Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.180 - 0.250 g/cc | 0.00650 - 0.00903 lb/in³ | typical range; ISO 845 |
3A Composites Core Materials AIREX® C70.200 Universal Structural Foam AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negli.. |
|||
Density | 0.180 g/cc | 0.00650 lb/in³ | |
Sharadaa Ceramics Saber Block, Pyroblock Services Offered: Retrofitting of Furnace, Installation of Castables/Bricks/Ceramic Fiber Modules, Castable Laying by Vibrocasting/Guiniting, Turnkey Installation Boiler/Chimney/Heater/Reformer/Rota.. |
|||
Density | 0.180 - 0.240 g/cc | 0.00650 - 0.00867 lb/in³ | ISO 1183 |
Fainplast Compounds EVAtech 807I Ethylene Vinyl Acetate Foam EVA (ethylene-vinyl acetate) designed for the production of crosslinked expanded products using injection technology.Information provided by Fainplast Compounds |
|||
Density | 0.180 - 0.220 g/cc | 0.00650 - 0.00795 lb/in³ | ISO 845-88 |
Eurofoam Siliconcell 412/BT 130 Silicone Foam Excellent thermal insulation and soundproofingInformation provided by Eurofoam s.r.l. |
|||
Density | 0.180 - 0.220 g/cc | 0.00650 - 0.00795 lb/in³ | True, 3M QCM 14.24.6 |
3M A20/1000 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Density | 0.180 - 0.220 g/cc | 0.00650 - 0.00795 lb/in³ | True, 3M QCM 14.24.6 |
3M H20/1000 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Density | 0.180 - 0.220 g/cc | 0.00650 - 0.00795 lb/in³ | |
3M K20 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Density | 0.180 - 1.99 g/cc | 0.00650 - 0.0717 lb/in³ | Average value: 1.03 g/cc Grade Count:671 |
Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Elastomer, Melt-Processible Rubber". Each property range of values reported is minimum and.. |
|||
Density | 0.180 - 0.220 g/cc | 0.00650 - 0.00795 lb/in³ | ISO 845-88 |
Eurofoam Porocell POR 304 CM-HD 200 EPDM Foam Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l. |