Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
PolyMirae Moplen HP640G Sheet and Thermoforming Grade Polypropylene Moplen HP640G is the polypropylene Homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP640G is a homopolymer particularly suitable for sheet and thermof.. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
PolyMirae Moplen HP653P Fiber (BCF/CF) Grade Polypropylene Moplen HP653P is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP653P is a homopolymer particularly suitable for heavy denier BCF .. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | Injection molded specimen; ASTM D1505 |
Phillips Sumika Marlex® AGM-110 Reactor Thermoplastic Polyolefins, Cold Temperature Impact Resistant
(discont Applications: Automotive fascias and claddingsConsumer productsTotes and binsInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. .. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D792B |
LyondellBasell Pro-fax 7523 Polypropylene Impact Copolymer Primary Processing Method: Injection MoldingKey Features: good cold impact resistance, good stiffness and impact balance, excellent dimensional stability, FDA acceptableApplications: seating, applia.. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D792B |
LyondellBasell Pro-fax SB787 Polypropylene Impact Copolymer Key Features: blush resistance, excellent dimensional satiability, fast cycling, easy molding, good cold impact resistance, good stiffness and impact balance, easily colored, FDA acceptableApplicati.. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
Flint Hills P4C5B-181B Polypropylene Homopolymer Features: Nucleated and Antistat. Product does not contain animal derived components. Phthalate-free.Applications: Injection Molding: Closures and cutleryInformation Provided by Flint Hills Resour.. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
Flint Hills P4C6B-134A Polypropylene Homopolymer Features: Excellent processability, nucleated and antistat. Product does not contain animal derived components. Phthalate-free.Applications: Injection Molding: Cutlery, Consumer Products, Cosmetic.. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
Flint Hills P4G2Z-026 Homopolymer Polypropylene Homopolymer, UL certified, and FDA compliant.Features: Low water carryover.Applications: Extrusion: tape and strapping.Former Huntsman polypropylene products are now produced by Flint Hills Resource.. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
Flint Hills P9G1Z-047 Polypropylene Features: Processing stability. Product does not contain animal derived components. Phthalate-free.Applications: Extrusion: Thick sheetingInformation Provided by Flint Hills Resources |
|||
Density | 0.900 g/cc @Temperature 23.0 °C |
0.0325 lb/in³ @Temperature 73.4 °F |
ISO 1183 |
Inno-Comp INNOPOL® CS 2-8000 Polypropylene Block-Copolymer INNOPOL® CS 2-8000 is a polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-8000 is highly suitable for pipe manufacturing where the required.. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ISO 1183 |
Iran Petrochemical (PCC) S 30 S Polypropylene This grade is for general injection molding applications.Applications: textile bobbins ,wheels ,fittings ,closures ,caps.Information provided by Iran Petrochemical Commercial Co. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
Mitsui ADMER® NF908A PE Type Polyolefin ADMER® Adhesive Resin is a modified polyolefin with functional groups, designed to bond to a variety of polyolefins, ionomers, polyamides, ethylene vinyl alcohol (EVOH), polyesters (PET), polycar.. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D792 |
Multibase Multi-Flex® TPE 6568 C 1 NATURAL This product was designed for 2 shot airbag covers with lower tensile strength than currently in use. The moisture content is 1%. The fogging test value is 70% according to ASTM GM 9305P. Multi-F.. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D792B |
LyondellBasell Pro-fax SR549M Polypropylene Random Copolymer, Clarified Primary Processing Method: Injection Molding and Injection Stretch Blow MoldingKey Features: clarified polypropylene random copolymer resin, superior clarity, good impact and rigidity balance, good .. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
Mitsui ADMER® SE800 Elastomer Type Polyolefin ADMER® Adhesive Resin is a modified polyolefin with functional groups, designed to bond to a variety of polyolefins, ionomers, polyamides, ethylene vinyl alcohol (EVOH), polyesters (PET), polycar.. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ISO 1183 |
