Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.07 g/cc | 0.0387 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Cycolac® MG8000SR ABS This data was supplied by SABIC-IP for the Americas region. |
|||
Density | 1.07 g/cc | 0.0387 lb/in³ | ASTM D792 |
PTS SAN-80HF High Flow SAN Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Density | 1.07 g/cc | 0.0387 lb/in³ | ASTM D792 |
Advanced Elastomer Systems VistaFlex® 715-N Thermoplastic Rubber
(discontinued **) Description: A black high-flow thermoplastic elastomer especially designed for injection molding applications. It replaces soft thermoplastics such as SBS, SEBS, and PVC blends. Supplied as free-f.. |
|||
Density | 1.07 g/cc | 0.0387 lb/in³ | ISO 1183 |
SABIC Innovative Plastics GELOY CR7500 ASA (Europe-Africa-Middle East) High heat ASA with optimum flow-impact balance. For Automotive applications and Automotive colors only. |
|||
Density | 1.07 g/cc | 0.0387 lb/in³ | DAM; ASTM D792 |
Ravago Manufacturing Americas Hylon® N1000STHL Nylon 6/6 (Cond) Information provided by Ravago |
|||
Density | 1.07 g/cc | 0.0387 lb/in³ | ASTM D792 |
Huntsman KRYSTALFLEX® PE 399 Polyurethane Optical Aliphatic Film Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers |
|||
Density | 1.07 g/cc | 0.0387 lb/in³ | ASTM D792 |
Huntsman KRYSTALFLEX® PE 499 Polyurethane Optical Aliphatic Film Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers |
|||
Density | 1.07 - 1.08 g/cc | 0.0387 - 0.0390 lb/in³ | |
Guarniflon TENFIL TF 200 Polytetrafluoroethylene Thread Sealant TENFIL TF200 is a PTFE-based thread sealant in water dispersion, which increases the tightness of the threaded parts and prevents leakage of water. The product is intended for the assembly of fitti.. |
|||
Density | 1.07 g/cc | 0.0387 lb/in³ | ASTM D792 |
LG Chemical 95HC SAN Resin Heat and chemical resistance, Good mechanical properties, Excellent processability, Superior transparency, Good dimensional stability, Applications include make-up cases and other products requiring.. |
|||
Density | 1.07 g/cc | 0.0387 lb/in³ | ASTM D792 |
Techmer ES Electrafil® PS-31/EC BK Polystyrene, Electrically Conductive Carbon Black |
|||
Density | 1.07 g/cc | 0.0387 lb/in³ | ASTM D792 |
Techmer ES HiFill® ABS GF5 5% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 5% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Density | 1.07 g/cc | 0.0387 lb/in³ | dry; ISO 1183 |
Styrolution Terblend® N NM-11 ABS/PA6 (Conditioned) Terblend N NM-11 is an ABS/PA6 blend combining very high impact strength, even at low temperatures, with an excellent processability and surface appearance.Information provided by STYROLUTION, which.. |
|||
Density | 1.07 g/cc | 0.0387 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Noryl PX0346 PPE+PS This data was supplied by SABIC-IP for the Americas region. |
|||
Density | 1.07 g/cc | 0.0387 lb/in³ | ASTM D792 |
PlastxWorld CEVIAN®-N 055 SAN resin These are typical values and are not intended for specification purposes. UL approved file No. is E142893. Information provided by PlastxWorld Inc. |
|||
Density | 1.07 g/cc | 0.0387 lb/in³ | ASTM D792 |
PlastxWorld CEVIAN®-V T180 ABS High Modulus ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Density | 1.07 g/cc | 0.0387 lb/in³ | ASTM D792 |
Tipco Tipcolene® FPC 20 HG - 20% Calcium Carbonate Reinforced, High Gloss Polypropylene Homopolymer 20% Calcium Carbonate Filled PP Homopolymer with High GlossApplications: Furniture & AppliancesProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Density | 1.07 g/cc | 0.0387 lb/in³ | ISO 1183 |
Tisan TISLAMID® 66 Impact Modified Nylon 66 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Density | 1.07 g/cc | 0.0387 lb/in³ | ISO 1183 |
Denka MALECCA K-200 ABS A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de.. |
|||
Density | 1.07 g/cc | 0.0387 lb/in³ | ISO 1183 |
Chi Mei Polylac® PA-777E ABS - High Heat Ultra High Heat |
|||
Density | 1.07 g/cc | 0.0387 lb/in³ | |
Arkema Group Pebax® MV 1074 Polyether Block Amide (PEBA) Typical application: Breathable filmInformation provided by Arkema Group |
|||
Density | 1.07 g/cc | 0.0387 lb/in³ | |
Arkema Group Rilsan® AESN G9 T6L Nylon 12, Graphite Filled (Dry) Designation ISO 1874-PA12,EHLS,22-010,CD10Rigid grade with graphite fillers for extrusion. Available color: steel gray. Reinforced light and heat stabilizing agents.Very low friction coefficient. No.. |
|||
Density | 1.07 g/cc | 0.0387 lb/in³ | |
BASF 1,6-Dichlorohexane Formula: C6H12Cl2CAS: 2163-00-0Description: Dichlorohexane is a colorless to yellowish liquid with an aromatic odor. Synonyms: 1,6-DichlorohexaneApplications: It is used as a Fragrances, Cosmetics, .. |
|||
Density | 1.07 g/cc | 0.0387 lb/in³ | ASTM D792 |
Ashley Polymers Ashlene® 733LD Nylon 6 A modified injection molding grade nylon for applications requiring flexibility.Data provided by the manufacturer |
|||
Density | 1.07 g/cc | 0.0387 lb/in³ | ASTM D792 |
Toyobo PELPRENE™ P40B Polyester TPE Features: Polyester TPEInformation provided by Toyobo. |
|||
Density | 1.07 g/cc | 0.0387 lb/in³ | Sintered; ASTM D792 |
ALM PA 601-CF Filled Nylon 12 Prototyping Polymer Carbon fiber filled nylon 12 easy to process, strong light weight filled material.Low density, good dimensional stability while maintaining excellent mechanical properties.Fibers have been optimized.. |
|||
Density | 1.07 g/cc | 0.0387 lb/in³ | |
Solvay RHODAFAC® RS-710 E Surfactant Identification: POLYOXYETHYLENE TRIDECYL PHOSPHATE ESTERCAS: 9046 – 01 – 9Solubility: Soluble in water and most polar and aromatic solvents.Available in: Asia Pacific, Europe, Latin America and No.. |
|||
Density | 1.07 - 1.07 g/cc @Temperature 270 - 270 °C |
0.0387 - 0.0387 lb/in³ @Temperature 518 - 518 °F |
Average value: 1.07 g/cc Grade Count:1 |
Overview of materials for Nylon 6, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Glass Fiber Filled".Specific grades with glass content between 15% and 24% are included. Ea.. |
|||
Density | 1.07 - 1.70 g/cc | 0.0387 - 0.0614 lb/in³ | Average value: 1.24 g/cc Grade Count:20 |
Overview of materials for Chlorosulfonated Polyethylene Rubber This property data is a summary of similar materials in the MatWeb database for the category "Chlorosulfonated Polyethylene Rubber". Each property range of values reported is minimum and maximum val.. |