Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.852 g/cc | 0.0308 lb/in³ | |
ConocoPhillips Syncon® 32 Synthetic R&O Oil Syncon R&O Oil is a premium quality, synthetic, rust and oxidation (R&O)-inhibited circulating oil developed for use in circulating systems, rotary air compressors, lightly loaded enclosed gear driv.. |
|||
Density | 0.852 g/cc @Temperature 15.6 °C |
0.0308 lb/in³ @Temperature 60.1 °F |
ASTM D4052 |
ExxonMobil SpectraSyn Ultra™ 300 High VI Polyalphaolefin (PAO) Fluid Product Description: SpectraSyn Ultra™ High VI Polyalphaolefin (PAO) have high viscosity indices, low pour points, low traction, good air release, and low foaming tendency. The extremely high visco.. |
|||
Density | 0.852 g/cc @Temperature 15.0 °C |
0.0308 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil 524 Mobil SHC 500 Series Mobil SHC 500 Series oils are supreme performance hydraulic oils formulated from synthesised, wax-free hydrocarbon base fluids combined with a carefully engineered super-stabilised additive system. .. |
|||
Density | 0.852 g/cc | 0.0308 lb/in³ | |
ConocoPhillips Hydroclear® 115 Industrial Oil Description: Conoco Hydroclear Industrial Oil is a high-quality, general-purpose industrial lubricant formulated from premium Conoco hydrocracked base stocks. Hydroclear Industrial Oil is recommende.. |
|||
Density | 0.852 g/cc @Temperature 15.0 °C |
0.0308 lb/in³ @Temperature 59.0 °F |
ASTM D4052 |
ExxonMobil 524 Mobil SHC 500 Series Mobil SHC 500 Series oils are supreme performance hydraulic oils formulated from synthesised, wax-free hydrocarbon base fluids combined with a carefully engineered super-stabilised additive system. .. |