Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.965 g/cc | 0.0349 lb/in³ | ASTM D1505 |
Petromont 3000 High Density Polyethylene Resin Petromont HDPE 3000 is a high density polyethylene resin produced using the UNIPOL® Process. This resin is designed for injection moulding applications such as crates, cases, trays, tote bins and o.. |
|||
Density | 0.965 g/cc | 0.0349 lb/in³ | ASTM D4883 |
ExxonMobil Escorene® HD-6908 HDPE, Injection Grade
(discontinued **) Data Provided by Exxon Chemical Canada.Characteristics: Excellent Stiffness, Good ImpactUses: Crates, Pails, Industrial containers |
|||
Density | 0.965 g/cc | 0.0349 lb/in³ | ASTM D4883 |
ExxonMobil HD 6908.18 Injection Molding Resin
(discontinued **) HD 6908 is a homopolymer with outstanding stiffness with a good balance of processability and cold temperature impact performance. This resin is ideally suited for articles requiring very high stif.. |
|||
Density | 0.965 g/cc | 0.0349 lb/in³ | ASTM D1505 |
LyondellBasell Alathon® H6030 High Density Polyethylene ApplicationsALATHON H 6030 is a homopolymer that provides enhanced processability, excellent stiffness and short molding cycles. Typical applications include thin wall and deep-drawRegulatory Statu.. |
|||
Density | 0.965 g/cc | 0.0349 lb/in³ | ASTM D1505 |
LyondellBasell Alathon® M6580 High Density Polyethylene ApplicationsALATHON M 6580 is a narrow molecular weight distribution homopolymer that enhances processability and stiffness, exhibits excellent color, low odor and good processing stability. Typica.. |
|||
Density | 0.965 g/cc | 0.0348 lb/in³ | Mixed |
ITW Plexus Plexusâ„¢ MA425 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive, long open time.Information provided by Illinois Tool Works. |
|||
Density | 0.965 g/cc | 0.0349 lb/in³ | ASTM D792B; ISO 1183 |
Styron INSPIREâ„¢ TF1301 Thermoplastic Polyolefin Information provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010 |
|||
Density | 0.965 g/cc | 0.0349 lb/in³ | |
Solvay MACKAMINE® C-8 Surfactant Product Description: Mackamine C-8 is a pure octyldimethylamine oxide that provides good wetting and very low foaming characteristics. It is compatible with most surfactants and because there are no.. |
|||
Density | 0.965 g/cc | 0.0349 lb/in³ | ASTM D1505 |
DuPont Elvax® 40W Ethylene-Vinyl Acetate Copolymer Resin Elvax® 40W has a higher vinyl acetate content compared with the other Elvax® resins resulting in higher elongation, reduced hardness, improved solubility and adhesion, and significant differences .. |
|||
Density | 0.965 g/cc | 0.0349 lb/in³ | ISO 1183 |
Borealis BS4641 High Density Polyethylene BS4641 is a bimodal high-density polyethylene homopolymer. Because of its excellent organoleptic properties, this grade is especially suitable for blow molding of bottles for food applications. App.. |
|||
Density | 0.965 g/cc | 0.0349 lb/in³ | ExxonMobil method |
ExxonMobil HDPE HD 6909.19 High Density Polyethylene Copolymer Resin Product Description: HD 6908 is a homopolymer with outstanding stiffness with a good balance of processability and cold temperature impact performance. This resin is ideally suited for articles requ.. |
|||
Density | 0.965 g/cc | 0.0349 lb/in³ | ExxonMobil method |
ExxonMobil HDPE HD 6909.65 High Density Polyethylene Copolymer Resin Product Description: HD 6908 is a homopolymer with outstanding stiffness with a good balance of processability and cold temperature impact performance. This resin is ideally suited for articles requ.. |
|||
Density | 0.965 g/cc | 0.0349 lb/in³ | ExxonMobil method |
ExxonMobil HDPE HD 7925.30 High Density Polyethylene Resin Product Description: HD 7925.30 is a medium molecular weight HDPE homopolymer for use in blown and cast film applications. Typical applications include those with low WVTR and clarity requirements.A.. |
|||
Density | 0.965 - 0.970 g/cc | 0.0349 - 0.0350 lb/in³ | BRCP 4843 |
ExxonMobil Jayflex™ DIDP Plasticizer Appearance: Clear and FreeAvailability: AmericasCAS Number: 68515-49-1Information provided by ExxonMobil |
|||
Density | 0.965 - 0.970 g/cc | 0.0349 - 0.0350 lb/in³ | BRCP 4843 |
ExxonMobil Jayflex™ DIDP-E Plasticizer Appearance: Clear and FreeAvailability: AmericasCAS Number: 68515-49-1Information provided by ExxonMobil |
|||
Density | 0.965 g/cc | 0.0349 lb/in³ | ASTM D792 |
Dow DMDA-8007 NT 7 High Density Polyethylene Resin DOW DMDA-8007 NT is a narrow molecular weight distribution high density homopolymer designed to offer excellent stiffness, low warpage, good/acceptable toughness, and good mold-ability. This resin .. |
|||
Density | 0.965 g/cc | 0.0349 lb/in³ | ASTM D792 |
Aclo Accutech Polypropylene Homopolymer HP0336W10L Wollastonite Reinforced |
|||
Density | 0.965 g/cc | 0.0348 lb/in³ | Mixed |
ITW Plexus Plexus™ MA925 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, low odor, long open time.Information provided by Illinois Tool Works. |
|||
Density | 0.965 g/cc | 0.0349 lb/in³ | ASTM D792 |
Aclo Accutech TPO TPO030T9V Paintable Grade Approved to Suzuki Spec Black B14257 |
|||
Density | 0.965 g/cc | 0.0349 lb/in³ | ASTM D1505 |
Amco PRIMATOP HDPE 006964EG Pipe Extrusion Polyethylene HDPE 006964 features high quality for critical food packaging requirements and excellent stiffness. Applications include milk, water, and juice packaging.Former A-Top Polymers product; part of Amco .. |