Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.921 - 0.924 g/cc | 0.0333 - 0.0334 lb/in³ | ASTM D1505 |
Petroquimica Triunfo Trithene® SX 7010 LDPE - Blow Molding The Trithene® SX 7010 resin is a medium molecular weight, low-density polyethylene (LDPE) which allows the production of flasks with an adequate combination of mechanical and impact strength, flexi.. |
|||
Density | 0.921 g/cc | 0.0333 lb/in³ | ASTM D792 |
NOVA Chemicals Novapol® PF-Y821-B Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Good stiffness and machinability, good clarity with LDPE.Applications: General purpose packaging, liners.Data provided by the manufacturer. |
|||
Density | 0.921 g/cc | 0.0333 lb/in³ | Exxon Method |
ExxonMobil Escorene® LL-3105 LLDPE/Hexene Premium Film Resin, Tough, 1.2 mil film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3105 have outstanding tensile and toughness properties. The superior strength propert.. |
|||
Density | 0.921 g/cc | 0.0333 lb/in³ | Exxon Method |
ExxonMobil Escorene® LL-3113 LLDPE/Hexene Premium High Strength 1.2 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An LLDPE hexene copolymer film resin. Films made from this resin have outstanding tensile, stiffness and toughness properties. These superior prope.. |
|||
Density | 0.921 g/cc | 0.0333 lb/in³ | ASTM D4883 |
Eastman 1840F Polyethylene
(discontinued **) Polyethylene 1840F is a low-density formulation with no slip or antiblock. It is suggested for film applications where enhanced processability and high clarity are required. It is characterized by.. |
|||
Density | 0.921 g/cc | 0.0333 lb/in³ | ASTM D4883 |
Eastman E6838-014F Polyethylene
(discontinued **) E6838-014F is a low density formulation that contains low slip and medium antiblock levels. It is suggested for film applications that require clarity.List of Applications: Food packagingFood-conta.. |
|||
Density | 0.921 g/cc | 0.0333 lb/in³ | ASTM D4883 |
Eastman E6838-795F Polyethylene
(discontinued **) E6838-795F is a low density formulation with no slip or antiblock level. It is suggested for film applications that require a good balance of properties such as converter film for industrial packag.. |
|||
Density | 0.921 g/cc | 0.0333 lb/in³ | ASTM D4883 |
Eastman E6838-997F Polyethylene
(discontinued **) E6838-997F natural is a low density formulation with no slip or antiblock. Outstanding optical properties make this material an excellent choice for calendering and as a clarity filler in co-extrud.. |
|||
Density | 0.921 g/cc | 0.0333 lb/in³ | ExxonMobil Method |
ExxonMobil LD 102.74 Thin Gauged Film Resin
(discontinued **) LD 102 series are homopolymer, good clarity, laundry and dry cleaning film resins capable of providing a tough film in very thin gaugesInformation provided by ExxonMobil Chemical |
|||
Density | 0.921 g/cc | 0.0333 lb/in³ | Exxon Method |
ExxonMobil Escorene® LD-140 LDPE Industrial Film resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A fractional melt index homopolymer resin for production of film with very good toughness.Applications: Heavy duty bags. Data for film properties b.. |
|||
Density | 0.921 g/cc | 0.0333 lb/in³ | ASTM D1505 |
Global JJ-4324 Low Density Polyethylene, Film Extrusion Grade
(discontinued **) Description-transparency, high toughness, flexibility, high impact strength, good chemical resistanceApplications-bagsMeets FDA requirements as listed in food additives regulation 21 CFR 117.1520 fo.. |
|||
Density | 0.921 g/cc | 0.0333 lb/in³ | ASTM D1505 |
M. Holland Company LD505 LDPE
(discontinued **) Additives: 0.050 % Slip Features: High Flow, Medium GlossUses: Household Goods, ToysProcessing Method: Injection MoldingInformation provided by M. Holland. |
|||
Density | 0.921 - 0.923 g/cc | 0.0333 - 0.0333 lb/in³ | ASTM D1505 |
Petroquimica Triunfo Trithene® TX 7003 LDPE - Heavy Duty and Industrial Film The Trithene® TX 7003 resin is a low-density, high molecular-weight polyethylene that offers high mechanical strength and environmental stress cracking resistance (ESCR). Additionally, this product.. |
|||
Density | 0.921 g/cc | 0.0333 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® NA345196 Low Density Polyethylene (Film Extrusion) ApplicationsPETROTHENE NA 345 is a series of homopolymer resins combining premium clarity with strength and stiffness. In addition, NA 345 exhibits good impact strength on both flat and creased fil.. |
