Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.940 g/cc | 0.0340 lb/in³ | ASTM D792 |
Multibase Multi-Flex® TPE A 7007 BLK Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | ASTM D792 |
Mytex Polymers AS14KW-02 Polypropylene, Talc filled, Compounded Description: Talc filled compounded polypropylene produced for automotive interior applications using Mytex® Technology.Key Applications: General purpose interiorInformation provided by Mytex Polym.. |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | ISO 1183-A |
Okulen® 1000 PE-UHMW, Multi-color OKULEN® 1000 is an ultra high molecular low pressure polyethylene with a molecular weight of < 3.5 g/mol. It has great wear resistance, high impact strength, and excellent sliding properties ideal .. |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | ISO 1183 |
Polykemi AB SCANCOMP PP BN140 T5 Polypropylene Information provided by Polykemi AB |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | Estimated by MatWeb |
DuPont™ Surlyn® 1652SBR Zinc Ionomer Resin for Blown/Cast Film and Extrusion Coating
(discontinued **) Surlyn® 1652SBR is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment and extrusion coating and coextrusion coating equipment designed to pro.. |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | ASTM D1505 |
ICO Polymers ICORENEâ„¢ 115-1654 LMDPE Rotational Molding Resin Description: ICORENE 115-1654 polyethylene developed for use in rotational molding. It is an easy processing material with good surface gloss, scratch resistance and generally balanced physical pro.. |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | ASTM D1505 |
ICO Polymers ICORENEâ„¢ 115-4060 LMDPE Rotational Molding Resin Description: ICORENE 115-4060 is a linear medium density polyethylene developed for use in rotational molding. It is an easy processing material with good surface gloss, scratch resistance and gene.. |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | Not Compounded |
KKPC KOSYN 1507L Styrene Butadiene Rubber Styrene Butadiene RubberCharacteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and.. |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | Yellow; ASTM D4883 |
Ineos TUB 172 HDPE TUB 172 is a yellow medium density polyethylene copolymer designed specifically for the extrusion of natural gas pipe. It exhibits excellent long term stress life and slow crack growth resistance. T.. |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | ASTM D1475 |
Lord Adhesives Chemglaze® V004 Polyurethane Coating Chemglaze® V-Line polyurethane coatings are moisture curing aliphatic polyurethane coatings. They are used in product finishing applications on polyvinyl-chloride (PVC) and other plastics where m.. |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | ASTM D792 |
Multibase Multi-Flex® TPE A 4002 BLK Multi-Flex® A 4002 is based on Shell's Kraton G polymer and is suitable for soft touch applications for the automotive industry. It exhibits excellent paintibility adhesion. Multi-Flex TPE cont.. |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | Not Compounded |
KKPC KOSYN 1507 Styrene Butadiene Rubber Styrene Butadiene RubberCharacteristics: KOSYN SBR, a useful synthetic rubber, is a copolymer made from butadiene and styrene by cold emulsion polymerization. It has superior abrasion resistance and.. |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | Not Compounded |
KKPC KOSYN KNB 35L Acrylonitrile Butadiene Rubber (NBR) Acrylonitrile Butadiene Rubber (NBR)Characteristics: KOSYN KNB is copolymer of high oil resistance and chemical resistance made from acrylonitrile and butadiene by the cold emulsion polymerization. .. |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | Not Compounded |
KKPC KOSYN KNB 40M Acrylonitrile Butadiene Rubber (NBR) Acrylonitrile Butadiene Rubber (NBR)Characteristics: KOSYN KNB is copolymer of high oil resistance and chemical resistance made from acrylonitrile and butadiene by the cold emulsion polymerization. .. |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | ASTM D792 |
Teknor Apex Sarlink® 3190 Thermoplastic Elastomer A medium hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3190 can be processed by blow molding, injection molding or.. |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | ASTM D792, ISO 1183 |
DuPont Elvax® 3165LG Ethylene Vinyl Acetate DuPont™ Elvax® 3165XZ is an extrudable ethylene-vinyl acetate copolymer resin containing low gel material available in pellet form for use in conventional extrusion equipment designed to process p.. |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | ASTM D1505 |
DuPont Elvax® 670 Ethylene Vinyl Acetate DuPont™ Elvax® 670 is an ethylene-vinyl acetate copolymer resin for use in industrial applications.Applications:Elvax® 670 resins can be used for the following applications: molding, compounding .. |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | ASTM D792 |
DuPont Nucrel® 3990 Ethylene-Acrylic Acid Copolymer Resin for Extrusion Coating/Laminating 9 wt% Acrylic Acid.Nucrel® 3990 is an ethylene-acrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment designed to .. |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | D1505 |
Westlake ELEVATE™ EF529 18.5% Ethylene Vinyl Acetate Copolymer Westlake ELEVATE™ EF529 is an ethylene vinyl acetate copolymer with 18.5% VA. It contains no slip or antiblock and is designed for blown and cast films requiring excellent optics and low heat seal .. |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | ASTM D 792 |
Total 3802 YCF MDPE pipe grade FINATHENE® 3802 Y CF is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low pressure slurry polymerization process. FINATHENE® 3802 Y CF is a yellow cadmi.. |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | ASTM D792, ISO 1183 |
DuPont™ Elvax® 3178Z Ethylene Vinyl Acetate DuPont™ Elvax® 3178Z is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. ELVAX® 3.. |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | ASTM D1505 |
Diamond Polymers NPP11-0242 Polyethylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | ASTM D792 |
DuPont™ Surlyn® 7930 Ionomer Resin, Lithium Surlyn® 7930 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with lithium ions. The amount of MAA and ne.. |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | |
Arkema Group Evatane® 1005 VN 5 Ethylene Vinyl Acetate EVA copolymer made by high pressure tubular process. Applications Grade for films with high transparency and high mechanical properties. Examples: coextrusion, stretch film, paper-stationary, fancy .. |
|||
Density | 0.940 g/cc @Temperature 23.0 °C |
0.0340 lb/in³ @Temperature 73.4 °F |
ISO 1183 |
Arkema Group LOTADER® 4700 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride LOTADER 4700 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized under high pressure in an autoclave process. Comonomer content is high. Due to its properties (reacti.. |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | ISO 2781 |
Alliance Polymers Viprene™ P45D-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P45D-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | ASTM D 792 |
Total Lacqtene® 6002 FLG 42 HDPE film
(discontinued **) LACQTENE® 6002 FLG 42 is a medium density polyethylene resin with hexene as comonomer. This shows a broad molecular weight distribution ensuring outstanding processability. LACQTENE® 6002 FLG 42 h.. |
|||
Density | 0.940 g/cc | 0.0340 lb/in³ | ISO 1183 |
Unipetrol PE HD LITEN® ZB 20 HDPE Made for blow molding, extrusion, and pipe applications.Information provided by Unipetrol RPA |