Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.170 g/cc | 0.00614 lb/in³ | |
Mo-Sci Corporation GL-0193 Hollow Glass Spheres Appearance: Hollow microspheres with white color in powder form.Applications: GL-0193 is a new, low cost, light weight, hollow glass extender for liquid resin systems offering low cost per unit volu.. |
|||
Density | 0.170 g/cc | 0.00614 lb/in³ | Pour Density; ASTM D1513 |
TIMCAL ENSACO™ 250G Conductive Carbon Black ENSACO™ & SUPER P™ conductive carbon blacks are carbon blacks with a high to very high void volume allowing the retention of a carbon network at low to very low filler content. The void volume can.. |
|||
Density | 0.170 g/cc | 0.00614 lb/in³ | Pour Density; ASTM D1513 |
TIMCAL ENSACO™ 260G Conductive Carbon Black ENSACO™ & SUPER P™ conductive carbon blacks are carbon blacks with a high to very high void volume allowing the retention of a carbon network at low to very low filler content. The void volume can.. |