Polymer Property : Density = 0.9852 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.9852 g/cc
0.03559 lb/in³
Finaprene 2602 Test
Total Finaprene® 602 Styrene-Butadiene TPE Copolymer Compound, Formulated to 57 Shore A  (discontinued **)
Styrene-Butadiene CopolymerDescription: Finaprene® 602 is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its broad molecular weight distribution, Finaprene® 60..
Density 0.9852 g/cc
0.03559 lb/in³
Finaprene 2602 Test
Total Finaprene® 602 Styrene-Butadiene TPE Copolymer Compound, Formulated to 62 Shore A  (discontinued **)
Styrene-Butadiene CopolymerDescription: Finaprene® 602 is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its broad molecular weight distribution, Finaprene® 60..