Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.892 g/cc | 0.0322 lb/in³ | ASTM D792 |
Lushan PR298 Polypropylene Copolymer Adhesive for Steel Pipe Coating Polypropylene copolymer adhesive resin Lushan PR298 is maleic grafted polymer in granule form. It is a high tech product and was developed by Guangzhou Hot-melt Adhesive Engineering and Technical R&.. |
|||
Density | 0.892 g/cc | 0.0322 lb/in³ | ASTM D792 |
LyondellBasell Adflexâ„¢ KS311P Polyolefin Description: Adflexâ„¢ KS-311P thermoplastic olefin resin is a barefoot formulation (no slip, no antiblock) designed for cast film extrusion applications. It is based on proprietary Basell proces.. |
|||
Density | 0.892 g/cc | 0.0322 lb/in³ | ASTM D792 |
LyondellBasell Adflexâ„¢ Q 402 F Polyolefin Description: Adflexâ„¢ Q 402 F thermoplastic olefin resin is designed for air quenched blown film applications. Q 402 F resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 1.. |
|||
Density | 0.892 g/cc | 0.0322 lb/in³ | ASTM D792 |
LyondellBasell Hifaxâ„¢ CA10GC Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CA10GC fractional melt flow, 100 MPa flexural modulus, precolored, UV-stabilized, reactor grade, extrudable thermoplastic elastomeric olefin (TEO) resin combines good proces.. |
|||
Density | 0.892 g/cc | 0.0322 lb/in³ | ASTM D792 |
LyondellBasell Hifaxâ„¢ CA138A Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CA138A low modulus thermoplastic olefin (TPO) resin is designed for impact modification and injection molding applications. It is based on material produced from Basell'.. |
|||
Density | 0.892 g/cc | 0.0322 lb/in³ | ASTM D792 |
LyondellBasell Hifaxâ„¢ EP2015/60 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ EP2015/60 medium melt flow, 690 MPa flexural modulus, extrusion coating grade, specialty polypropylene copolymer has a very good balance of properties and processability. Th.. |
|||
Density | 0.892 g/cc @Temperature 15.0 °C |
0.0322 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil 30 Exxon XD-3 Exxon XD-3 20, 30, 40 and 50 are premium diesel engine oils blended from high quality base oils and a balanced additive system to meet or exceed the lubrication protection requirements of American d.. |
|||
Density | 0.892 g/cc @Temperature 15.0 °C |
0.0322 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil 30 Exxon XD-3 Exxon XD-3 20, 30, 40 and 50 are premium diesel engine oils blended from high quality base oils and a balanced additive system to meet or exceed the lubrication protection requirements of American d.. |
|||
Density | 0.892 g/cc | 0.0322 lb/in³ | |
ConocoPhillips Hydroclear® 320 Rock Oil Description: Conoco Hydroclear Rock Drill Oil is a high-quality, heavy-duty, extreme-pressure pneumatic tool lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Rock Drill .. |
|||
Density | 0.892 g/cc @Temperature 15.0 °C |
0.0322 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Mobil Delvac 40 1640 Mobil Delvac 1630, 1640, and 1650 are high performance monograde diesel engine oils formulated from advanced technology base oils and a balanced additive system. They are specifically engineered f.. |
|||
Density | 0.892 g/cc @Temperature 15.0 °C |
0.0322 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil Mobil Delvac 40 1640 Mobil Delvac 1630, 1640, and 1650 are high performance monograde diesel engine oils formulated from advanced technology base oils and a balanced additive system. They are specifically engineered f.. |
|||
Density | 0.892 g/cc | 0.0322 lb/in³ | ASTM D792 |
LyondellBasell Hifax™ CA207A Thermoplastic Polyolefin Elastomer Description: Hifax™ CA207A thermoplastic olefin resin is designed to reduce shrinkage and improve paint adhesion of PP compound. It is based on proprietary Basell process technology. All ingredien.. |