Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.190 g/cc | 0.00686 lb/in³ | Effective density of spheres |
Potters Industries Q-Cel® 5019 Performance Benefits: A low-density, performance-enhancing additive.Fewer defects: excellent mold flow, uniform dispersionReduced compound density and viscosityIncreased acoustic and thermal insulat.. |
|||
Density | 0.190 g/cc | 0.00686 lb/in³ | Effective density of spheres |
Potters Industries Q-Cel® 6019 Performance Benefits: A low-density, performance-enhancing additive.Fewer defects: excellent mold flow, uniform dispersionReduced compound density and viscosityIncreased acoustic and thermal insulat.. |
|||
Density | 0.190 g/cc | 0.00686 lb/in³ | Effective Density as measured by liquid displacement |
Potters Industries Q-Cel® 6019S Hollow Engineered Glass Microspheres Q-CEL® hollow glass microspheres are alternatives to conventional fillers and additives such as silicas, calcium carbonates, talc, clay, etc. A variety of particle sizes, densities and strengths me.. |
|||
Density | 0.190 g/cc | 0.00686 lb/in³ | Effective Density as measured by liquid displacement |
Potters Industries Q-Cel® 7019 Hollow Engineered Glass Microspheres Q-CEL® hollow glass microspheres are alternatives to conventional fillers and additives such as silicas, calcium carbonates, talc, clay, etc. A variety of particle sizes, densities and strengths me.. |
|||
Density | 0.190 g/cc | 0.00686 lb/in³ | |
Pyrotek Jacketed mesh core Tadpoles 304 stainless steel mesh core with continuous fiberglass jacket. Excellent where no mounting flange is required.AdvantagesGood Abrasion Resistance Excellent Compression and Recall Information provi.. |
|||
Density | 0.190 - 4.80 g/cc | 0.00686 - 0.173 lb/in³ | Average value: 1.49 g/cc Grade Count:273 |
Overview of materials for Epoxy Adhesive This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive". Each property range of values reported is minimum and maximum values of appropriate Mat.. |
|||
Density | 0.190 g/cc | 0.00686 lb/in³ | Pour Density |
TIMCAL ENSACO™ 150G Conductive Carbon Black ENSACO™ & SUPER P™ conductive carbon blacks are carbon blacks with a high to very high void volume allowing the retention of a carbon network at low to very low filler content. The void volume can.. |
|||
Density | 0.190 - 0.250 g/cc | 0.00686 - 0.00903 lb/in³ | |
3M S22 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Density | 0.190 g/cc | 0.00686 lb/in³ | |
Pyrotek Mesh core / V-5 Tadpoles Inconel mesh core with jacket and mounting flange consisting of high-temperature, ceramic fiber.AdvantagesFair Abrasion Resistance Excellent Compression and Recall Information provided by Pyrotek. |
|||
Density | 0.190 g/cc | 0.00686 lb/in³ | |
Pyrotek Mesh core / Z-6W Tadpoles 304 stainless steel mesh core with jacket and mounting flange consisting of wire reinforced, densely woven glass cloth.AdvantagesExcellent Abrasion Resistance Excellent Compression and Recall Inform.. |