Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.0230 - 0.0600 g/cc | 0.000831 - 0.00217 lb/in³ | Pressurized batch pre-foamer; Usual Use |
NOVA Chemicals Gedexcel® 44B Expandable Polystyrene Styrene homopolymer containing pentane, used as a blowing agent. Fast molding cycle product reduced stabilization time in silo. Especially adapted to high density molding and thin thickness, and fr.. |
|||
Density | 0.0230 - 0.0400 g/cc | 0.000831 - 0.00145 lb/in³ | Usual Use |
NOVA Chemicals Gedexcel® 44XA Expandable Polystyrene Styrene homopolymer containing pentane, used as a blowing agent with an additive improving its reaction to fire. Fast molding cycle product allowing to obtain optimum mechanical properties for form .. |
|||
Density | 0.0230 - 0.0600 g/cc | 0.000831 - 0.00217 lb/in³ | |
Polimeri Europa Extir® E 2000 AE Expandable Polystyrene
(discontinued **) Extir E 2000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of fine particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. Thi.. |
|||
Density | 0.0230 - 0.0330 g/cc | 0.000831 - 0.00119 lb/in³ | sheet density |
Zotefoams Plastazote® HD30 High Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |