Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.919 g/cc | 0.0332 lb/in³ | ASTM D792 |
NOVA Chemicals Novapol® LA-0219-AM LDPE Foam Resin Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Industrial packaging, Liners, Blends with LLDPE, Foam articlesAdditives: Base resinFilm properties are typical of blo.. |
|||
Density | 0.919 g/cc | 0.0332 lb/in³ | ASTM D792 |
NOVA Chemicals Novapol® LF-0219-A LDPE Blow Molding Resin Good heat sealing latitude, Easy processabilityApplications: Food contact, Squeeze bottles, Non-ESCRAdditives: Base resinInformation provided by NOVA Chemicals. |
|||
Density | 0.919 g/cc | 0.0332 lb/in³ | ASTM D792 |
NOVA Chemicals Novapol® LF-0219-D LDPE Film Resin Film Properties. Features: Good heat sealing latitude, moderate toughness, easy processability.Applications: Liners, industrial packaging, blends with LLDPE.Data provided by the manufacturer. |
|||
Density | 0.919 g/cc | 0.0332 lb/in³ | ASTM D 792 |
NOVA Chemicals Sclair® FP619-A Octene Copolymer LLDPE Film Resin FP619-A complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, withou.. |
|||
Density | 0.919 g/cc | 0.0332 lb/in³ | ASTM D792 |
NOVA Chemicals Sclair® 61C Octene LLDPE Extrusion Resin
(discontinued **) Features: Octene co-polymer, excellent sealability and toughness, high drawdown, high adhesion, good barrier, good abrasion resistance.Applications: Food packaging, milk cartons, paperboard containe.. |
|||
Density | 0.919 g/cc | 0.0332 lb/in³ | ExxonMobil Method |
ExxonMobil LD 103.MP Industrial Film Resin
(discontinued **) LD 103 resins are homopolymer industrial film resins are used in box and drum liners, industrial packaging, medium duty shrink wrap, construction and agriculture film, and rubber bale wrap.Informati.. |
|||
Density | 0.919 - 0.922 g/cc | 0.0332 - 0.0333 lb/in³ | TSTM 209 B |
Iran Petrochemical (PCC) Bandar Imam Poliran LF0450 LDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Density | 0.919 g/cc | 0.0332 lb/in³ | ASTM D1505 |
M. Holland Company LD220 LDPE
(discontinued **) Features: Good Heat Seal, Good Processability, Good ToughnessUses: Industrial Applications, Liners, PackagingProcessing Method: Blown FilmInformation provided by M. Holland. |
|||
Density | 0.919 g/cc | 0.0332 lb/in³ | ASTM D792 |
NOVA Chemicals Novapol® LA-0218-AF LDPE Foam Resin
(discontinued **) Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Specifically designed for foam process, Blends with LLDPEAdditives: Base resinFilm properties are typical of blown fi.. |
|||
Density | 0.919 g/cc | 0.0332 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® NA149000 Low Density Polyethylene, Sheet Extrusion Grade PETROTHENE NA149000 resin exhibits an excellent balance of toughness and softness, with excellent dimensional stability. Typical applications include housewares, toys, containers and novelty items. .. |
|||
Density | 0.919 g/cc | 0.0332 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® NA951080 Low Density Polyethylene ApplicationsPETROTHENE NA 951-080 is designed for use as a base resin for compounding material including gas-injected or chemically expanded insulation. NA 951-080 is a natural, low density, medium.. |
|||
Density | 0.919 g/cc | 0.0332 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® NA952000 Low Density Polyethylene ApplicationsPETROTHENE NA 952 is a series of homopolymer resins especially designed for industrial and consumer packaging, and liner and bag applications. NA 952 has an excellent balance of process.. |
|||
Density | 0.919 g/cc | 0.0332 lb/in³ | ASTM D1505 |
LyondellBasell Petrothene® NA967000 Low Density Polyethylene, Film Extrusion Grade Petrothene NA967000 is a low density polyethylene resin designed for blown film, general purpose and industrial packaging applications. NA967000 exhibits good processing characteristics and impact s.. |
|||
Density | 0.919 g/cc | 0.0332 lb/in³ | |
LyondellBasell Lupolen® 1810 D LDPE Blow moldings, sheet, profile, film.Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Density | 0.919 g/cc | 0.0332 lb/in³ | |
LyondellBasell Lupolen® 1812 D LDPE Insulation for cableData was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Density | 0.919 g/cc | 0.0332 lb/in³ | GOST 15139 |
Sibur 15803-020 Low Density Polyethylene For production of films and film articles, including thermoset films, thin films, food contact grade films
