Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.986 g/cc | 0.0356 lb/in³ | Mixed |
ITW Plexus Plexusâ„¢ MA1020 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low shrinkage, low odor, all purpose.Information provided by Illinois Tool Works. |
|||
Density | 0.986 g/cc | 0.0356 lb/in³ | Mixed |
ITW Plexus Plexusâ„¢ MA1021 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, low shrinkage.Information provided by Illinois Tool Works. |
|||
Density | 0.986 g/cc | 0.0356 lb/in³ | Mixed |
ITW Plexus Plexusâ„¢ MA1023 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low shrinkage, low odor, all purpose.Information provided by Illinois Tool Works. |
|||
Density | 0.986 g/cc | 0.0356 lb/in³ | Mixed |
ITW Plexus Plexusâ„¢ MA1025 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Low shrinkage, low odor, able to be used 1" thick.Information provided by Illinois Tool Works. |