|||
Density | 0.921 g/cc | 0.0333 lb/in³ | ASTM D1505 |
LyondellBasell Plexar® PX3236 Extrudable Tie-Layer Resin - Anhydride Modified LLDPE General DescriptionPLEXAR tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins a.. |
|||
Density | 0.921 g/cc | 0.0333 lb/in³ | TSTM 209 B |
Iran Petrochemical (PCC) LH0075 Low Density Polyethylene LH0075 is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties.Applications: carrier bags, shrink film, industria.. |
|||
Density | 0.921 g/cc | 0.0333 lb/in³ | ASTM D1505 |
Westlake EF923 Low Density Polyethylene Westlake Polyethylene EF923 is a low density formulation suggested for film applications that require a good balance of properties such as converter film for industrial packaging and general purpose.. |
|||
Density | 0.921 g/cc | 0.0333 lb/in³ | ASTM D-1505 |
Chevron Phillips MarFlex® 1125 Polyethylene; LDPE Low density polyethylene. This LDPE is tailored for blown film applications that require: Good impactNo slip, includes antiblockGood processabilityGood sealabilityGood drawdown Applications: Typi.. |
|||
Density | 0.921 g/cc | 0.0333 lb/in³ | ExxonMobil Method |
ExxonMobil LD 201.48 Extrusion Coating for Milk Carton Resin Product Description: LD 201.48 is an LDPE extrusion coating grade, designed to have excellent processability combined with heat sealability and adhesion. It offers – Excellent neck-in/draw down bal.. |
|||
Density | 0.921 g/cc | 0.0333 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 201.48 Low Density Polyethylene Resin Product Description: LD 201.48 is an LDPE extrusion coating grade, designed to have excellent processability combined with heat sealability and adhesion. It offers – Excellent neck-in/draw down bal.. |
|||
Density | 0.921 g/cc | 0.0333 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 419.MV Low Density Polyethylene Resin Product Description: LD 419.MV is a LDPE designed for wire and cable applications and is suitable for making crosslinkable compounds for medium voltage insulation.Availability: Latin America, North .. |
|||
Density | 0.921 g/cc | 0.0333 lb/in³ | |
Dow LDPE 640IM Low Density Polyethylene DOW LDPE 640IM resin is a broad molecular weight distribution homopolymer designed to offer excellent impact strength and stress crack resistance with moderate stiffness for general purpose, and cap.. |
|||
Density | 0.921 g/cc | 0.0333 lb/in³ | ExxonMobil Method |
ExxonMobil LD 419.MV Wire & Cable Resin
(discontinued **) LD 419.MV is a LDPE designed for wire and cable applications and is suitable for making crosslinkable compounds for medium voltage insulation.Information provided by ExxonMobil Chemical |
|||
Density | 0.921 g/cc | 0.0333 lb/in³ | base resin; ISO 1183 |
Borealis LE6025 Polyethylene Modified Jacketing Compound LE6025 is a black low density copolymer modified polyethylene compound. It is characterized by excellent stress crack resistance and mechanical properties and low temperature performance in combinat.. |
|||
Density | 0.921 g/cc | 0.0333 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 11B4 Octene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, excellent seal characteristics, easy processability.Applications: Specialty lamination, co-extrusion.Data provided by the manufacturer. |
|||
Density | 0.921 g/cc | 0.0333 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 11E1 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, strength and toughness.Applications: Base resin.Data provided by the manufacturer. |
|||
Density | 0.921 g/cc | 0.0333 lb/in³ | ASTM D4883 |
Eastman E6838-963F Polyethylene
(discontinued **) E6838-963F is a low density formulation with medium slip and medium antiblock. It is suggested for film applications that require a good balance of physical and optical properties.List of Applicati.. |
|||
Density | 0.921 g/cc | 0.0333 lb/in³ | ASTM D4883 |
Eastman E6838-975F Polyethylene
(discontinued **) E6838-975F is a low density formulation with medium slip and medium antiblock. The formula is used in general purpose packaging where impact strength and processability are important. End-use film.. |