Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | >= 0.810 g/cc @Temperature 20.0 °C |
>= 0.0293 lb/in³ @Temperature 68.0 °F |
|
Kazanorgsintez E-14 Petroleum Resin Production Method: Obtained as a by-product in the process of hydrocarbon gas pyrolysis on ethylene production plants. Application: Feedstock for production of motor fuel, solvents and aromatic .. |
|||
Density | 0.810 g/cc | 0.0293 lb/in³ | ISO 1183 |
Menzolit Menzolit® SMC 0520 Unsaturated Polyester UP SMC 0520 is a special SMC with significantly reduced density. The glass level has been selected to combine good moulding with sufficient strength and stiffness properties. Even without a specific fi.. |
|||
Density | 0.810 g/cc | 0.0293 lb/in³ | |
Lord Adhesives Chemglaze® 9974 Roller Additive Chemglaze® thinners are formulated with urethane grade solvents and are used to reduce viscosity, aid bubble release, minimize orange peel, and make application easier.Chemglaze 9974 additive is .. |
|||
Density | 0.810 - 0.834 g/cc | 0.0293 - 0.0301 lb/in³ | |
Lord Adhesives HPC-5B Hydrogenated Nitrile Butadiene Rubber Coating LORD HPC-5B and HPC-5C are one-part, room temperature curing HNBR coatings which feature robust adhesion and exceptional mechanical properties. These coatings greatly enhance fluid and ozone resista.. |
|||
Density | >= 0.810 g/cc @Temperature 20.0 °C |
>= 0.0293 lb/in³ @Temperature 68.0 °F |
|
Kazanorgsintez E-8 Petroleum Resin Production Method: Obtained as a by-product in the process of hydrocarbon gas pyrolysis on ethylene production plants. Application: Feedstock for production of motor fuel, solvents and aromatic .. |
|||
Density | 0.810 - 0.890 g/cc | 0.0293 - 0.0322 lb/in³ | Apparent |
Gouda Vuurvast GI 26 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |
|||
Density | 0.810 g/cc | 0.0293 lb/in³ | |
DuPont™ Nomex® N196 Paper, 5 mil Nominal Thickness Nomex® Type N196 is a high floc grade of Nomex® paper. This leads to a high degree of saturability combined with high stiffness and mechanical properties. Type N196 is used where good saturabili.. |
|||
Density | 0.810 g/cc @Temperature 20.0 °C |
0.0293 lb/in³ @Temperature 68.0 °F |
ASTM D4052 |
ExxonMobil SBA Secondary Butyl Alcohol Appearance: Clear/Transparent LiquidAvailability: Africa & Middle East, Europe, Asia Pacific, Central America, North America and South AmericaInformation provided by ExxonMobil |
|||
Density | 0.810 g/cc | 0.0293 lb/in³ | |
BASF Isobutyleneoxide Formula: C4H8OCAS: 558-30-5Description: Isobutyleneoxide is a colorless to yellow liquid, with an ether-like odor. It is miscible in water.Synonyms: 2,2-DimethyloxiranApplications: Intermediate use.. |
|||
Density | 0.810 - 0.813 g/cc | 0.0293 - 0.0294 lb/in³ | |
BASF N-Butanol Formula: C4H10OCAS: 71-36-3Description: n-Butanol is a clear, mobile, neutral liquid with a characteristic odor. It is miscible with all common solvents, e.g., alcohols, ketones, aldehydes, ethers, .. |
|||
Density | 0.810 g/cc | 0.0293 lb/in³ | |
BASF 2-Methylpentanal Formula: C6H12OCAS: 123-15-9Description: 2-Methylpentanal is a colorless to yellow liquid with a pungent odor. Synonyms: 2-Methyl-1H-imidazolApplications: Intermediate used in the production of Phar.. |
|||
Density | 0.810 g/cc | 0.0293 lb/in³ | |
LATI Latimass 52/11-04 D008 PP Homopolymer Specific density compound based on Polypropylene homopolymer (PPh). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati.. |