Physical Properties Metric English Comments
Density 0.904 g/cc
0.0327 lb/in³
ASTM D792-91
Multibase Multi-Flex® TPO D 3105
The following is the actual data obtained from the above sample number. This material is based on new generation TPO technology. It has been designed for use as the first shot for airbag covers.Da..
Density 0.904 g/cc
0.0327 lb/in³
ASTM D792
Network Polymers NPP 30-0300
Description: Homopolymer PolypropyleneInformation provided by Network Polymers Inc.
Density 0.904 g/cc
0.0327 lb/in³
ASTM D792
Network Polymers NPP 30-0400
Description: Homopolymer PolypropyleneInformation provided by Network Polymers Inc.
Density 0.904 g/cc
0.0327 lb/in³
ASTM D792
Network Polymers NPP 30-0500 A
Description: Homopolymer Polypropylene with AntistaticInformation provided by Network Polymers Inc.
Density 0.904 g/cc
0.0327 lb/in³
ASTM D792
Network Polymers NPP 30-1800
Description: Homopolymer PolypropyleneInformation provided by Network Polymers Inc.
Density 0.904 g/cc
0.0327 lb/in³
ASTM D792
Phillips 66 COPYLENE® CH003T Polypropylene, Homopolymer, Sheet
COPYLENE™ CH003T, a fractional melt flow polypropylene homopolymer resin, is available in pellet form. Replacement alternative for Pro-fax® HL561CInformation provided by Phillips 66.
Density 0.904 - 0.908 g/cc
0.0327 - 0.0328 lb/in³
ASTM D1505
Ineos H20Z-03 Polypropylene Homopolymer
This is a homopolymer containing nucleation and antistatic. It is designed for injection molding and meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520...
Density 0.904 - 0.908 g/cc
0.0327 - 0.0328 lb/in³
ASTM D1505
Ineos H36G-00 Polypropylene Homopolymer
This is a high flow rate homopolymer. This material is designed for fiber spinning and spun bonded processes. It meets the requirements of the U.S. Food and Drug Administration as specified in 21 ..
Density 0.904 g/cc
0.0327 lb/in³
ASTM D792
Multibase Multi-Flex® TPE A 6001 BLK
TPE A 6001 is designed for gasket seals, rotational valves, and electrical applications as well as low friction applications. Multi-Flex TPE contains Kratonâ„¢ G.Data provided by Multibase.
Density 0.904 g/cc
0.0327 lb/in³
ISO 1183
Borealis BC650MO Polypropylene Copolymer
BC650MO is a very high impact polypropylene heterophasic copolymer intended for injection molding. This product offers a good UV resistance, further enhanced by pigmentation. This grade features hig..
Density 0.904 g/cc
0.0327 lb/in³
ISO 1183
Borealis BH345MO Polypropylene Copolymer
BH345MO is a heterophasic copolymer. This grade is characterized by optimum combination of very high stiffness, good flow properties and good impact strength. and is designed for high speed injectio..
Density 0.904 g/cc
0.0327 lb/in³
ISO 1183
Borealis BJ100HP Polypropylene Copolymer
BJ100HP is a special low viscosity polypropylene compound developed to fit the production of PP-GF composites in the direct LFT compression and injection molding process as well as in combination wi..
Density 0.904 g/cc
0.0327 lb/in³
ASTM D1505
Formosa Plastics Formolene® 4101N Staple Fiber and Injection Molding Polypropylene
HomopolymerApplications: Staple Fiber and General Purpose Injection MoldingFormolene 4101N is a medium viscosity, highly isotactic polypropylene homopolymer designed for Staple Fiber and general pur..
Density 0.904 g/cc
0.0327 lb/in³
ASTM D1505
UBE UMERIT 500F Metallocene LLDPE
Description: UBE Super Polyethylene Umerit® is an ethylene-olefin copolymer made by UBE using the metallocene catalytic method. The metallocene catalytic method results in superior physical propert..
Density 0.904 g/cc
0.0327 lb/in³
ASTM D792, ISO 1183
DuPont™ Fusabond® P353 Polymer Modifier
DuPont Fusabond® P353 is a chemically modified polypropylene. Uses: Automotive Applications Plastics Modification Polymer Modifier Applications: Coupling agent Long glass fiber filled PP compoun..
Density 0.904 g/cc
0.0327 lb/in³
ASTM D792
Diamond Polymers NPP30-0500 Homopolymer Polypropylene
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Density 0.904 g/cc
0.0327 lb/in³
ASTM D792
Dow ATTANE™ 4404G, 0.8mil Ultra Low Density Ethylene/Octene Copolymer
ATTANE™ 4201G provides improved cling in one-sided cling applications, and has improved toughness and optical properties. It complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a.Information provided by..
Density 0.904 g/cc
0.0327 lb/in³
ASTM D792
Dow ATTANE™ 4404G, 2mil Ultra Low Density Ethylene/Octene Copolymer
ATTANE™ 4201G provides improved cling in one-sided cling applications, and has improved toughness and optical properties. It complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a.Information provided by..
Density 0.904 g/cc
0.0327 lb/in³
ASTM D1505
Bapolene® PP5072 Polypropylene, Injection Grade
Bapolene PP 5072 is a multipurpose, high flow impact copolymer with excellent color and processability. This resin also exhibits a superior balance of stiffness and impact strength. This product m..
Density 0.904 g/cc
0.0327 lb/in³
BASF BAPMA N,N-Bis-(3-aminopropyl)methylamine
Formula: C7H18N3CAS: 105-83-9Description: N,N-Bis-(3-aminopropyl)methylamine is a colorless to yellow liquid, with an amine-like odor. It is miscible with water in all proportion.Synonyms: BAPMA, M..
Density 0.904 g/cc
0.0327 lb/in³
ASTM D1505
Bapolene® 4022 Polypropylene, Biaxially Oriented Film Grade
Bapolene PP4022 is a PP homopolymer designed for oriented film applications. It offers good clarity and optical properties. This resin meets FDA standards for food contact applications.Application..
Density 0.904 - 0.908 g/cc
0.0327 - 0.0328 lb/in³
ASTM D1505
Ineos H03G-01 Polypropylene Homopolymer
This is a homopolymer designed for tenter frame BOPP processing and meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.ApplicationsFood packagingOverwrap..
Density 0.904 g/cc
0.0327 lb/in³
ASTM D792
Ineos H20E-00 Polypropylene Homopolymer
This is a homopolymer containing antistatic designed for injection molding. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.Application..