Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.0200 - 0.0400 g/cc | 0.000723 - 0.00145 lb/in³ | Density range normally used |
Polimeri Europa Extir® B 2000 AE Expandable Polystyrene, Fast Molding Flame Retardant Particle size range is 0.4 - 0.75 mm. Minimum apparent density on a discontinuous pre-expander is 19 g/l.Processing technology used for Type B 2000 AE is: Molding, Vacuum.Specific characteristics: .. |
|||
Density | >= 0.0200 g/cc | >= 0.000723 lb/in³ | Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure |
NOVA Chemicals Dytherm® 140R Expandable Polystyrene This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma.. |
|||
Density | >= 0.0200 g/cc | >= 0.000723 lb/in³ | Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure |
NOVA Chemicals Dytherm® 150F Expandable Polystyrene This is a special flame retardant grade consisting of spherical beads of a blend of polystyrene and polyphenylene ether containing pentane as expansion agent, and a internal flame-retardant additive.. |
|||
Density | 0.0200 - 0.100 g/cc | 0.000723 - 0.00361 lb/in³ | Normal molded density assuming cost optimized selection of processing conditions. |
NOVA Chemicals Dytherm® 150F Expandable Polystyrene This is a special flame retardant grade consisting of spherical beads of a blend of polystyrene and polyphenylene ether containing pentane as expansion agent, and a internal flame-retardant additive.. |
|||
Density | >= 0.0200 g/cc | >= 0.000723 lb/in³ | Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure |
NOVA Chemicals Dytherm® 150R Expandable Polystyrene This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma.. |
|||
Density | >= 0.0200 g/cc | >= 0.000723 lb/in³ | Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure |
NOVA Chemicals Dytherm® 240R Expandable Polystyrene This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma.. |
|||
Density | 0.0200 - 0.100 g/cc | 0.000723 - 0.00361 lb/in³ | Normal molded density assuming cost optimized selection of processing conditions. |
NOVA Chemicals Dytherm® 240R Expandable Polystyrene This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma.. |
|||
Density | >= 0.0200 g/cc | >= 0.000723 lb/in³ | Minimum achievable; Single stage pre-expansion in continuous expander at atmospheric pressure |
NOVA Chemicals Dytherm® 250R Expandable Polystyrene This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma.. |
|||
Density | 0.0200 - 0.100 g/cc | 0.000723 - 0.00361 lb/in³ | Normal molded density assuming cost optimized selection of processing conditions. |
NOVA Chemicals Dytherm® 250R Expandable Polystyrene This is a special grade consisting of spherical beads of a blend of polystyrene-polyphenylene ether containing pentane as expansion agent, typically used for medium density foam with improved therma.. |
|||
Density | >= 0.0200 g/cc | >= 0.000723 lb/in³ | Single Pass Continuous Expansion |
NOVA Chemicals EPS 33MC Modified Expandable Polystyrene Applications: Insulation, SIP's, ICF's, fabricated and custom packagingInformation provided by NOVA Chemicals. |
|||
Density | >= 0.0200 g/cc | >= 0.000723 lb/in³ | Single Pass Continuous Expansion |
NOVA Chemicals EPS 34RC Regular Expandable Polystyrene Applications: PackagingInformation provided by NOVA Chemicals. |
|||
Density | >= 0.0200 g/cc | >= 0.000723 lb/in³ | Single Pass Continuous Expansion |
NOVA Chemicals EPS 35MB Modified Expandable Polystyrene Applications: Fabricated and custom packagingInformation provided by NOVA Chemicals. |
|||
Density | >= 0.0200 g/cc | >= 0.000723 lb/in³ | Batch Expansion |
NOVA Chemicals EPS M97C Expandable Polystyrene Resin Applications Insulation, SIP's, ICF's, Fabricated PackagingInformation provided by NOVA Chemicals |
|||
Density | 0.0200 - 0.0400 g/cc | 0.000723 - 0.00145 lb/in³ | |
Polimeri Europa Extir Leonardo B 2000 AE Expandable Polystyrene
(discontinued **) Extir B 2000 AE is a flame retardant expandable polystyrene in the form of spherical beads of fine particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Extir B 200.. |
|||
Density | 0.0200 g/cc | 0.000723 lb/in³ | 0.9 minute residence time pre-expander |
