Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.962 g/cc | 0.0348 lb/in³ | ASTM D1505 |
Network Polymers NPP 50-1060 Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 19A Homopolymer HDPE Film Resin Film Properties.Data provided by the manufacturer. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 2909 HDPE Injection Molding Resin High stiffness, Maximum impact strength and toughness, Good top loading capability, High surface glossApplications: Tote boxes, Beverage cratesAdditives: Antioxidant, Ultraviolet light stabilizersIn.. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 59A HDPE Injection Molding Resin Features: Homopolymer, high drop impact resistance and high stiffness.Applications: Juice, water containers, personal protective equipment, grain elevator buckets, designed for accumulator and recip.. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ASTM D1505 |
Chevron Phillips HiD® 9605D HDPE Cast Film Resin
(discontinued **) Characteristics: Very Low Gel Levels, Produces Very "Clear" Film, Draws to Thin Gauges, Low Taste and Odor Transfer, Excellent MVTR for a Chill Cast Film, Excellent Processability, Excellent Optical.. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ASTM D1505 |
Chevron Phillips HiD® 9607D HDPE Cast Film Resin
(discontinued **) Characteristics: Very Low Gel Levels, Produces Very "Clear" Film, Draws to Thin Gauges, Low Taste and Odor Transfer, Excellent MVTR for a Chill Cast Film, Excellent Processability, Excellent Optical.. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ASTM D1505 |
Chevron Phillips MarFlex® 9607XD HDPE Cast Film Resin
(discontinued **) Characteristics: Very Low Gel Levels, Produces Very "Clear" Film, Draws to Thin Gauges, Low Taste and Odor Transfer, Excellent MVTR for a Chill Cast Film, Excellent Processability, Excellent Optical.. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ASTM D1505 |
Chevron Phillips HiD® 9662 HDPE Blown Film Resin
(discontinued **) Resin Type: Linear Polyethylene HomopolymerCharacteristics: Unique Molecular Architecture Gives Outstanding Moisture Barrier Properties, Excellent Film Strength and Toughness for a Homopolymer, Give.. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ASTM D4883 |
Chevron Phillips HiD® 9706 HDPE Injection Molding Resin
(discontinued **) Resin Type: linear homopolymerCharacteristics: moderate flow, good impact strength, excellent stiffness, good ESCR, moderate shrinkage resistanceApplications: crates and totes, structural foamInform.. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ASTM D4883 |
Chevron Phillips HiD® 9720 HDPE Injection Molding Resin
(discontinued **) Resin Type: linear homopolymerCharacteristics: good flow, moderate impact strength, excellent stiffness, moderate ESCR, moderate shrinkage resistanceApplications: pails, structural foamInformation p.. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 69A HDPE Extrusion Resin
(discontinued **) Features: High tensile strength, better moisture barrier, better oil and solvent resistance, lower friction coefficient, lower brittleness temperature, better abrasion resistance, better temperature.. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ASTM D792 |
Entec Hypel® PEHD.8/.962 HDPE
(discontinued **) Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Density | 0.962 - 1.54 g/cc | 0.0348 - 0.0555 lb/in³ | Average value: 1.29 g/cc Grade Count:107 |
Overview of materials for Polycarbonate/ABS Alloy, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Glass Fiber Filled". Each property range of values reported is minimum and maxi.. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ASTM D 792 |
NOVA Chemicals Sclair® 99K Homopolymer HDPE Film Resin 99K complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, without te.. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ASTM D1505 |
Braskem BT 003 HDPE Blow Molding Polyethylene
(discontinued **) Applications: Bottles for food products, lubricating and cooking oil; toys; bottler for surface-active agents; sheets. Information provided by Braskem |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ASTM D1505 |
Global J-2208 High Density Polyethylene Description-industrial injection grade w/ UV stabilizer, good for high impact
strengthApplications-high quality industrial products, outdoor applications such as pallets & cratesInformation provided.. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ASTM D1505 |
Global J-2308 High Density Polyethylene Description-industrial injection grade w/ UV stabilizer, good for high impact
strengthApplications-high quality industrial products, outdoor applications such as pallets & cratesInformation provided.. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ASTM D792 |
IRPC Polimaxx Polene G2865 High Density Polyethylene CHARACTERISTICS: HIGH STIFFNESS, GOOD IMPACT STRENGTH, GOOD PROCESSABILITYAPPLICATIONS: BLOW MOLDING FOR CONTAINERS FROM A FEW ml TO ABOUT 20 LITRES, DIARY PRODUCT BOTTLES, FRUIT JUICE BOTTLES, ONE-.. |
|||
Density | 0.962 g/cc @Temperature 20.0 °C |
0.0348 lb/in³ @Temperature 68.0 °F |
|
LyondellBasell TPM Tripropylene glycol methyl ether Information provided by Lyondell. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ISO 1183 |
Borealis CG9620 High Density Polyethylene CG9620 is a high density polyethylene film grade which combine excellent extrusion behavior with superior mechanical properties. Applications: CG9620 is recommended for coated film and co-extrusion.. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ISO 1183 |
Borealis MG9621B Polyethylene Applications: crates, and pailsInformation provided by Borealis AG |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ISO 1183 |
Borealis MG9621S Polyethylene MG9621S is a natural high-density polyethylene with a narrow molecular weight distribution, which is produced in a low-pressure gas-phase process. This grade is designed for the injection molding of.. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ASTM D1505 |
Chevron Phillips MarFlex® 9607 HDPE Cast Film Resin Characteristics: Very Low Gel Levels, Produces Very "Clear" Film, Draws to Thin Gauges, Low Taste and Odor Transfer, Excellent MVTR for a Chill Cast Film, Excellent Processability, Excellent Optical.. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ASTM D1505 |
Chevron Phillips MarFlex® 9659 HDPE Blown Film Resin Resin Type: Linear Polyethylene HomopolymerCharacteristics: Unique Molecular Architecture Gives Outstanding Moisture Barrier Properties, Excellent Film Strength and Toughness for a Homopolymer, Give.. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ASTM D792, ISO 1183 |
DuPont™ Fusabond® C250 Polymer Modifier DuPont™ Fusabond® C250 is a modified ethylene vinyl acetate copolymer. Used as an adhesion promoter and coupling agent. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ASTM D1505 |
Chevron Phillips Marlex® 9708 HDPE Injection Molding Resin Resin Type: Linear Homopolymer; ASTM D 4976 Classification: PE 243, A 63700Characteristics: Moderate Flow, Good Impact Strength, Excellent Stiffness, Good ESCR, Moderate Shrinkage ResistanceApplicat.. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | |
Dow HDPE 10462N High Density Polyethylene DOW HDPE 10462N resin is a narrow molecular weight distribution polymer designed to offer good stress crack resistance and impact strength with excellent rigidity. This resin has good processability.. |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ASTM D1505 |
Chevron Phillips Marlex® HMN 6060 Polyethylene, Injection Molding Grade, HDPE
(discontinued **) Meets FDA Regulation 177.1520.Data provided by the manufacturer |
|||
Density | 0.962 g/cc | 0.0348 lb/in³ | ASTM D1505 |
Chevron Phillips MarFlex® 9608XD HDPE Film Grade This HDPE is tailored for applications that require:Very low gel levelsVery "clear" filmExcellent drawdownEnhanced stiffnessExcellent WVTR for a chill cast filmExcellent ProcessibilityTypical Cast F.. |