Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.990 g/cc | 0.0358 lb/in³ | ASTM D792 |
Mytex Polymers AS33L-16 Polypropylene, Rubber modified, Talc filled, Compounded Description: AS33L-16 is a compounded, talc, rubber modified polypropylene for exterior automotive applications. Material has outstanding moldability and excellent balance of high stiffness and goo.. |
|||
Density | 0.990 - 2.26 g/cc | 0.0358 - 0.0816 lb/in³ | Average value: 1.28 g/cc Grade Count:31 |
Overview of materials for Epoxy, High Temperature This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Mineral Filled". Each property range of values reported is minimum and maximum val.. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ISO 1183 |
Lucobit Lucofin® 1410 Polyolefin TPO Granules, Grey Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ISO 1183 |
Lucobit Lucofin® 1411 Polyolefin TPO Granules, White Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ISO 1183 |
Lucobit Lucofin® 1414 Polyolefin TPO Granules, Silk Grey Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ISO 1183 |
Lucobit Lucofin® 1453 Polyolefin TPO Granules, Red Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ISO 1183 |
Lucobit Lucofin® 1454 Polyolefin TPO Granules, Green Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ISO 1183 |
Lucobit Lucofin® 1452 Polyolefin TPO Granules, Blue Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ISO 1183 |
Lucobit Lucofin® 1455 P Polyolefin TPO Granules, Black Lucofin is a colored, highly stabilized, bitumen-free TPO raw material based on polyolefins. Lucofin products display excellent tear resistance, flexibility, and weathering resistance. Lucofin exhi.. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ASTM D 792 |
SABIC Innovative Plastics LNP Lubricomp FX00617 PE (Asia Pacific) LNP* Lubricomp* FX00617 is a compound based on Polyethylene resin containing Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia.. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ISO 1183 |
SABIC Innovative Plastics SABIC PPCOMPOUND 7727 PP SABIC® PPcompound 7727 is a mineral filled, impact modified polypropylene TPO. This material combines impact resistance, heat stability, and is used in injection molded applications. The IMDS ID.. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | |
Solvay ALKAMULS® VO/2003 Surfactant Identification: MIXTURE OF FATTY ACID POLYETHYLENE GLYCOL ESTERSCAS: 220037 – 02 – 5Solubility: Dispersible in water, soluble in most polar and aromatic solventsAvailable in: Asia Pacific,.. |
|||
Density | 0.990 - 1.03 g/cc | 0.0358 - 0.0372 lb/in³ | AV15 |
Solvay Duraphos Octyl Acid Phosphate Surfactant Identification: DI(N-OCTYL) PHOSPHORIC ACID, N-OCTYL PHOSPHORIC ACID, PHOSPHORIC ACID CAS: 3115-39-7; 3991-73-9; 7664-38-2Solublility: Soluble in common organic solvents and slightly soluble in wate.. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ISO 1183 |
SABIC Innovative Plastics NORYL PPX PPX7200 PPE+PP+PS PP+PPE+PS. Improved chemical resistance and surface aesthetics in injection molded applications. NSF61-capable. UL-94 HB listed. |
|||
Density | 0.990 - 1.01 g/cc @Temperature 20.0 °C |
0.0358 - 0.0365 lb/in³ @Temperature 68.0 °F |
|
Silikony Polskie Polsil E1 Silicone Emulsion POLSIL® E – water emulsions of POLSIL® OM methylsilicone fluid. These are milky-white liquids easily mixed with water, smooth to touch, with a specific smell. They are chemically inert. .. |
|||
Density | 0.990 - 1.01 g/cc @Temperature 20.0 °C |
0.0358 - 0.0365 lb/in³ @Temperature 68.0 °F |
|
Silikony Polskie Polsil E2 Silicone Emulsion POLSIL® E – water emulsions of POLSIL® OM methylsilicone fluid. These are milky-white liquids easily mixed with water, smooth to touch, with a specific smell. They are chemically inert. .. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | |
Solvay RHODASURF® 860/P Surfactant Identification: ETHOXYLATED ISODECYL ALCOHOLCAS: 78330 – 20 – 8Available in: Asia Pacific, Europe, Latin America and North AmericaSolubility: Soluble in water and most polar and aromatic s.. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ISO 1183 |
Borealis Daplen™ EE115AE TPO Compound Daplen EE115AE is a 10% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EE115AE is a material with excellent impact /stiffness ratio. Thanks to its low .. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ISO 1183 |
Borealis Daplen™ EE115T TPO Compound Daplen EE115T is a 10% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EE115T is a material with excellent impact /stiffness ratio. Thanks to its low th.. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ASTM D792 |
UBE UBESTA® 3030JI7 Plasticized Industrial Grade Nylon 12 Description: UBE UBESTA® Industrial grade Nylon 12Comments: low migrationInformation provided by UBE. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ASTM D792 |
Tipco Tipcolene® SEB 100 - 10% Chemically Coupled Glass Fiber Polypropylene Homopolymer with High Heat Stability 10% Chemically Coupled Glass Reinforced PP HomopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ASTM D792 |
Tipco Tipcolene® UV 1022 - Polymeric-HALS (20% UV Stabilizer) Masterbatch in Polypropylene Homopolymer |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ASTM D 792 |
Cossa Polimeri ESTAPROP 1040 V2 K Flame Retardant Polypropylene PP copolymerFlame retardant class V2, halogen free, good mechanical characteristicsInformation provided by Cossa Polimeri S.r.l. |
|||
Density | 0.990 g/cc @Temperature 15.6 °C |
0.0358 lb/in³ @Temperature 60.0 °F |
ASTM D4052 |
ExxonMobil Solvesso™ Aromatic 200 Aromatic Fluid Appearance: Clear/Transparent LiquidAvailability: North AmericaInformation provided by ExxonMobil |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ISO 1183 |
Eurotec® Tecolen® CP10 GR15 NL PPCP, 15% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | |
BASF 1,5-Pentanediol (PDO) Formula: C5H12O2CAS: 111-29-5Description: 1,5-Pentanediol (PDO) is a colorless, oily liquid with characteristic odor. It is miscible in water and organic solvents.Synonyms: 1,5-Dihydroxypentane, 1,5.. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | |
BASF Lupragen® DMI 1,2-Dimethyl Imidazole Formula: C5H8N2CAS: 1739-81-0Description: 1,2-Dimethylimidazole is a colorless to yellowish solid with an amine-like odor. Synonyms: DMI, 1,2-Dimethyl-1H-imidazolApplications: It is used as a Cataly.. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | ISO R 1183 D |
Arkema Group Rilsan® Clear G350 Polyamide Rilsan® Clear G350 is a high performance transparent polyamide. This grade has been specially designed for injection molding applications, ideally suited for optics as high end eyewear frames.Infor.. |
|||
Density | 0.990 g/cc | 0.0358 lb/in³ | DIN 53479 |
Polyram RamOfin PPC300S4BK10 Polypropylene, 20% Glass beads 20% glass beads reinforced polypropylene copolymer for injection molding applicationsInformation provided by Polyram Ram On Ind. |