Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.160 - 0.200 g/cc | 0.00578 - 0.00723 lb/in³ | ASTM D792 |
Microcell Composite Company CELLAMP® M5130 Thermoplastic Foam CELLAMP® FOAM can be mixed with high polymer materials to form traditional compound rubbers and plastics like EPDM, IIR, NBR, SBR, SILICONE, and EVA. Injection or hot-press PE compounds have high.. |
|||
Density | >= 0.160 g/cc | >= 0.00579 lb/in³ | |
Monmouth Rubber & Plastics Durafoamâ„¢ C43NBR Nitrile Rubber Information provided by Monmouth Rubber & Plastics Corp. |
|||
Density | 0.160 g/cc | 0.00578 lb/in³ | |
Sawbones Solid Rigid Polyurethane Foam 10 pcf Density Solid Rigid Polyurethane FoamPrimary UseSolid rigid polyurethane foam is primarily used as an alternative test medium for human cancellous bone. These products are not intended to replicate the mech.. |
|||
Density | 0.160 g/cc | 0.00578 lb/in³ | |
Sawbones Cellular Rigid Polyurethane Foam 10 pcf Density Cellular Rigid Polyurethane FoamPrimary UseCellular rigid polyurethane foam is primarily used as an alternative test medium for human cancellous bone. Its outward appearance matches cancellous bone .. |
|||
Density | 0.160 g/cc | 0.00579 lb/in³ | |
Unifrax Fiberfrax® Roll Board Ceramic Fiber Paper The lower density, binder chemistry, and bulk ceramic fiber grade used to manufacture Fiberfrax Rollboard paper result in a product with lower cost, higher flexibility, and reduced smoke and odor du.. |
|||
Density | 0.160 g/cc | 0.00579 lb/in³ | |
Unifrax Isofrax® 1260C Paper Fiber Isofrax® 1260C Paper is a unique product which is manufactured by forming Isofrax 1260C Fiber in a nonwoven matrix. The fibers are randomly oriented during manufacture, then held in place with a l.. |
|||
Density | 0.160 g/cc | 0.00578 lb/in³ | |
Zircar Refractory Composites RSPA-SOL2 Silica-Magnesia, Non-RCF Paper ZRCI Silica-Magnesia Papers Type RSPA-SOL are thermal insulation products capable of withstanding continuous operating temperatures up to 1260°C (2300°F). Type RSPA-SOL papers are designed to have.. |
|||
Density | 0.160 g/cc | 0.00578 lb/in³ | |
Zircar Refractory Composites RSPA-SOL4 Silica-Magnesia, Non-RCF Paper ZRCI Silica-Magnesia Papers Type RSPA-SOL are thermal insulation products capable of withstanding continuous operating temperatures up to 1260°C (2300°F). Type RSPA-SOL papers are designed to have.. |
|||
Density | 0.160 g/cc | 0.00579 lb/in³ | Nominal |
Hexcel® HexWeb® CR III 1/8-5052-.0025 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Density | 0.160 g/cc | 0.00578 lb/in³ | |
Zircar Refractory Composites ASPA-970 Alumina-Silica Fiber Paper ASPA-970 is an industrial grade, lightweight refractory material made from alumina-silica fibers formed into highly flexible sheets. This alumina-silica fiber paper exhibits very low thermal conduct.. |
|||
Density | 0.160 - 0.200 g/cc | 0.00578 - 0.00723 lb/in³ | ISO 845-88 |
Eurofoam Evacell EVA 200 EVA + PE Foam Foamed polyethylene charged with EVA, with extremely fine cells, excellent elasticity, resilience and mechanical resistance. It can be thermoformed several times. It has completely closed cells, di.. |
|||
Density | 0.160 g/cc | 0.00578 lb/in³ | Typical, 3M QCM 14.24.6 |
3M A16/500 Glass Bubbles 3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli.. |
|||
Density | 0.160 g/cc | 0.00579 lb/in³ | |
Unifrax Fiberfrax® 970 Ceramic Fiber Paper 970 paper is made from high-purity Fiberfrax washed fiber. During the manufacture of this product, a large portion of the unfiberized particles in the bulk fiber are removed prior to paper lay-up. .. |
|||
Density | 0.160 g/cc | 0.00579 lb/in³ | Edge Grain |
Unifrax Fibermass® 2600 Ceramic Fiber Blocks Fibermass® ceramic fiber blocks combine advancements in fiber chemistry and manufacturing technology to provide an economical lining material for a wide range of heat processing equipment. The Fib.. |