Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | >= 0.0481 g/cc | >= 0.00174 lb/in³ | Single Pass Continuous Expansion |
NOVA Chemicals Dylite® F271T Specialty Expandable Polystyrene Features: Highly consistent bead size; high gloss characteristics; low energy consumption; fast cyclingApplications: Drinking cups -hot and cold, noodle bowls, take-out and ice cream containers, and.. |
|||
Density | >= 0.0481 g/cc | >= 0.00174 lb/in³ | Batch Expansion |
NOVA Chemicals Dylite® F271T Specialty Expandable Polystyrene Features: Highly consistent bead size; high gloss characteristics; low energy consumption; fast cyclingApplications: Drinking cups -hot and cold, noodle bowls, take-out and ice cream containers, and.. |
|||
Density | 0.0481 - 0.0801 g/cc | 0.00174 - 0.00289 lb/in³ | |
Monmouth Rubber & Plastics Durafoamâ„¢ IVN 41 NEO/PVC/NBR Information provided by Monmouth Rubber & Plastics Corp. |
|||
Density | 0.0481 g/cc | 0.00174 lb/in³ | Nominal |
Hexcel® HexWeb® CR III 3/8-5056-.002 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Density | 0.0481 g/cc | 0.00174 lb/in³ | |
Hexcel® HexWeb® HRH-10 - 1/8- 3.0 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |
|||
Density | 0.0481 g/cc | 0.00174 lb/in³ | |
Hexcel® HexWeb® HRH-10 - 3/16 - 3.0 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |
|||
Density | 0.0481 g/cc | 0.00174 lb/in³ | |
Hexcel® HexWeb® HRH-10 - 3/8 - 3.0 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |
|||
Density | 0.0481 g/cc | 0.00174 lb/in³ | |
Hexcel® HexWeb® HRH-10/OX - 1/4 - 3.0 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |
|||
Density | 0.0481 g/cc | 0.00174 lb/in³ | |
Hexcel® HexWeb® HRH-10/OX - 3/16 - 3.0 Aramid Fiber/Phenolic Resin Honeycomb Designation: Material-Cell Size-Density.Hexweb HRH-10 is manufactured from NOMEX aramid fiber sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after expanding to the h.. |
|||
Density | 0.0481 g/cc | 0.00174 lb/in³ | |
Hexcel® HexWeb® HRH-36 - 1/8 - 3.0 Para-Aramid/Phenolic Core Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-36 is manufactured using KEVLAR® paper. The standard resin system is phenolic.Features: Mechanical properties equivalent to KOREX®; Low.. |
|||
Density | 0.0481 g/cc | 0.00174 lb/in³ | |
Hexcel® HexWeb® HRH-36/OX - 3/16 - 3.0 Para-Aramid/Phenolic Core Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-36 is manufactured using KEVLAR® paper. The standard resin system is phenolic.Features: Mechanical properties equivalent to KOREX®; Low.. |
|||
Density | 0.0481 g/cc | 0.00174 lb/in³ | |
Hexcel® HexWeb® HRH-36® Flex-Core® HRH-36 - F50 - 3.0 Aramid Honeycomb Designation: Material-Cell Size (cells per lineal foot in W direction)-Density (lb per cubic foot)HexWeb HRH-36 Flex-Core aramid paper is reinforced with a high temperature phenolic resin. This prod.. |
|||
Density | 0.0481 g/cc | 0.00174 lb/in³ | |
Hexcel® HexWeb® HRH-78 - 1/4 - 3.0 Commercial Grade Nomex Honeycomb/Phenolic Resin Designation: Material-Cell Size (inches)-DensityHexWeb HRH-78 is manufactured from commercial grade aramid paper sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after.. |
|||
Density | 0.0481 g/cc | 0.00174 lb/in³ | |
Hexcel® HexWeb® HRH-78 - 1/8 - 3.0 Commercial Grade Nomex Honeycomb/Phenolic Resin Designation: Material-Cell Size (inches)-DensityHexWeb HRH-78 is manufactured from commercial grade aramid paper sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after.. |
|||
Density | 0.0481 g/cc | 0.00174 lb/in³ | |
Hexcel® HexWeb® HRH-78 - 3/16 - 3.0 Commercial Grade Nomex Honeycomb/Phenolic Resin Designation: Material-Cell Size (inches)-DensityHexWeb HRH-78 is manufactured from commercial grade aramid paper sheets. A thermosetting adhesive is used to bond these sheets at the nodes, and after.. |
|||
Density | 0.0481 g/cc | 0.00174 lb/in³ | Nominal |
Hexcel® HexWeb® CR III 3/8-5052-.002 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Density | 0.0481 g/cc | 0.00174 lb/in³ | Nominal |
Hexcel® HexWeb® CR-PAA™ 3/8-5052-0.002 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Density | 0.0481 g/cc | 0.00174 lb/in³ | Nominal |
Hexcel® HexWeb® CR-PAA™ 3/8-5056-0.002 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Density | 0.0481 g/cc | 0.00174 lb/in³ | Free Rise Density, 2% H<sub>2</sub>O |
ACC EP LS EPI Engineered Polymers Leak Stop MDI EP LS, “Powered by Reactamine® Technology”, is a special MDI prepolymer designed to be pumped into voids or walls. EP LS reacts with water to create a shaving cream-like foam. This foam will soli.. |