Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.880 g/cc | 0.0318 lb/in³ | STN EN ISO 1183-1 |
Plastcom PLASTALEN® PH 91 SDU Polypropylene Modified homopolymer PP for injection molding. General use in all industry branches. Delivered in natural mode and in full RAL color.Information Provided by Plastcom spol. s r.o. |
|||
Density | 0.880 g/cc | 0.0318 lb/in³ | ASTM D3574A |
Mearthane Durethaneâ„¢ F DF-255A Closed Cell Foam Polyurethane TDI backbone: ester.Summary: Durethane F is chemically blown urethane closed cell foam. Mearthane can custom formulate Durethane F, varying the physical properties (coefficient of friction, abrasio.. |
|||
Density | 0.880 g/cc | 0.0318 lb/in³ | |
Stellarchem GP-915UB TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Density | 0.880 g/cc | 0.0318 lb/in³ | |
Stellarchem GP-930 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
Density | 0.880 g/cc | 0.0318 lb/in³ | ASTM D792 |
Sumitomo Chemical ESPOLEX® 3675 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Density | 0.880 g/cc | 0.0318 lb/in³ | ASTM D792 |
Sumitomo Chemical ESPOLEX® 4675 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Density | 0.880 g/cc | 0.0318 lb/in³ | ASTM D792 |
Sumitomo Chemical ESPOLEX® UT461A Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Density | 0.880 g/cc | 0.0318 lb/in³ | ASTM D792 |
Sumitomo Chemical ESPOLEX® WT315 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Density | 0.880 g/cc | 0.0318 lb/in³ | ASTM D792 |
Sumitomo Chemical ESPOLEX® WT361 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Density | 0.880 g/cc | 0.0318 lb/in³ | ASTM D792 |
Sumitomo Chemical ESPOLEX® WT487X Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Density | 0.880 g/cc | 0.0318 lb/in³ | ASTM D792 |
Sumitomo Chemical ESPOLEX® WT521 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Density | 0.880 g/cc | 0.0318 lb/in³ | ASTM D792 |
Sumitomo Chemical ESPOLEX® WT525 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Density | 0.880 - 0.920 g/cc | 0.0318 - 0.0332 lb/in³ | RP-17617 |
Solvay RHODOLINE® 622 Surfactant Description: Mineral oil based defoamers for flat to gloss paints, great process foam know down.Identification: OIL BASE DEFOAMERAvailable in: North AmericaSolubility: Not dispersible in waterApplic.. |
|||
Density | 0.880 g/cc @Temperature 15.6 °C |
0.0318 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil 24 Mobil Mist Lube Series Mobil Mist Lube Series are extra high performance oils designed for the oil-fog or mist-lubrication of machine components such as slideways, bearings, gears, chains etc. They are formulated from hig.. |
|||
Density | 0.880 - 0.888 g/cc @Temperature 15.0 °C |
0.0318 - 0.0321 lb/in³ @Temperature 59.0 °F |
|
Unipetrol Benzene Benzene is manufactured by pyrolysis of oil fractions. It is a transparent, colourless, highly combustible, inflammable, volatile liquid, free of impurities and water.Information provided by Unipetr.. |
|||
Density | 0.880 g/cc | 0.0318 lb/in³ | |
ConocoPhillips Syncon® 460 Synthetic R&O Oil Syncon R&O Oil is a premium quality, synthetic, rust and oxidation (R&O)-inhibited circulating oil developed for use in circulating systems, rotary air compressors, lightly loaded enclosed gear driv.. |
|||
Density | 0.880 g/cc @Temperature 15.6 °C |
0.0318 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil 65 Exxon Aviation Oil EE Series Aviation Oil EE is the brand name of a premium quality line of ashless-dispersant piston engine oils. Formulated with select, highly refined base oils together with ashless-dispersant and anti-oxida.. |
|||
Density | 0.880 g/cc | 0.0318 lb/in³ | |
ConocoPhillips 150 Gear Oil AGMA Lubricant No. 4 EP Description: Conoco Gear Oil is a heavy-duty extreme-pressure industrial gear lubricant formulated from high-quality hydrocracked base stocks to provide excellent oxidation inhibition, EP load-carry.. |
|||
Density | 0.880 - 2.06 g/cc | 0.0318 - 0.0744 lb/in³ | Average value: 1.37 g/cc Grade Count:1191 |
Overview of materials for PVC, Wire and Cable Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Wire and Cable Grade". Each property range of values reported is minimum and maximum values of appr.. |
|||
Density | 0.880 - 0.910 g/cc | 0.0318 - 0.0329 lb/in³ | RP-17617 |
Solvay RHODOLINE® 679 Surfactant Description: Highly effective mineral oil defoamer for latex processing.Identification: OIL BASE DEFOAMERAvailable in: North AmericaApplications: RHODOLINE© 679 is recommended for application at 0... |