Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Density = 0.250 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Density 0.250 g/cc
0.00903 lb/in³
True Density as as measured by gas displacement
Potters Industries Sphericel® 25P45 Hollow Engineered Glass Microspheres
Sphericel® hollow glass microspheres are alternatives to conventional fillers and additives such as silicas, calcium carbonates, talc, clay, etc. A variety of particle sizes, densities and strength..
Density 0.250 g/cc
0.00903 lb/in³
Pyrotek Pyrite Vacuum Formed Product
Off White ColorApplicationsTap hole cones Riser sleeves Launder insulation Head boxes Ladle lining Pouring cups AdvantagesGood thermal shock resistance High strength/weight ratio Low thermal conduct..
Density 0.250 g/cc
0.00903 lb/in³
Pyrotek S-1100 Compressible Insulation Board
The Pyrotek S-1100 board is a low density calcium silicate product typically used for back-up insulation in refractory constructions.ApplicationsReduction cell insulation Trough covers Back-up insul..
Density 0.250 - 1.00 g/cc
0.00903 - 0.0361 lb/in³
available range
MarkeTech Carbon Nanofoam
Electrically conductive carbon nanofoams possess many of the properties of traditional aerogel material. These materials are available in the form of monoliths, granules, powders and papers. They ar..
Density 0.250 g/cc
0.00903 lb/in³
SPHERE ONE EXTENDOSPHERESâ„¢ XOL-200 Hollow Spheres
EXTENDOSPHERESâ„¢ XOL-200 are white aluminosilicate multicellular hollow spheres. The density of this product averages 0.25 g/cc. In plastic and coating applications, EXTENDOSPHERESâ„¢ XOL-200..
Density 0.250 g/cc
0.00903 lb/in³
Sharadaa Ceramics Calcium Silicate Block
Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota..
Density 0.250 g/cc
0.00903 lb/in³
Foam
Aptek DI-STRATE 95209 Microwave/RF Foam Substrate
DI-STRATE™ Tiles are fully-crosslinked, low density, composite foam substrates which exhibit a low characteristics in the microwave frequency range.Uses: Patch Radiators/SatelliteInformation provid..
Density 0.250 g/cc
0.00903 lb/in³
average; ISO 845
3A Composites Core Materials AIREX® C70.250 Universal Structural Foam
AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negligible ..
Density 0.250 g/cc
0.00903 lb/in³
3M K25 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Density 0.250 - 0.300 g/cc
0.00903 - 0.0108 lb/in³
DIN 53479 A
BIW ASTM Class 2D1 Silicone Foam
Products are a closed cell foam and there fore good for use in damp or liquid applications. A variety of physical properties and foam qualities are available by adjusting the processing parameters...