Iran Petrochemical (PCC) S 28 F Polypropylene Film Biaxially oriented poly propylene films suitable for metallization Applications: cosmetics , food stuffs , lamination and other flexible films.Information provided by Iran Petrochemical Commercial C.. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D792B |
LyondellBasell Astryn CA743GA Polypropylene Copolymer Key Features: low melt flow, low modulus, UV-stabilized polypropylene copolymer with antiblock, good heat seamability, good puncture resistance, plasticizer-free, excellent low temperature impact re.. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ISO 1183 |
LyondellBasell Hostacomâ„¢ CA278A Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ CA278A is a thermoplastic polyolefin elastomer that is used for automotive interior partsFeatures: Good StiffnessHigh FlowGood MoldabilityGood Impact ResistanceLow Temper.. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Polidan® EC/51 Polyethylene, Crosslinked (XLPE) Flexible low density polyethylene based compound crosslinkable by moisture; it consists of a silane pregrafted base compound (Sioplas® method) to be used with a catalyst masterbatch.Standards com.. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® 5102KR Cast Film Polypropylene HomopolymerApplications: Biaxially oriented film.Formolene 5102KR is a highly isotactic polypropylene homopolymer designed primarily for cast film applications such as slit tape fabric stock and cor.. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
Formosa Plastics Formolene® 5140N Homopolymer Polypropylene Homopolymer for Injection Molded Applications Formolene 5140N is a highly isotactic, polypropylene homopolymer with fast cycle time and improved mold release. It has use in injection molded applicat.. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | |
ExxonMobil ACHIEVE 3854 Exxpol Metallocene Grade for Nonwovens Fiber and General Extrusion Applications Product Description: A premium homopolymer resin produced using ExxonMobil Chemical’s Exxpol™ Technology designed specifically for spunbpond technology. Narrow molecular weight distribution of the.. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ExxonMobil Method |
ExxonMobil PP5032E3 Polypropylene Copolymer Product Description: A polypropylene homopolymer type designed for production of monofilaments, tapes for the textile industry, geo textiles, fibrillated tapes for ropes and twines in the packaging.. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
Entec Hypro™ PP-CP0.5/10 Impact Copolymer, Fractional Melt Flow This is a high impact copolymer intended for use in blow molding, pipe, tubing, sheet and other extrusion applications.Information provided by Entec |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D792 |
Dow 5E89 Polypropylene Homopolymer Resin OverviewConsistent processabilityGood color stabilityHigh strength propertiesLow water "carry-over"High speed processingComplies with U.S. FDA 21 CFR 177.1520 (c)1.1aDOW 5E89 Polypropylene Resin is .. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ISO 1183/A |
Addiplast Addilene J 310 Polypropylene Copolymer UnreinforcedInformation provided by Addiplast. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D1505 |
Bapolene® PP5021 Polypropylene, Blow Molding Grade Bapolene PP5021 is a PP Random Copolymer designed for blow molding and extrusion applications. This resin exhibits excellent clarity, impact strength, stiffness and processability. This product me.. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | A Component; ASTM D1475 |
Aptek 2506-A/B Room temperature curing, low modulus urethane conformal coating Room temperature curing, low modulus urethane conformal coatingAPTEK 2506-A/B is an unfilled, two component, electrically insulating, transparent, flexible urethane coating system designed for the e.. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ISO 1183 |
ExxonMobil Exxtral™ CNW 010 Performance Polyolefin Product Description: A specialty thermoplastic polyolefin resin designed for injection molded automotive interior trim applications requiring low warpage.Availability: Africa & Middle East, Asia Pac.. |
|||
Density | 0.900 g/cc | 0.0325 lb/in³ | ASTM D792 |
Braskem INSPIRE™ 117 Performance Polypropylene Polymer D 117.00 Developmental Performance Polymer is a propylene-based resin intended for use in extrusion blow molding and thermoforming applications where stiffness, toughness, high temperature resistanc.. |