Physical Properties Metric English Comments
Density 0.140 - 0.180 g/cc
0.00506 - 0.00650 lb/in³
nominal
Microtherm Group SlimVac Filament Reinforced Silica Vacuum Insulation Panel
Microtherm® SlimVac panels are high performance evacuated microporous insulation panels covered in an impermeable outer envelope. The insulation is an opacified blend of filament reinforced silic..
Density 0.140 - 0.160 g/cc
0.00506 - 0.00578 lb/in³
Zircar Refractory Composites SB-2000 SILICA BLANKET
ZIRCAR Silica Blanket Type SB-2000 is a high temperature insulation blanket made of mechanically interlocked continuous filament amorphous silica fibers with useful properties to temperatures of 110..
Density 0.140 g/cc
0.00506 lb/in³
Zircar Refractory Composites RS-3000 ALUMINA FELT
ZRCI Alumina Felt Type RS-3000 is 97% high purity alumina fiber, ceramic felt with less than 1% shot. Type RS-3000 is a strong, flexible material with fibers held together with an organic binder. It..
Density 0.140 - 0.180 g/cc
0.00506 - 0.00650 lb/in³
ISO 845-88
Eurofoam Porocell POR 304 CM-HD EPDM Foam
Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.
Density 0.140 - 0.180 g/cc
0.00506 - 0.00650 lb/in³
True, 3M QCM 14.24.6
3M A16/500 Glass Bubbles
3M™ Glass Bubbles are engineered hollow glass microspheres that are alternatives to conventional fillers and additives such as silicas, calcium carbonate, talc, clay, etc., for many demanding appli..
Density 0.140 g/cc
0.00506 lb/in³
average; ISO 845
3A Composites Core Materials AIREX® R63.140 Damage Tolerant Foam
AIREX® R63 is a closed-cell, linear, thermoplastic polymer foam with extremely high damage tolerance. This formula combines high elongation and excellent bond strength. AIREX® R63 is cold formable..
Density 0.140 g/cc
0.00506 lb/in³
Zircar Refractory Composites ASPA-1 Alumina-Silica Fiber Paper
ASPA-1 is a premium grade, lightweight refractory material made from high purity alumina-silica fibers formed into highly flexible sheets. This alumina-silica fiber paper exhibits very low thermal c..
Density 0.140 g/cc
0.00506 lb/in³
Effective density of spheres
Potters Industries Q-Cel® 6014
Performance Benefits: A low-density, performance-enhancing additive.Fewer defects: excellent mold flow, uniform dispersionReduced compound density and viscosityIncreased acoustic and thermal insulat..
Copyright © lookpolymers.com All Rights Reserved