lexan® 953 PC Opaque colors, high viscosity, superior flame retardance. UV-stabilized. |
|||
Density | 1.217 g/cc | 0.04397 lb/in³ | ASTM D792 |
SABIC Innovative Plastics Lexan® 953 PC (Asia Pacific) Opaque colors, high viscosity, superior flame retardance. UV-stabilized. |
|||
Density | 1.217 g/cc | 0.04397 lb/in³ | ASTM D792 |
SABIC Innovative Plastics Lexan® 953A PC (Asia Pacific) Clear, tints and opaque colors, high viscosity, flame retardant with exceptional surface. UV-stabilized. |
|||
Density | 1.217 g/cc | 0.04397 lb/in³ | |
3M Scotchcast™ 2131 Flame-Retardant Compound 3M Scotchcast Flame-Retardant Compound 2131 is a two-part polyurethane resin designed to replace the cable jacket when splicing or repairing mine and portable cables. It formulation makes it particu.. |
|||
Density | 1.217 g/cc | 0.04397 lb/in³ | ASTM D792 |
SABIC Innovative Plastics Lexan® 940 PC Opaque colors, medium viscosity, superior flame retardance. |
|||
Density | 1.217 g/cc | 0.04397 lb/in³ | ASTM D792 |
SABIC Innovative Plastics Lexan® 940A PC (Asia Pacific) Medium viscosity, flame retardant PC. Exceptional surface. Clear, tints and opaque colors. |
|||
Density | 1.217 g/cc | 0.04397 lb/in³ | ASTM D792 |
SABIC Innovative Plastics Lexan® 950A PC Transparent, clear and colors, high viscosity, flame retardant with exceptional surface. |
|||
Density | 1.217 g/cc | 0.04397 lb/in³ | ASTM D792 |
SABIC Innovative Plastics Lexan® 953A PC Clear, tints and opaque colors, high viscosity, flame retardant with exceptional surface. UV-stabilized. |
|||
Density | 1.217 g/cc | 0.04397 lb/in³ | ASTM D792 |
SABIC Innovative Plastics Lexan® 940 PC (Asia Pacific) Opaque colors, medium viscosity, superior flame retardance. |
|||
Density | 1.217 g/cc | 0.04397 lb/in³ | ASTM D792 |
SABIC Innovative Plastics Lexan® 950 PC (Asia Pacific) Opaque colors, high viscosity, superior flame retardance. |