(including tight packing), general-purpose films, and bags. |
|||
Density | 0.919 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Westlake EF608 Low Density Polyethylene Westlake EF608 is a high melt index LDPE resin suggested for thin gauge garment films and other films requiring excellent drawdown. The high melt index makes this material a good choice in compound.. |
|||
Density | 0.919 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® L42022B Film (Butene Grade) LLDPE Butene Copolymer (Barefoot)Applications: Blown and cast filmBlown and cast filmMeets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of p.. |
|||
Density | 0.919 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® L62009X Film (Hexene Grade) LLDPE Hexene Copolymer (Barefoot)Applications: Cross laminated filmCross laminated filmMeets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of.. |
|||
Density | 0.919 g/cc | 0.0332 lb/in³ | ExxonMobil Method |
ExxonMobil LD 051.LQ Shrink Film Resin L Product Description: LD 051.LQ blown film resin is a fractional melt index grade designed for demanding heavy duty film applications, and combines excellent strength properties with outstanding pr.. |
|||
Density | 0.919 g/cc | 0.0332 lb/in³ | ExxonMobil Method |
ExxonMobil LD 617.LN Molding, Extrusion and Compounding Resin Product Description: LD 617.LN is a high flow, low density polyethylene homopolymer resin designed to provide excellent processability, flexibility and surface appearance. This multipurpose resin is.. |
|||
Density | 0.919 g/cc | 0.0332 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 516.LN Low Density Polyethylene Resin Product Description: LD 516.LN is a medium MI, low density polyethylene resin designed for use in color concentrates and masterbatches where its flow properties ensure improved processability and un.. |
|||
Density | 0.919 g/cc | 0.0332 lb/in³ | |
Dow DOWLEX™ 2035 Linear Low Density Polyethylene, Cast Film Grade DOWLEX® 2035 Polyethylene resin is for cast film extrusion. It offers excellent tear strength, toughness and good processability. It complies with FDA regulation 21 CFR 177.1520(c) 3.2a when used u.. |
|||
Density | 0.919 g/cc | 0.0332 lb/in³ | |
Dow DOWLEX™ 2535 Linear Low Density Polyethylene, Narrow MW Distribution DOWLEX® 2535 Polyethylene resin is a narrow molecular weight distribution copolymer designed to offer excellent impact strength and stress crack resistance with good flexibility. It has good proces.. |
|||
Density | 0.919 g/cc | 0.0332 lb/in³ | ASTM D792 |
Dow TUFLIN™ HS-7021 NT 7 Linear Low Density Polyethylene Resin Industrial pallet wrap stretch film applications Premium film packaging applications Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a TUFLIN™ HS-7021 NT 7 is an ethylene-hexene-1 copolymer designed.. |
|||
Density | 0.919 g/cc | 0.0332 lb/in³ | ASTM-D1505 |
Braskem LF118 LLDPE Blown Film Extrusion Polyethylene Copolymer LF118 is a linear low-density polyethylene, copolymer of butene-1, produced by the gas phase process. It is developed for blown film extrusion in blends with polyethylene. Films obtained with this p.. |
|||
Density | 0.919 g/cc | 0.0332 lb/in³ | ASTM D-1505 |
Bapolene® 105F Low Density Polyethylene Film Resin Description: Bapolene LD105F is an unmodified low density polyethylene which extrudes into a low gloss high impact film. It contains antiblock additives and no slip additives. This product meets th.. |
|||
Density | 0.919 g/cc | 0.0332 lb/in³ | ASTM-D792 |
Braskem IP2418 LDPE Injection Molding Polyethylene IP2418 is a low-density polyethylene with good processability and high fluidity, flexibility, and mechanical strength. It does not contain additives. Its applications include injection molding and b.. |
|||
Density | 0.919 g/cc | 0.0332 lb/in³ | ASTM D1505 |
M. Holland Company LD220MM LDPE
(discontinued **) Additives: Medium Antiblock, SlipFeatures: Medium Antiblocking, Good Heat Seal, Medium SlipUses: Liners, PackagingProcessing Method: Blown FilmInformation provided by M. Holland. |
|||
Density | 0.919 g/cc | 0.0332 lb/in³ | ASTM D1505 |
Amco PRIMATOP LLDPE 009919B Linear Low Density Polyethylene, Butene Copolymer for Film LLDPE 009919B features excellent toughness and strength when drawn down to thin gauges. Applications include blending resin, industrial packaging, coextrusion, industrial liners, and garment bags.Fo.. |