Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.867 g/cc | 0.0313 lb/in³ | |
BASF Cyclohexylamine (CHA) Formula: C6H13NCAS: 108-91-8Description: Cyclohexylamine i(CHA) s a colorless to yellow liquid with an amine-like odor. It is miscible with water.Synonyms: CHA, Cyclohexylamine, Cyclohexyl amine, 1-.. |