Polymer Property : Density = 0.560 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.560 - 0.580 g/cc
0.0202 - 0.0210 lb/in³
Sibur PVC S-5868-PZ Suspension Polyvinyl Chloride (PVC)
For production of films and volume polymer containers for packing of food products and goods of public use.
Density 0.560 g/cc
0.0202 lb/in³
ASTM D792
Covestro Baydur® 730 IBS Polyurethane Structural Foam RIM, Density 35 pcf, MDI-based 2-Component Liquid System
0.25 in. thickness. IBS = Interactive Blowing System RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience ..
Density 0.560 g/cc
0.0202 lb/in³
3M Cushion-Mount™ E1840H Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion
3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam m..
Density 0.560 g/cc
0.0202 lb/in³
3M Cushion-Mount™ E1860H Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion
3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive and High Plateside Adhesion are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam m..
Density 0.560 g/cc
0.0202 lb/in³
Henkel SynSpand 9899 Expanding Syntactic Film
Very high expansion, closed cell expanding film designed for use as shop floor aid in closed mold processes.