Jackon JACKOCELL® R311 Expanded Polystyrene Packaging and Shape Molding 100% Polystyrene.Pre-expansionHigh density stability in pre-expansion, transportation and silo storage reduces opportunity losses through achieving typical lower average density during regular produ.. |
|||
Density | 0.0200 g/cc | 0.000723 lb/in³ | 110 second cycle time |
Jackon JACKOCELL® S214 Expanded Polystyrene Construction and Block Molding Pre-ExpansionThe unique design of polystyrene chains and additive chemistry in Jackocell® S214 gives pre-expanded beads high dimensional stability even at low densities, which typically reduces a.. |
|||
Density | 0.0200 g/cc | 0.000723 lb/in³ | 125 rpm |
Jackon JACKOCELL® S214 Expanded Polystyrene Construction and Block Molding Pre-ExpansionThe unique design of polystyrene chains and additive chemistry in Jackocell® S214 gives pre-expanded beads high dimensional stability even at low densities, which typically reduces a.. |
|||
Density | 0.0200 - 0.0280 g/cc | 0.000723 - 0.00101 lb/in³ | sheet density |
Zotefoams Evazote® VA25 Ethylene Vinyl Acetate Copolymer Foam Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta.. |
|||
Density | 0.0200 - 0.0400 g/cc | 0.000723 - 0.00145 lb/in³ | ISO 845-88 |
Eurofoam Polycell PE 30 Polyethylene Foam Closed-cell polyethylene foam. Extruded reticulated pieces. Excellent physical properties both for active and static uses. Adjustable softness, elasticity, thermal deformation, shock absorbing. Use.. |
|||
Density | 0.0200 g/cc | 0.000723 lb/in³ | |
BASF E-por® 0.02 g/cc Density; Styrene and Ethylene (Europe) Description: Expandable granules made of styrene and ethylene containing polymers without flame retardant (blowing agent: pentane).Application: For the production of elastic, multi-shock absorbing e.. |
|||
Density | <= 0.0200 g/cc | <= 0.000723 lb/in³ | TMA |
Akzo Nobel Expancel® 053 DU 40 Dry unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Density | <= 0.0200 g/cc | <= 0.000723 lb/in³ | TMA |
Akzo Nobel Expancel® 053 WU 40 Wet unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Density | <= 0.0200 g/cc | <= 0.000723 lb/in³ | TMA |
Akzo Nobel Expancel® 461 DU 40 Dry unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Density | <= 0.0200 g/cc | <= 0.000723 lb/in³ | TMA |
Akzo Nobel Expancel® 461 WU 40 Wet unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Density | <= 0.0200 g/cc | <= 0.000723 lb/in³ | TMA |
Akzo Nobel Expancel® 551 DU 80 Dry unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Density | <= 0.0200 g/cc | <= 0.000723 lb/in³ | TMA |
Akzo Nobel Expancel® 551 WU 80 Wet unexpanded microspheres Expancel microspheres are thermoplastic hollow spheres. The microspheres are white spherically formed particles with a thermoplastic shell encapsulating a gas. When the microspheres are heated the.. |
|||
Density | 0.0200 - 0.0300 g/cc | 0.000723 - 0.00108 lb/in³ | molding density range |
IRPC Polimaxx Pentfoam 422F Expandable Polystyrene GENERAL: PENTFOAM "422F" IS A REGULAR GRADE (STANDARD GRADE) EXPANDABLE POLYSTYRENE (EPS) CONTAINING PENTANE AS BLOWING AGENT. THIS GRADE IS DEVELOPED TO MEET THE DEMAND FOR FAST MOLDING CYCLES IN V.. |
|||
Density | 0.0200 g/cc | 0.000723 lb/in³ | 120 rpm |
Jackon JACKOCELL® S314 Expanded Polystyrene Construction and Block Molding Pre-ExpansionThe unique design of polystyrene chains and additive chemistry in Jackocell® S314 gives pre-expanded beads high dimensional stability even at low densities, which typically reduces ave.. |
|||
Density | 0.0200 g/cc | 0.000723 lb/in³ | 105 second cycle |
Jackon JACKOCELL® S314 Expanded Polystyrene Construction and Block Molding Pre-ExpansionThe unique design of polystyrene chains and additive chemistry in Jackocell® S314 gives pre-expanded beads high dimensional stability even at low densities, which typically reduces ave.. |
|||
Density | 0.0200 - 0.0350 g/cc | 0.000723 - 0.00126 lb/in³ | Final Product Density |
Iran Petrochemical (PCC) TPC - 426 WP Expandable Polystyrene TPC - 426 WPApplications: very low water absorption, cycling shape molding of 6-10 mm wall thicknessInformation provided by Iran Petrochemical Commercial Co. |