Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.868 g/cc | 0.0314 lb/in³ | |
Dow AFFINITY™ EG 8150 Polyolefin Elastomer AFFINITY® EG 8150 polyolefin elastomer is a saturated ethylene-octene copolymer for general purpose elastomeric applications that is efficiently crosslinked by peroxide, silane or irradiation It ex.. |
|||
Density | 0.868 g/cc | 0.0314 lb/in³ | ASTM D792 |
Dow AFFINITY™ EG 8150G Ethylene alpha-olefin copolymer AFFINITY™ EG 8150G Polyolefin Plastomer (POP) is produced via INSITE™ Technology. It is a general purpose ethylene alpha-olefin copolymer exhibiting high flexibility and elasticity. It can be ut.. |
|||
Density | 0.868 g/cc | 0.0314 lb/in³ | ASTM D792 |
Dow Engage® 8150 Polyolefin Elastomer Description: Engage® 8150 and Engage® 8157 polyolefin elastomers are ethylene-octene copolymers that have excellent flow characteristics and provide good impact properties in blends with polypropy.. |
|||
Density | 0.868 g/cc | 0.0314 lb/in³ | ASTM D792 |
Dow Engage® 8157 Polyolefin Elastomer Description: Engage® 8157 polyolefin elastomer is a loose talc surface coated ethylene-octene copolymer. The talc is untreated and has a nominal 1µm particle size. This product offers the exceptio.. |
|||
Density | 0.868 g/cc | 0.0313 lb/in³ | |
ConocoPhillips Conoco® El Mar® Geo Low Ash Oil, SAE Viscosity Grade 15W-40 Conoco® El Mar GEO Oil is a high-quality, non-detergent, ashless gas engine oil designed primarily for use in Ajax 2-stroke cycle natural gas engines. The SAE 15W-40 viscosity grade meets the low-t.. |
|||
Density | 0.868 g/cc | 0.0313 lb/in³ | |
ConocoPhillips El Mar® 2000 Oil SAE Grade 15W-40 Conoco® El Mar 2000 is a high-quality, very low-ash, dispersant detergent gas engine oil designed for use in naturally aspirated and moderately turbocharged, low- to medium-speed 2-stroke cycle and.. |
|||
Density | 0.868 - 0.881 g/cc @Temperature 15.0 °C |
0.0314 - 0.0318 lb/in³ @Temperature 59.0 °F |
|
Unipetrol Heavy Stabilized Oil Hydrogenate Stabilized oil hydrogenates are a fraction boiling above approximately 250°C, obtained from crude oil through distillation and mild hydrocracking. They are a mixture of light colour hydrocarbons of.. |