Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.368 g/cc | 0.0133 lb/in³ | ASTM D1056 |
Monmouth Rubber & Plastics Durafoamâ„¢ C45 Closed Cell Epichlorohydrin Information provided by Monmouth Rubber & Plastics Corp. |
|||
Density | 0.368 g/cc @Temperature 121 °C |
0.0133 lb/in³ @Temperature 250 °F |
Dry Density |
Mid-Mountain Materials THERMOSEAL® FIBERPAK® M22 Moldable Description: A family of high temperature moldables designed for a wide variety of uses. THERMOSEAL® FIBERPAK® MOLDABLES may be formed into shapes or linings, pushed into cracks and holes, or .. |
|||
Density | 0.368 g/cc @Temperature 121 °C |
0.0133 lb/in³ @Temperature 250 °F |
Dry Density |
Mid-Mountain Materials THERMOSEAL® FIBERPAK® M607 Moldable Description: A family of high temperature moldables designed for a wide variety of uses. THERMOSEAL® FIBERPAK® MOLDABLES may be formed into shapes or linings, pushed into cracks and holes, or .. |
|||
Density | 0.368 - 0.481 g/cc @Treatment Temp. 982 °C, Time 86400 sec |
0.0133 - 0.0174 lb/in³ @Treatment Temp. 1800 °F, Time 24.0 hour |
Fired |
Unifrax Foamfrax® Isofoam® RG Insulation Foamfrax® RG (Refractory Grade) Insulation is an extension of the Foamfrax Insulation product line. Foamfrax RG Insulation is a combination of refractory ceramic fiber or soluble fiber, refractory.. |
|||
Density | 0.368 - 0.481 g/cc @Treatment Temp. 982 °C, Time 86400 sec |
0.0133 - 0.0174 lb/in³ @Treatment Temp. 1800 °F, Time 24.0 hour |
Fired |
Unifrax Foamfrax® RG Insulation Foamfrax® RG (Refractory Grade) Insulation is an extension of the Foamfrax Insulation product line. Foamfrax RG Insulation is a combination of refractory ceramic fiber or soluble fiber, refractory.. |
|||
Density | 0.368 - 0.481 g/cc @Treatment Temp. 1260 °C, Time 86400 sec |
0.0133 - 0.0174 lb/in³ @Treatment Temp. 2300 °F, Time 24.0 hour |
Fired |
Unifrax Foamfrax® RG Plus Insulation Like Foamfrax RG, Foamfrax® RG Plus combines refractory ceramic fiber, refractory cement, and a high-temperature binder solution that can be combined in the field using the uniqued Foamfrax process.. |