Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.510 g/cc | 0.0184 lb/in³ | |
Zircar Ceramics AL-30AAH Alumina Insulation AL-30AAH was developed for use in copper vapor lasers where the ultimate in low mass alumina purity is required.Information provided by Zircar Ceramics. |
|||
Density | 0.510 g/cc | 0.0184 lb/in³ | |
Zircar Ceramics SALI-2 Alumina Insulation SALI-2 is a premium grade rigid insulation board used as hotface insulation or a precision machined furnace fixtures.Information provided by Zircar Ceramics. |
|||
Density | 0.510 g/cc | 0.0184 lb/in³ | ASTM D792 |
Covestro Baydur® STR/F-375 Polyurethane Composite SRIM Foam, 20% Glass Filled, MDI-based 2-Component Liquid System Contains continuous strand fiberglass mat.0.125 in. thickness.Information provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer .. |
|||
Density | 0.510 g/cc | 0.0184 lb/in³ | |
3M Cushion-Mount™ 1815M Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Density | 0.510 g/cc | 0.0184 lb/in³ | |
3M Cushion-Mount™ 1820M Plus Plate Mounting Tape 3M™ Cushion-Mount™ Plus Plate Mounting Tapes are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excellent print quality for pr.. |
|||
Density | 0.510 g/cc | 0.0184 lb/in³ | |
3M Cushion-Mount™ E1820 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |
|||
Density | 0.510 g/cc | 0.0184 lb/in³ | |
3M Cushion-Mount™ E1815 Plus Plate Mounting Tapes with Easy Mount Adhesive 3M™ Cushion-Mount™ Plus Plate Mounting Tapes with Easy Mount Adhesive are designed for mounting flexographic print plates to cylinders or sleeves. This family of foam mounting tapes provides excel.. |