Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.10 - 1.20 g/cc | 0.0397 - 0.0434 lb/in³ | |
Prodways PLASTCure Cast 200 3D Printing Polymer Good reactivity and low viscosity. Outstanding burnout properties with nearly zero ash content.Highly suitable for direct investment casting or dental applications.Information provided by Genistar. |
|||
Density | 1.10 - 3.80 g/cc | 0.0397 - 0.137 lb/in³ | Average value: 1.49 g/cc Grade Count:605 |
Overview of materials for Polyphthalamide (PPA) This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Density | 1.10 g/cc | 0.0397 lb/in³ | ISO 1183 |
Nilit FRIANYL B63 D-S10 Nylon 6., std. viscosity for injection molding Nylon 6., std. viscosity for injection molding, permanently flexible, increased dry impact resistance (for dowels).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Density | 1.10 g/cc | 0.0397 lb/in³ | ASTM D792 |
Techmer ES Electrablend® ABS 03010 Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: ESD Protection and Good MoldabilityInformation provided by TP Composites, Inc. |
|||
Density | 1.10 g/cc | 0.0397 lb/in³ | |
Solvay IGEPAL® CA 897 Surfactant Chemical Name: ETHOXYLATED OCTYLPHENOL, BRANCHED (40) CAS: 9002-93-1; 7732-18-5 Available in: Asia Pacific, Europe, Latin America and North AmericaApplications: IGEPAL© CA-897 is an excellent pri.. |
|||
Density | 1.10 g/cc | 0.0397 lb/in³ | ISO 1183 |
SABIC Innovative Plastics NORYL GTX GTX918W PPE+PA (Europe-Africa-Middle East) NORYL GTX918W is an unfilled global grade, which offers an excellent combination of processability and heat resistance. |
|||
Density | 1.10 g/cc | 0.0397 lb/in³ | ISO R1183 |
Styron Pulse® A20-95 PC/ABS A medium impact strength PC/ABS blend with high heat distortion and excellent processability.Information provided by DowThis product line was spun off from Dow Chemical to Styron in 2010. |
|||
Density | 1.10 g/cc | 0.0397 lb/in³ | ISO 1183 |
Wellman Wellamid® 22LHI6 XE-N Impact Modified Nylon 66, Lubricated & Heat Stabilized Typical Applications: Automotive fasteners, living hinge, head lamp adjustment devices, ink pen components, wire separators, hardware components, window installation clips, safety equipment.Data pro.. |
|||
Density | 1.10 g/cc | 0.0397 lb/in³ | |
Dow FOUNDATIONS 885 High Performance Latex for Carpet Carboxylated Styrene/Acrylate Latex Applications: FOUNDATIONS 885 Latex offers properties not available in standard styrene-butadiene latexes. FOUNDATIONS 885 Latex is a high solids, low VOC acrylic latex that provides outstanding wet.. |
|||
Density | 1.10 g/cc | 0.0397 lb/in³ | ISO 1183 |
Eurostar Starpylen HT 25 MC PP, Mineral Filled, Injection Molding Starpylen HT 25 MC is a Mineral Filled Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Density | 1.10 g/cc | 0.0397 lb/in³ | ASTM D792 |
Covestro Bayflex® WR-20 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System 0.118 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of.. |
|||
Density | 1.10 g/cc | 0.0397 lb/in³ | ISO 1183 |
DuPont Performance Polymers Hytrel® PC948 NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester Elastomer Developed for the Healthcare Industry Hytrel SC948 NC010 is a low modulus grade with nom. durometer hardness of 40D contains non-discoloring stabilize.. |
|||
Density | 1.10 g/cc | 0.0397 lb/in³ | |
Arkema Group Rilsan® ASR 20 Nylon 12, 20% Carbon Fiber Filled (Conditioned) Designation ISO 1874-PA12,M,16-090,CF20Rigid grade with carbon fiber filler (20%) for injection molding. Available color: black. High strength-to-weight ratio. Very low shrinkage: include 0,5% on av.. |
|||
Density | 1.10 g/cc | 0.0397 lb/in³ | ASTM D792 |
Aclo Accutech Polypropylene Copolymer CP0437G5M25CL Glass/Mineral Reinforced Coupled |
|||
Density | 1.10 g/cc | 0.0397 lb/in³ | Silicone Property; Arlon SQA-TMS-024 |
Arlon R30960T030 0.030" (0.762 mm) Uncured Silicone Rubber with Kodacel Substrate Design/Construction:Interleave: PolyethyleneAdd-on: Uncured Silicone Rubber Substrate: Kodacel CarrierAppearance: Translucent, high viscosity gum on release linersThis data represents typical values.. |
|||
Density | 1.10 g/cc | 0.0397 lb/in³ | ISO 1183 |
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, DAM Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4.. |
|||
Density | 1.10 - 1.14 g/cc | 0.0397 - 0.0412 lb/in³ | Average value: 1.13 g/cc Grade Count:28 |
Overview of materials for Nylon 6, Nucleated This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Nucleated". Each property range of values reported is minimum and maximum values of appropriate.. |
|||
Density | 1.10 g/cc | 0.0397 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Amodel® EXT-1800 Polyphthalamide, extrusion
(discontinued **) AMODEL EXT-1800 was developed specifically for the extrusion process. Unlike the grades targeted for injection molding, AMODEL EXT-1800 resin can be successfully extruded into tube, pipe, sheet, fil.. |
|||
Density | 1.10 g/cc | 0.0397 lb/in³ | ASTM D792 |
Polymer Resources PPX-FR4 Modified PPO, UL 94 V-1 with HDT of 185 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Density | 1.10 g/cc | 0.0397 lb/in³ | |
Solvay MACKAM® 2CYSF Surfactant Product Description: Mackam 2CYSF is a low foaming surfactant suggested for systems where sodium chloride would be detrimental to performance or cause corrosion problems. Mackam 2CYSF is soluble and.. |
|||
Density | 1.10 g/cc | 0.0397 lb/in³ | |
Loctite® 5182 Flexible Cure Anaerobic Sealant Anaerobic GasketingLoctite® 5182 Flexible Cure Anaerobic SealantRecommended Primer: 7649 (N). Typical Use: Robotic application on flanges, seals, covers |