Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.903 g/cc | 0.0326 lb/in³ | STN 64 0111 |
Plastcom SLOVALEN PC 53 N Polypropylene Copolymer, UV Stabilization FeaturesModified copolymer PP for injection moulding, with the ability of modeling the melt flow rate within the interval 5 - 20 g/10 min. Can be used for simple small as well as for large complica.. |
|||
Density | 0.903 g/cc | 0.0326 lb/in³ | Injection molded specimen; ASTM D1505 |
Phillips Sumika Marlex® CHP-015 Thermoplastic Polyolefin
(discontinued **) Applications: Driver-side air-bag coversSoft interior trimSoft touch overmoldingInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 201.. |
|||
Density | 0.903 g/cc | 0.0326 lb/in³ | Injection molded specimen; ASTM D1505 |
Phillips Sumika Marlex® CHP-010 Thermoplastic Polyolefin
(discontinued **) Applications: Soft interior trimSoft touch overmoldingInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. |
|||
Density | 0.903 g/cc | 0.0326 lb/in³ | ASTM D792 |
M. Holland Company CP502 Polypropylene Copolymer Features: Copolymer, High Flow, High Impact ResistanceUses: Closures, Medical Applications, Thin-walled PartsProcessing Method: Injection MoldingInformation provided by M. Holland. |
|||
Density | 0.903 g/cc | 0.0326 lb/in³ | ISO 1183 |
Borealis Bormed™ BH348MO Polypropylene Heteroplastic Copolymer for Injection Molding Bormed™ BH348MO is a polypropylene copolymer characterized by high impact strength, fast flow and crystallization speed. The material is nucleated with Borstar® Nucleation Technology (BNT). This .. |
|||
Density | 0.903 g/cc | 0.0326 lb/in³ | ISO 1183 |
Borealis Bormod™ BJ368MO Polypropylene Heteroplastic Copolymer for Injection Molding Bormod™ BJ368MO is a polypropylene copolymer characterized by good flow, and optimum combination of high stiffness and high impact strength. The material is nucleated with Borstar® Nucleation Tec.. |
|||
Density | 0.903 g/cc | 0.0326 lb/in³ | ASTM D792, ISO 1183 |
DuPont™ Fusabond® P613 Polymer Modifier DuPont™ Fusabond® P613 is a anhydride modified polypropylene. FUSABOND P613 resin conforms with the Code of Federal Regulations, Title 21, Paragraph 175.105, covering the use of adhesive interlay.. |
|||
Density | 0.903 g/cc @Temperature 15.0 °C |
0.0326 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil HD Plus 85W-140 Mobilube HD Plus 80W-90 and 85W-140 are extra high performance commercial gear lubricants formulated from select base oils and an advanced additive system. These lubricants are engineered for perfor.. |
|||
Density | 0.903 g/cc | 0.0326 lb/in³ | ASTM D1505 |
Bapolene® PP5052 Polypropylene, Injection Grade Polypropylene injection impact copolymer with excellent color and processability. This resin also has a superior balance of stiffness and impact strength. This product meets FDA standards for food.. |
|||
Density | 0.903 g/cc | 0.0326 lb/in³ | ASTM D1505 |
Bapolene® PP5082 Polypropylene, Injection Grade Bapolene PP 5082 is a multipurpose, high flow impact copolymer with excellent color and processability. This resin also exhibits a superior balance of stiffness and impact strength. This product m.. |
|||
Density | 0.903 g/cc | 0.0326 lb/in³ | ASTM D792 |
Aclo Accucomp Polypropylene HPO306L Homopolymer |
|||
Density | 0.903 g/cc | 0.0326 lb/in³ | ASTM D1505 |
Amco PRIMATOP PP HOMO 040 Polypropylene for Cast Film PP HOMO 040 features low water carry over, excellent melt stability, and contains a unique combination of stabilizers. Applications include slit tape fabric stock and cordage.Former A-Top Polymers p.. |
|||
Density | 0.903 g/cc @Temperature 15.0 °C |
0.0326 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil HD Plus 85W-140 Mobilube HD Plus 80W-90 and 85W-140 are extra high performance commercial gear lubricants formulated from select base oils and an advanced additive system. These lubricants are engineered for perfor.. |
|||
Density | 0.903 g/cc | 0.0326 lb/in³ | |
BASF N-Methylpiperazine Formula: C5H12N2CAS: 109-01-3Description: N-Methylpiperazine is a colorless to yellow liquid with an amine-like odor. It is miscible in water. Synonyms: 1-Methylpiperazine, N-MethylpiperazinApplica.. |
|||
Density | 0.903 g/cc | 0.0326 lb/in³ | ASTM D792 |
M. Holland Company MAGMA® LM233-A LLDPE
(discontinued **) Features: Good Heat Seal, Good ProcessabilityUses: Coating Applications, Film, Cast Film, PackagingProcessing Method: Coextrusion, Blown FilmInformation provided by M. Holland. |