Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.15 - 1.17 g/cc | 0.0415 - 0.0423 lb/in³ | Polymerized; ASTM D792 |
Proto3000 Objet DurusWhite FullCure430 Polypropylene-like Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | ASTM D792 |
Covestro Texin® DP7-3008 Thermoplastic Polyurethane, Polyester-based, Aliphatic
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | ISO 2781 |
Termopol Termoton® K2GA5050A TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | |
Polimeri Europa KOBLEND PCA 839F PC+ABS
(discontinued **) Symbol according to ISO 1043/1: PC+ABSUnfilled. Suitable for Injection Molding. Supplied as pellets.ISO data. Information provided by EnichemPolimeri Europa now has Enichem's plastics businesses... |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | ASTM D792 |
Huntsman IROGRAN® CA 117-200 DP TPU-Polyester Polyester-based TPUs that are specially designed for adhesives applications where high green strength and a fast crystallization rate are essential qualities.Information provided by Alliance Polymer.. |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | ASTM D792 |
Global PC/ABS-1216 General Purpose Polycarbonate/ABS Alloy Information provided by Global Polymers Corporation. |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | ASTM D792 |
Global PC/ABS-MC1220 General Purpose Polycarbonate/ABS Alloy Information provided by Global Polymers Corporation. |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | Relative, no post cure; ASTM D792 |
Multibase C6-570 Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP LUBRICOMP ZL003 PPE+PS LNP* LUBRICOMP* ZL003 is a compound based on PPE+PS resin containing 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | ASTM D792 |
Techmer ES HiFill® HIPS GF15 15% Glass Filled Availability: North AmericaForms: PelletsGlass Fiber Reinforcement, 15% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP MX85738 PP (Asia Pacific) LNP* Thermocomp* MX85738 is a compound based on Polypropylene resin containing Glass Fiber. |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | |
Solvay RHODACAL® DSB Surfactant Identification: SODIUM ALKYL DIPHENYL OXIDE SULFONATECAS: 28519-02-0Polarity: Strongly AnionicAvailable in: Asia Pacific, Europe, Latin America and North AmericaApplications: RHODACAL DBS is produce.. |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | ISO 1183 |
SABIC Innovative Plastics NORYL LTA5020 PPE+PS Noryl* LTA5020 is an unfilled, injection moldable grade. Designed for improved long term heat aging, this resin also uses non-chlorinated, non-brominated FR additives to achieve a V0 UL94 rating. No.. |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | ISO R 1183 |
Schwartz Technical Plastics OPTAMID® Cast Polyamide 6, Conditioned Application: deflection rope sheaves for elevatorsInformation provided by Schwartz Technical Plastics GmbH |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | ASTM D792 |
Lubrizol Pellethane® 2363-55D Thermoplastic Polyurethane Elastomer Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | DIN 53479 |
Polyram PlusTek PB507 Nylon 6, Flame Retardant Flame retardant halogen free polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | ISO 1183 |
Polyram Polytron P60B08-S Polypropylene, 60% Long Glass Fiber Polytron P60B08-S (Single strand) is a chemically coupled polypropylene 60% long glass fiber with extra load of additives for dilution.Information provided by Polyram. |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | ISO 1183 |
Covestro Desmopan® DP 9095AU Polyurethane injection molding gradewith special UV stabilizersvery good hydrolysis and microbial resistancegood wear resistancelow warpargeshort cycle timesApplicationEar-tagsPreprocessingMax. Water content |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | ASTM D792 |
Entec Hypro™ PPC-CC30 Natural Copolymer Polypropylene, 30% Calcium Carbonate Filled Information provided by Entec |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | ISO 1183 |
Eurotec® Tecomid® NT40 NL MB PPA, impact modified, heat stabilized, natural Information provided by Eurotec® |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
Arlon 51576R015A 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone RubberInterleave: Polyethylene This data represents typical values for the production mate.. |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
Arlon 930-10Bxx-P0 0.030" (0.762 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 30 mil thick, Black, Rectangular cross-section, Self-fu.. |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | ASTM D792 |
Plastics Group Polifil® T-30 30% Talc-Reinforced Polypropylene Polifil® T series compounds are homopolymer polypropylene resins reinforced with asbestos-free talc. They possess high flex modulus, high deflection temperature, good chemical resistance and colora.. |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | ISO 1183 |
DSM Arnitel® EB464 Polyether Ester Elastomer (European and Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | |
DuPont Performance Polymers Zytel® 70G25HSLR NC010 Nylon 66
(Unverified Data**) 25% Glass Reinforced Heat Stabilized Hydrolysis Resistant Polyamide 66 Zytel 70G25HSLR NC010 is a 25% glass fiber reinforced heat stabilized hydrolysis resistant polyamide 66 resin for injection mol.. |
|||
Density | 1.15 - 1.20 g/cc | 0.0415 - 0.0434 lb/in³ | Average value: 1.18 g/cc Grade Count:14 |
Overview of materials for Acrylic, UV Stabilized, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, UV Stabilized, Molded". Each property range of values reported is minimum and maximum values of.. |
|||
Density | 1.15 g/cc | 0.0415 lb/in³ | |
Plastcom SLOVALEN PH 69 GF 40 PP, 40% glass fibre, mod. of mech. properties FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 40% glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP... |