Density 0.0769 g/cc
0.00278 lb/in³
Lendell Nolatex® Latex Free Foam
This foam is used in the cosmetics industry and also possesses insulation qualities.Applications:Cosmetic Wedges and Puffs, Padding, High Insulative Value Applications, Makovers ® Disposable Make..
Density 0.0769 g/cc
0.00278 lb/in³
Nominal
Hexcel® HexWeb® ACG®-1/4 Honeycomb Aluminum Commercial Grade