Physical Properties Metric English Comments
Density 0.0700 g/cc
0.00253 lb/in³
Nominal skin/skin; BS ISO 7214 1998
Zotefoams Evazote® EV70CN Conductive Ethylene Vinyl Acetate Copolymer Foam
Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta..
Density 0.0700 g/cc
0.00253 lb/in³
Nominal skin/skin; BS ISO 7214 1998
Zotefoams Plastazote® LD70 Low Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Density 0.0700 g/cc
0.00253 lb/in³
ISO 845
BASF Neopolen® P 9035 0.07 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9035 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9035.Note: In order to mea..
Density 0.0700 g/cc
0.00253 lb/in³
ISO 845
BASF Neopolen® P 9230 A 0.07 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9230 A is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 A.Note: In order to..
Density 0.0700 g/cc
0.00253 lb/in³
ISO 845
BASF Neopolen® P 9255 0.07 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9255 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9255.Note: In order to mea..
Density 0.0700 g/cc
0.00253 lb/in³
ISO 845
BASF Neopolen® P 9280 0.07 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9280 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9280.Note: In order to mea..
Density 0.0700 g/cc
0.00253 lb/in³
ISO 845
BASF Neopolen® P 9335 MG 0.07 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9333 MG is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9333 MG.Note: In order ..
Density 0.0700 g/cc
0.00253 lb/in³
ISO 845
BASF Neopolen® P 9230 D 0.07 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9230 D is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 D.Note: In order to..
Density 0.0700 g/cc
0.00253 lb/in³
ISO 845
BASF Neopolen® P 9230 K 0.07 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9230 K is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9230 K.Note: In order to..
Density 0.0700 g/cc
0.00253 lb/in³
ISO 845
BASF Neopolen® P 9235 0.07 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9235 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9235.Note: In order to mea..
Density 0.0700 g/cc
0.00253 lb/in³
ISO 845
BASF Neopolen® P 9270 0.07 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9270 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9270.Note: In order to mea..
Density 0.0700 g/cc
0.00253 lb/in³
ISO 845
BASF Neopolen® P 9435 0.07 g/cc Core density; Expanded Polypropylene (Europe)
Description: Neopolen® P 9435 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9435.Note: In order to mea..
Density 0.0700 - 0.100 g/cc
0.00253 - 0.00361 lb/in³
Normal molded density
NOVA Chemicals Styrocell® D933A Expandable Polystyrene  (discontinued **)
This grade is a special molding grade consisting of spherical polystyrene beads containing pentane as expansion agent, typically used for dry molding of drinking cups and thin wall containers.Applic..
Copyright © lookpolymers.com All Rights Reserved