Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.043 g/cc | 0.03768 lb/in³ | |
Lucite International Elvacite ® 2550 Acrylic Resin Elvacite® 2550 is a solid bead methacrylate copolymer resin. It is designed to provide excellent adhesion to metal surfaces and is a resin with good flexibility and medium molecular weight. As su.. |
|||
Density | 1.043 g/cc | 0.03768 lb/in³ | ISO 1183 |
Styrolution Polystyrol 143 E GR 2 PS Description: Polystyrol 143 E is a medium strength, easy flowing general purpose grade, suitable for blending with impact modified Polystyrol, Styrolux and coextruded gloss layers.Applications: In b.. |
|||
Density | 1.043 g/cc | 0.03768 lb/in³ | ISO 1183 |
Styrolution Polystyrol 143 E GR 21 PS Description: Polystyrol 143 E is a medium strength, easy flowing general purpose grade, suitable for blending with impact modified Polystyrol, Styrolux and coextruded gloss layers.Applications: In b.. |
|||
Density | 1.043 g/cc | 0.03768 lb/in³ | |
BASF N-Vinyl-2-pyrrolidone, Non-Stabilized Formula: C6H9NOCAS: 88-12-0Description: Vinyl pyrrolidone is a colorless to yellowish liquid, with a characteristic odor. It is miscible in water and organic solvents.Synonyms: N-Vinylpyrrolidone, .. |
|||
Density | 1.043 g/cc | 0.03768 lb/in³ | ASTM D792-ISO 1183 |
DuPont Surlyn® SURSG201UG
(discontinued **) Surlyn Reflections® SG201UG is a modified ionomer resin for applications that require a high gloss, molded in color surface finish directly from the mold. The material is weatherable, durable and p.. |