Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.915 g/cc | 0.0331 lb/in³ | |
Plastcom SLOVALEN PC 16 FRD 1 PP, flame retardant Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0.. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® FORMAX® L91507E2 Film (Hexene Grade) LLDPE
(discontinued **) Superior Performance Linear Low Density Polyethylene for Film Extrusion Formolene FORMAX® L9 is a superior strength linear low density hexene copolymer polyethylene made using a gas-phase process. .. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ASTM D4883 |
Eastman E6838-850P Polyethylene
(discontinued **) E6838-850P is a low density resin designed for applications where high coating speeds and good drawdown are required. The combination of high melt index and low density also provides good heat seal.. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ISO 1183-A |
Carmel Olefins IPETHENE® 800 Low Density Polyethylene
(discontinued **) IPETHENE® 800 is a low density polyethylene injection molding grade. This grade is a good carrier for masterbatches production. It exhibits high flow and flexibility. APPLICATIONS IPETHENE® 800 i.. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ASTM D1505 |
LyondellBasell Montell 0800 Polybutene Key Features: highly isotactic, semi-crystalline homopolymer, good creep resistance, good environmental crack resistance, miscible with polypropylenes, FDA acceptableApplications: concrete carrierMe.. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ASTM D1505 |
LyondellBasell Microthene® G MN71020 Low Density Polyethylene General DescriptionMicrothene G polyolefin powders are ground, irregularly-shaped particles designed for use in a broad range of specialty applications. Microthene G powders combine the unique prop.. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ASTM D1505 |
ICO Polymers ICOFLOâ„¢ 510-5021 400 Micron LDPE Powder Description: ICOFLO 510-5021 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ASTM D1505 |
ICO Polymers ICOFLOâ„¢ 510-5060 800 Micron LDPE Powder Description: ICOFLO 510-5060 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a barrier in ma.. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ASTM D1505 |
ICO Polymers ICOFLOâ„¢ 510-5061 1200 Micron LDPE Powder Description: ICOFLO 510-5061 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ASTM D1505 |
ICO Polymers ICOTEXâ„¢ 520-5059 500 Micron LDPE Powder Description: ICOTEX 520-5059 is a low density polyethylene powder that has been developed to meet the special requirements of the textile coating industry. Information provided by ICO Polymers.A Sch.. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | |
Silon Tabond 3021 Adhesive Resin TABOND 3021 is LLDPE based adhesive resin for co-extruded three layer barrier and composite pipe applications.Characteristics: • Strong adhesion to aminosilane treated glass, Nylon,
EVOH, PET, .. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ISO 1183 |
Borealis CA9150 Low Density Polyethylene CA9150 is a low-density polyethylene for extrusion coating. CA9150 contains no additives. Applications: coating and lamination of aluminum foil, coating of various plastic films and cellophane, and.. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ASTM D792 |
DuPont Bynel® 4288 Anhydride-Modified LDPE Adhesive Resin Bynel® Series 4200 resins are anhydride-modified, low-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process .. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ISO 1183 |
Tisan TISETILEN® UNR Polyethylene TISETILEN has a wide area of application in construction, building auxiliary materials, lighting equipment, household appliance, toy industries, etc. General specifications include Low densityFlexib.. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ASTM D1505 |
Westlake EC850AA Low Density Polyethylene WESTLAKE low-density polyethylene EC850 is a resin designed for applications where high coating speeds and good drawdown are required. The combination of high melt index and low density provides goo.. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | Melt |
Covestro Desmopan® W DP 89051D Polyurethane PreprocessingMax. Water content |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ISO 1183 |
ExxonMobil Exxtral™ CNU 013 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin with good UV resistance designed for automotive exterior applications. Availability: Africa & Middle East, Asia Pacific, Europe, South.. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ExxonMobil Method |
ExxonMobil LD 200.48 Extrusion Coating and Laminating Resin Product Description: LD 200.48 is a general purpose LDPE extrusion coating grade, designed for flexible packaging applications. It offers – Low neck-in – Very good adhesion – Excellent heat seala.. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 200.48 Low Density Polyethylene Resin Product Description: LD 200.48 is a general purpose LDPE extrusion coating grade, designed for flexible packaging applications. It offers – Low neck-in – Very good adhesion – Excellent heat seala.. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ExxonMobil method |
ExxonMobil LDPE LD 259 Low Density Polyethylene Resin (European Grade) Product Description: LD 259 is a LDPE extrusion coating grade, especially introduced for coating on non-woven substrates. Its high melt-index combines with low density gives this grade the right bal.. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | |
Dow AFFINITY™ FM 1570 Polyolefin Plastomer AFFINITY® FM 1570 polyolefin plastomer is an ethylene alpha-olefin resin designed to provide film products with excellent sealability and high hot tack strength, outstanding blown film optics, and .. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ASTM D792 |
Dow ELITE™ 5220G Enhanced Polyethylene Resin High impact and puncture resistance Excellent on-pallet load elongation for higher yields on regular loads Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ASTM D1505 |
Braskem PB 608 LDPE Injection Molding Polyethylene Description: PB608 is a grade produced under high pressure in an autoclave reactor. This grade is especially designed for injection molding of articles that must show excellent flexibility propertie.. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ASTM D-1505 |
Bapolene® 152A Polyethylene Film Grade Bapolene 152A is a hexene linear low density polyethylene with a combination of superior impact strength and HSIT. Product is designed to exhibit performance similar to that of metallocene products... |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ASTM D-1505 |
Bapolene® 152B Polyethylene Film Grade Bapolene 152B is a hexene linear low density polyethylene with a combination of superior impact strength and HSIT. Product is designed to exhibit performance similar to that of metallocene products... |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | |
BASF CHAPA 3-(Cyclohexylamino) propylamine Formula: C9H20N2CAS: 3312-60-5Description: CHAPA is a colorless to yellow liquid, with an amine-like odor. It is miscible with water.Synonyms: CHAPA, Cyclohexylaminopropylamine, 3-Cyclohexylaminopr.. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ISO 1183-A |
Carmel Olefins IPETHENE® 900 Low Density Polyethylene IPETHENE® 900 is a low density polyethylene injection molding grade. This grade is a good carrier for masterbatches production. It exhibits high melt flow rate, good transparency, and flexibility. .. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ISO 1183-A |
Carmel Olefins IPETHENE® 600 Low Density Polyethylene IPETHENE® 600 is a low density polyethylene injection molding grade. This grade is a good carrier for masterbatches production. It exhibits good stiffness and moderate melt flow rate. APPLICATIONS.. |
|||
Density | 0.915 - 0.919 g/cc | 0.0331 - 0.0332 lb/in³ | ASTM D1505 |
Petroquimica Triunfo Trithene® JX 7300 LDPE - Injection Molding The Trithene® JX 7300 resin is a low-density polyethylene (LDPE) with outstanding flow ability and flexibility. Those attributes are especially important to meet the requirements for fast injection.. |
|||
Density | 0.915 g/cc | 0.0331 lb/in³ | ExxonMobil method |
ExxonMobil Exceed™ 1015HA Metallocene Polyethylene Resin Product Description: Exceed 1015 mVLDPE resin is metallocene ethylene-hexene copolymer. Films made from Exceed 1015 mVLDPE have outstanding cold temperature toughness, impact strength and puncture. .. |