Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.068 g/cc | 0.03858 lb/in³ | |
Saint-Gobain Chemfab® 2 Porous PTFE-Coated Glass Description: Chemfab® Porous Series products are lightweight, highly porous materials commonly used as a release (non-stick) layer for composite curing, molding, and other processes that "off-gas.. |
|||
Density | 1.068 g/cc | 0.03858 lb/in³ | |
Cyclewood Solutions Xylomer™ XM2-FPC Sustainable Injection Molding Resin 100% biodegradable and compostable thermoplastic. The sustainable bio-based resin properties perform between polypropylene and polystyrene. Xylomer™ is modified lignin, an abundant, natural bypro.. |
|||
Density | 1.068 g/cc | 0.03858 lb/in³ | |
Dow Glycidyl Methacrylate Glycidyl Methacrylate For Aliphatic Epoxy Polymers (Clear, colorless liquid)Information provided by Dow |